Synthesis and characterization of surface-modified rutile nanoparticles and transparent polymer composites thereof

被引:73
作者
Nussbaumer, RJ [1 ]
Caseri, W [1 ]
Tervoort, T [1 ]
Smith, P [1 ]
机构
[1] ETH Zentrum, Inst Polymers, Dept Mat, CH-8092 Zurich, Switzerland
关键词
rutile; nanoparticles; nanocomposites; surface-modification; UV absorption; visual transparency;
D O I
10.1023/A:1021141124257
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
Nanoparticles of rutile, a crystal modification of titanium dioxide, were synthesized in strongly acidic solutions by hydrolysis of titanium tetrachloride. The particles of average diameter 2 nm were coated in situ with a layer of dodecylbenzenesulfonic acid (DBSA) and isolated as a powder. Remarkably, dispersions of this powder in toluene were essentially transparent at the visible wavelengths but absorbed UV radiation over a broad wavelength range. The DBSA-coated rutile was also embedded in poly(styrene) and a poly( carbonate), resulting in polymer nanocomposites acting as visually transparent UV filters.
引用
收藏
页码:319 / 323
页数:5
相关论文
共 18 条
[1]  
Allen NS, 1996, ADV CHEM SER, V249, P537
[2]  
Allen NS., 1992, FUNDAMENTALS POLYM D
[3]   PHOTOCATALYTIC HYDROGENATION OF CH3CCH WITH H2O ON SMALL-PARTICLE TIO2 - SIZE QUANTIZATION EFFECTS AND REACTION INTERMEDIATES [J].
ANPO, M ;
SHIMA, T ;
KODAMA, S ;
KUBOKAWA, Y .
JOURNAL OF PHYSICAL CHEMISTRY, 1987, 91 (16) :4305-4310
[4]  
BALFOUR JG, 1990, J OIL COLOUR CHEM AS, V73, P478
[5]  
Caseri W, 2000, MACROMOL RAPID COMM, V21, P705, DOI 10.1002/1521-3927(20000701)21:11<705::AID-MARC705>3.0.CO
[6]  
2-3
[7]   Infrared spectroscopic evaluation of the photodegradation of paint - Part II: The effect of UV intensity & wavelength on the degradation of acrylic films pigmented with titanium dioxide [J].
Christensen, PA ;
Dilks, A ;
Egerton, TA ;
Temperley, J .
JOURNAL OF MATERIALS SCIENCE, 2000, 35 (21) :5353-5358
[8]  
*FLUK LAB, 2001, FLUK LAB CHEM CAT
[9]   Influence of titanium dioxide pigments on the photodegradation of poly(vinyl chloride) [J].
Gesenhues, U .
POLYMER DEGRADATION AND STABILITY, 2000, 68 (02) :185-196
[10]  
Gesenhues U., 1999, FARBE LACK, V105, P151