Mineralogical characterisation of vanadium slag under different treatment conditions

被引:42
作者
Diao, J. [1 ]
Xie, B. [1 ]
Wang, Y. [1 ]
Ji, C. Q. [1 ]
机构
[1] Chongqing Univ, Coll Mat Sci & Engn, Chongqing 400044, Peoples R China
关键词
Vanadium slag; Spinel; Silicate; Grain size; Cooling rate;
D O I
10.1179/174328109X410622
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Synthetic vanadium slags were melted at 1673 K and then cooled to a predetermined temperature at different cooling rates. The mineralogical phases and crystallisation behaviour were investigated based on optical microscopy, SEM, EDS and XRD analyses. The results show that spinels and silicates were the major phases in the complex vanadium slag samples, and V is enriched in the spinel phases, i.e. FexV3-xO4 and Mg-x(V,Ti)(3-x)O-4. The apparent diameter of spinel crystal grains decreases with increasing cooling rate, e.g. from 14 to 5 mm at 1523 K. Crystal grain size increases significantly with increasing holding time. It is also found that the grain sizes of spinels at higher temperatures, 1573 and 1623 K, are considerably smaller than at lower temperatures, 1473 and 1523 K. At lower temperature, large blocked spinel crystals between grey silicate phases are formed, whereas there only a few smaller blocked spinels when performed at higher temperature. Better control of the process cooling parameters will benefit vanadium slag quality.
引用
收藏
页码:476 / 480
页数:5
相关论文
共 13 条
[11]  
Ye G., 2006, Recovery of Vanadium from LD Slag, a State of the Art Report: Part 1-Facts and Metallurgy of Vanadium
[12]   Concentrating of vanadium oxide in vanadium rich phase(s) by addition of SiO2 in converter slag [J].
Yu, L. ;
Dong, Y-C ;
Ye, G. Z. ;
Du Sichen .
IRONMAKING & STEELMAKING, 2007, 34 (02) :131-137
[13]  
ZHOU JZ, 2005, VANADIUM RESOURCE EX, P103