Optimizing the fitting-surface preparation of zirconia restorations for bonding to dentin

被引:11
作者
Franz, Alexander [1 ]
Winkler, Olivia [1 ]
Lettner, Stefan [1 ]
Oppinger, Simon [1 ]
Hauser, Anna [1 ]
Haidar, Marwan [1 ]
Moritz, Andreas [1 ]
Watts, David C. [2 ,3 ]
Schedle, Andreas [1 ]
机构
[1] Med Univ Vienna, Univ Clin Dent, Vienna, Austria
[2] Univ Manchester, Sch Med Sci, Manchester, Lancs, England
[3] Univ Manchester, Photon Sci Inst, Manchester, Lancs, England
关键词
Zirconia restorations; Adhesive cementation; Zirconia-cement-interface; Glaze-on-technique; Air abrasion; LUTING CEMENT; RESIN CEMENT; AIR-ABRASION; STRENGTH; ADHESION; METAANALYSIS; RETENTION;
D O I
10.1016/j.dental.2020.12.001
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objectives. The aim of this study was to identify the relative strengths and weaknesses of different interfaces within the multilayer structure of a zirconia crown restoration when applying different surface pretreatments. These include the influence on shear strengths of different air abrasion protocols, glaze-on techniques, zirconia primers and self-adhesive cements for either the complex structure: zirconia / self adhesive resin composite cement (RCC) / bovine dentin substrate (part 1) or the RCC / zirconia substrate (part 2). Methods. In Part 1, zirconia discs, pretreated by either glaze-on techniques or air abrasion using Rocatec (TM) Soft, were bonded to bovine dentin substrates with different self-adhesive RCCs. In Part 2, steel-cylinders were bonded to zirconia cuboid substrates, pretreated by either different protocols for air-abrasion or a glaze-on-technique, with different self-adhesive RCCs. Shear bond strengths (SBS) were measured for all interfacial combinations. Results. In part 1, application of air abrasion using Rocatec (TM) Soft significantly increased the SBS of zirconia to dentin compared to control specimens without pretreatment, while glaze-on techniques did not increase the SBS. Pretreatment of zirconia surfaces with two primers (either Clearfil Ceramic Primer, or Monobond S) showed significantly higher SBS than the controls. Cementations with RelyX Unicem 2 Automix showed significantly higher SBS than with MaxCem Elite. In Part 2, all air abrasion protocols increased the SBS, but there was no significant difference between these protocols. Again the glaze-on technique did not increase SBS. A significant difference between the two RCCs was again observed. When zirconia substrates were air abraded, regardless of which protocol was applied, the highest SBS were obtained by Calibra with P&B active followed by Panavia with or without Clearfil Ceramic Primer Plus. Calibra applied without P&B active exhibited the lowest SBS. Significance. Pretreatment of zirconia substrates using air abrasion and/or ceramic primers increased the SBS of the zirconia cement interface. For all tested glaze-on treatments, in our experimental setting no effect was observed. (C) 2021 The Authors. Published by Elsevier Inc. on behalf of The Academy of Dental Materials. This is an open access article under the CC BY license (http://creativecommons.org/licenses/by/4.0/)
引用
收藏
页码:464 / 476
页数:13
相关论文
共 41 条
  • [1] [Anonymous], 104772018 ISO
  • [2] Does air particle abrasion affect the flexural strength and phase transformation of Y-TZP? A systematic review and meta-analysis
    Aurelio, Iana L.
    Marchionatti, Ana Maria E.
    Montagner, Anelise F.
    May, Liliana G.
    Soares, Fabio Z. M.
    [J]. DENTAL MATERIALS, 2016, 32 (06) : 827 - 845
  • [3] Bonding Effectiveness to Differently Sandblasted Dental Zirconia
    Bielen, Vincent
    Inokoshi, Masanao
    De Munck, Jan
    Zhang, Fei
    Vanmeensel, Kim
    Minakuchi, Shunsuke
    Vleugels, Jozef
    Naert, Ignace
    Van Meerbeek, Bart
    [J]. JOURNAL OF ADHESIVE DENTISTRY, 2015, 17 (03) : 235 - 242
  • [4] Adhesion to tooth structure: A critical review of "macro" test methods
    Braga, Roberto R.
    Meira, Josete B. C.
    Boaro, Leticia C. C.
    Xavier, Tathy A.
    [J]. DENTAL MATERIALS, 2010, 26 (02) : E38 - E49
  • [5] Effect of MDP-Based Primers on the Luting Agent Bond to Y-TZP Ceramic and to Dentin
    Butler, Sheila
    Linke, Bernie
    Torrealba, Ysidora
    [J]. BIOMED RESEARCH INTERNATIONAL, 2018, 2018
  • [6] Shear Bond Strength of Al2O3 Sandblasted Y-TZP Ceramic to the Orthodontic Metal Bracket
    Byeon, Seon Mi
    Lee, Min Ho
    Bae, Tae Sung
    [J]. MATERIALS, 2017, 10 (02)
  • [7] Effect of Surface Treatments of Zirconia Ceramics on the Bond Strength to Resin Cement
    Cheung, Guy C. K.
    Botelho, Michael G.
    Matinlinna, Jukka P.
    [J]. JOURNAL OF ADHESIVE DENTISTRY, 2014, 16 (01) : 49 - 56
  • [8] Bond strength of composite luting cement to zirconia ceramic surfaces
    Derand, T
    Molin, M
    Kvam, K
    [J]. DENTAL MATERIALS, 2005, 21 (12) : 1158 - 1162
  • [9] Improved bonding of zirconia substructures to resin using a "glaze-on" technique
    Everson, Peter
    Addison, Owen
    Palin, William M.
    Burke, F. J. Trevor
    [J]. JOURNAL OF DENTISTRY, 2012, 40 (04) : 347 - 351
  • [10] Can low-fusing glass application affect the marginal misfit and bond strength of Y-TZP crowns?
    Felipe Antunes, Monize Carelli
    Miranda, Jean Soares
    Almeida de Carvalho, Ronaldo Luis
    de Carvalho, Rodrigo Furtado
    Kimpara, Estevao Tomomitsu
    de Assuncao E Souza, Rodrigo Othavio
    Pereira Leite, Fabiola Pessoa
    [J]. BRAZILIAN ORAL RESEARCH, 2018, 32 : 1 - 10