共 108 条
[41]
Improved understanding of environment-induced cracking (EIC) of sensitized 5XXX series aluminium alloys
[J].
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING,
2017, 682
:613-621
[42]
Holroyd N.J.H., 1989, Environmentally-Induced Cracking of Metals, P311
[43]
Holroyd N.J. H., 1984, ENV SENSITIVE FRACTU, P202
[46]
Stress Corrosion Cracking in Al-Zn-Mg-Cu Aluminum Alloys in Saline Environments
[J].
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE,
2013, 44A (03)
:1230-1253
[47]
Crack Propagation During Sustained-Load Cracking of Al-Zn-Mg-Cu Aluminum Alloys Exposed to Moist Air or Distilled Water
[J].
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE,
2011, 42A (13)
:3979-3998
[50]
Holtz R.L., 2011, DOD CORR C