Immobilisation of heavy metals in hazardous waste incineration residue using SiO2-Al2O3-Fe2O3-CaO glass-ceramic

被引:44
作者
Chen, Hongcai [1 ,2 ]
Lin, Huirong [2 ,3 ]
Zhang, Pengpeng [1 ,2 ]
Yu, Lin [2 ]
Chen, Liangjun [4 ]
Huang, Xiao [1 ,2 ]
Jiao, Binquan [1 ,2 ]
Li, Dongwei [1 ,2 ,3 ]
机构
[1] Chongqing Univ, State Key Lab Coal Mine Disaster Dynam & Control, Chongqing 400044, Peoples R China
[2] Chongqing Univ, Sch Resources & Safety Engn, Chongqing 400044, Peoples R China
[3] Natl & Local Joint Engn Res Ctr Hazardous Waste I, Chongqing 401147, Peoples R China
[4] Anhui Univ Technol, Sch Met Engn, Hefei 243002, Anhui, Peoples R China
关键词
Hazardous waste incineration residue; SiO2-Al2O3-Fe2O3-CaO glass-ceramics; Heavy metals; Immobilisation mechanism; ORE PROCESSING RESIDUE; FLY-ASH; BOTTOM ASH; SLAG; CRYSTALLIZATION; VITRIFICATION; DURABILITY; STRENGTH; BEHAVIOR; SODIUM;
D O I
10.1016/j.ceramint.2020.11.213
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Hazardous waste incineration residue (HWIR) is categorised as hazardous waste due to the presence of heavy metals such as Zn, Cu, and Cr. Based on the abundant components of silica, aluminium oxide, iron oxide, and calcium oxide in a HWIR from an environmental protection corporation in China, a 100% HWIR was used to prepare SiO2-Al2O3-Fe2O3-CaO glass-ceramic samples. The results showed that Zn, Cu, and Cr present in the glass-ceramic samples were effectively immobilised through the melting-sintering process. Among the four parameters of heat treatment, crystallisation temperature played the most significant role. The glass-ceramic that was formed under optimal conditions contained haematite, pseudobrookite, and anorthite, and exhibited a superior compressive strength, volume density, and water absorption of 204.84 MPa, 2.80 g/cm(3), and 1.20%, respectively. Compared with the raw HWIR sample, the leaching concentrations of Zn, Cu, and Cr from the prepared glass-ceramic samples decreased significantly, and their immobilisation efficiencies exceeded 99%. Physical encapsulation in the glass-ceramic samples along with ion exchange in the amorphous glassy matrix and iron-rich crystalline phases were the main immobilisation mechanisms of Zn, Cu, and Cr.
引用
收藏
页码:8468 / 8477
页数:10
相关论文
共 55 条
  • [1] Fast-Sintered Gehlenite Glass-Ceramics from Plasma-Vitrified Municipal Solid Waste Incinerator Fly Ashes
    Bernardo, Enrico
    Scarinci, Giovanni
    Edme, Erika
    Michon, Ulysse
    Planty, Nicholas
    [J]. JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2009, 92 (02) : 528 - 530
  • [2] Sinterability, microstructure and compressive strength of porous glass ceramics from metallurgical silicon slag and waste glass
    Cao, Jianwei
    Lu, Jinshan
    Jiang, Longxiang
    Wang, Zhi
    [J]. CERAMICS INTERNATIONAL, 2016, 42 (08) : 10079 - 10084
  • [3] Production of glass-ceramics from incinerator ash using lab-scale and pilot-scale thermal plasma systems
    Cheng, T. W.
    Tu, C. C.
    Ko, M. S.
    Ueng, T. H.
    [J]. CERAMICS INTERNATIONAL, 2011, 37 (07) : 2437 - 2444
  • [4] Characterisation of glass ceramics made from incinerator fly ash
    Cheng, TW
    Chen, YS
    [J]. CERAMICS INTERNATIONAL, 2004, 30 (03) : 343 - 349
  • [5] Effect of Fe2O3 concentration on the structure of the SiO2-Na2O-Al2O3-B2O3 glass system
    Dantas, Noelio O.
    Ayta, Walter E. F.
    Silva, Anielle C. A.
    Cano, Nilo F.
    Silva, Sebastiao W.
    Morais, Paulo C.
    [J]. SPECTROCHIMICA ACTA PART A-MOLECULAR AND BIOMOLECULAR SPECTROSCOPY, 2011, 81 (01) : 140 - 143
  • [6] Additional high-energy milling to enhance the performance of porcelain stoneware manufacturing
    Darolt, Radamez D.
    Cargnin, Maykon
    Peterson, Michael
    De Noni, Agenor, Jr.
    [J]. INTERNATIONAL JOURNAL OF APPLIED CERAMIC TECHNOLOGY, 2020, 17 (04) : 1742 - 1751
  • [7] Processing technologies for sealing glasses and glass-ceramics
    de Pablos-Martin, Araceli
    Rodriguez-Lopez, Sonia
    Pascual, Maria J.
    [J]. INTERNATIONAL JOURNAL OF APPLIED GLASS SCIENCE, 2020, 11 (03) : 552 - 568
  • [8] Chemically Strengthened Low Crystallinity Black Glass-Ceramics with High Liquidus Viscosities
    Dejneka, Matthew
    Dutta, Indrajit
    Smith, Charlene
    [J]. INTERNATIONAL JOURNAL OF APPLIED GLASS SCIENCE, 2014, 5 (02) : 146 - 160
  • [9] Influence of Cr2O3 on the viscosity and crystallization behavior of glass ceramics based on blast furnace slag
    Deng, Leibo
    Jia, Ruidong
    Yun, Fei
    Zhang, Xuefeng
    Li, Hao
    Zhang, Mingxing
    Jia, Xiaolin
    Ren, Da
    Li, Baowei
    [J]. MATERIALS CHEMISTRY AND PHYSICS, 2020, 240
  • [10] Glass-ceramic from mixtures of bottom ash and fly ash
    Dinh Hieu Vu
    Wang, Kuen-Sheng
    Chen, Jung-Hsing
    Bui Xuan Nam
    Bui Hoang Bac
    [J]. WASTE MANAGEMENT, 2012, 32 (12) : 2306 - 2314