Fracture, fatigue and environmentally-assisted failure of a Zr-based bulk amorphous metal

被引:35
|
作者
Ritchie, RO [1 ]
Schroeder, V [1 ]
Gilbert, CJ [1 ]
机构
[1] Univ Calif Berkeley, Dept Mat Sci & Mineral Engn, Berkeley, CA 94720 USA
关键词
fatigue resistance and crack growth; fracture toughness;
D O I
10.1016/S0966-9795(99)00155-7
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Bulk amorphous alloys, such as the Zr41.2Ti13.8Cu12.5Ni10Be22.5 (at%) alloy, have received much interest of late. This study seeks to investigate mechanical properties of this amorphous metal, including fracture and fatigue behavior in the presence of air and sodium chloride solution. For the fully amorphous Zr41.2Ti13.8Cu12.5Ni10Be22.5 (at%) alloy, plane-strain fracture toughness (K-1c) values of 18 to 68 MPa root m have been measured, the significant sample-to-sample variability being associated with the presence of residual stresses following processing and a dependence on loading rate. Upon partial or complete crystallization, the alloy becomes severely embrittled, with K(1)c dropping to similar to 1 MPa root m. Moreover, in NaCl solution, static load testing reveals a threshold value for cracking, K-ISCC, as low as similar to 0.8 MPa root m. Results from fatigue testing in air and sodium chloride, as well as fatigue testing under potential control, suggest that quite distinct mechanisms of fatigue-crack propagation are active in air and NaCl solution. Specifically, in air, fatigue-crack propagation behavior is similar to that observed in polycrystalline metals and is associated with alternating blunting and re-sharpening of the crack tip, as evidenced by the presence of fatigue striations. In NaCl solution, conversely, the high crack-growth rates likely depend on an anodic process, which results in a brittle mode of failure. (C) 2000 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:469 / 475
页数:7
相关论文
共 50 条
  • [41] Stable fracture of a malleable Zr-based bulk metallic glass
    Sun, B. A.
    Tan, J.
    Pauly, S.
    Kuehn, U.
    Eckert, J.
    JOURNAL OF APPLIED PHYSICS, 2012, 112 (10)
  • [42] Temperature Effect on Fracture of a Zr-Based Bulk Metallic Glass
    Yang, Na
    Yi, Jun
    Yang, Yu Hang
    Huang, Bo
    Jia, Yan Dong
    Kou, Sheng Zhong
    Wang, Gang
    MATERIALS, 2020, 13 (10)
  • [44] Compressive fracture characteristics of Zr-based bulk metallic glass
    Fan ZhenJun
    Zheng ZhiYuan
    Jiao ZengBao
    SCIENCE CHINA-PHYSICS MECHANICS & ASTRONOMY, 2010, 53 (05) : 823 - 827
  • [45] Compressive fracture characteristics of Zr-based bulk metallic glass
    ZhenJun Fan
    ZhiYuan Zheng
    ZengBao Jiao
    Science China Physics, Mechanics and Astronomy, 2010, 53 : 823 - 827
  • [46] Stable fracture of a malleable Zr-based bulk metallic glass
    IFW Dresden, Institut für Komplexe Materialien, Helmholtzstr. 20, D-01069 Dresden, Germany
    不详
    不详
    Sun, B.A. (bs7@ifw-dresden.de), 1600, American Institute of Physics Inc. (112):
  • [47] Thermal stability and mechanical properties of a Zr-based bulk amorphous alloy
    Fátay, D
    Gubicza, J
    Szommer, P
    Lendvai, J
    Blétry, M
    Guyot, P
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2004, 387 : 1001 - 1004
  • [48] Response of a Zr-based bulk amorphous alloy to shock wave compression
    Turneaure, Stefan J.
    Winey, J. M.
    Gupta, Y. M.
    JOURNAL OF APPLIED PHYSICS, 2006, 100 (06)
  • [49] Pressure-induced crystallization in a bulk amorphous Zr-based alloy
    He, DW
    Zhao, Q
    Wang, WH
    Che, RZ
    Liu, J
    Luo, XJ
    Wang, WK
    JOURNAL OF NON-CRYSTALLINE SOLIDS, 2002, 297 (01) : 84 - 90
  • [50] Progress in consolidation of amorphous Zr-based powder into bulk metallic glass
    Mathaudhu, SN
    Im, JT
    Barber, RE
    Anderson, IE
    Karaman, I
    Hartwig, KT
    SUPERCOOLED LIQUIDS, GLASS TRANSITION AND BULK METALLIC GLASSES, 2003, 754 : 191 - 198