An experimental study on the dynamic fracture of extruded AA6xxx and AA7xxx aluminium alloys

被引:48
|
作者
Chen, Y. [1 ]
Pedersen, K. O. [2 ,3 ]
Clausen, A. H. [1 ,3 ]
Hopperstad, O. S. [1 ,3 ]
机构
[1] Norwegian Univ Sci & Technol, Dept Struct Engn, N-7034 Trondheim, Norway
[2] SINTEF Mat & Chem, Trondheim, Norway
[3] Norwegian Univ Sci & Technol, Ctr Res Based Innovat, SIMLab, N-7034 Trondheim, Norway
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2009年 / 523卷 / 1-2期
关键词
Instrumented Charpy tests; Ductile fracture; Intergranular fracture; Transgranular fracture; Precipitate-free zones; DUCTILE FRACTURE; MG ALLOY; BEHAVIOR; TOUGHNESS; STRENGTH; MICROSTRUCTURE; DEFORMATION; FORMABILITY; TEXTURE;
D O I
10.1016/j.msea.2009.06.007
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The dynamic fracture behaviour of extruded AA6xxx and AA7xxx aluminium alloys is investigated using an instrumented Charpy test machine and V-notch specimens. The specimens are made from extruded flat profiles with a rectangular cross-section of 10 mm thickness and 83 mm width. The material is in T6 temper, i.e. the peak hardness condition. The alloys have either recrystallized or fibrous grain structure. For each alloy six different Charpy impact tests are carried out in two series. In Series 1, the notch is parallel to the thickness direction of the profile (i.e. through the thickness), while the notch is perpendicular to the thickness direction in Series 2 (i.e. lying in the plane of the flat profile). In each series, the longitudinal direction of the specimen is parallel, 45 degrees or 90 degrees to the extrusion direction. Comprehensive fractographic investigations are carried out for the different tests and alloys. It is found that the dissipated energy is practically invariant to specimen orientation and notch direction for the recrystallized alloy. For the fibrous alloys the dissipated energy is lower when the longitudinal direction of the specimen is 90, to the extrusion direction, i.e. when the notch is parallel with the fibrous grain structure. Further, the energy dissipation is higher for Series 2 than for Series 1 due to substantial delamination and secondary cracking in Series 2. The precipitate-free zones (PFZs) formed adjacent to the grain boundary are weak areas, preferable for crack initiation and growth. This is seen in the fracture surface as facets with high density of small dimples and is more pronounced for specimens with the notch parallel to the fibre direction. (C) 2009 Elsevier B.V. All rights reserved.
引用
收藏
页码:253 / 262
页数:10
相关论文
共 50 条
  • [1] Influence of pre-compression on the ductility of AA6xxx aluminium alloys
    Frodal, B. H.
    Pedersen, K. O.
    Borvik, T.
    Hopperstad, O. S.
    INTERNATIONAL JOURNAL OF FRACTURE, 2017, 206 (02) : 131 - 149
  • [2] Influence of pre-compression on the ductility of AA6xxx aluminium alloys
    B. H. Frodal
    K. O. Pedersen
    T. Børvik
    O. S. Hopperstad
    International Journal of Fracture, 2017, 206 : 131 - 149
  • [3] Ageing of brazed aluminium AA6xxx alloys for vehicle radiators
    Stenqvist, Torkel
    Bang, Kristoffer
    Kahl, Soren
    Contet, Arnaud
    Karlsson, Oskar
    ALUMINIUM ALLOYS 2014 - ICAA14, 2014, 794-796 : 1239 - +
  • [4] Analysis of AA2XXX/AA7XXX friction stir welds
    Bertrand, Remi
    Robe, Hugo
    Texier, Damien
    Zedan, Yasser
    Feulvarch, Eric
    Bocher, Philippe
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2019, 271 : 312 - 324
  • [5] Correlation of textures and hemming performance of an AA6XXX aluminium alloy
    Zhang, Kai
    He, Qingsheng
    Rao, Jeremy H.
    Wang, Yuan
    Zhang, Ruifeng
    Yuan, Xini
    Feng, Weijun
    Huang, Aijun
    JOURNAL OF ALLOYS AND COMPOUNDS, 2021, 853
  • [6] An Advanced Industrial Methodology for Optimizing the Properties and the Process of Homogenization for Extruded AA2xxx and AA6xxx
    Recnik, Simon
    Medved, Jozef
    Kevorkijan, Varuzan M.
    Zist, Sandi
    LIGHT METALS 2022, 2022, : 228 - 234
  • [7] Experimental analysis and modelling of natural aging in AA7xxx Al alloys
    Abolhasani, Atekeh
    Langelier, Brian
    Worswick, Michael J.
    Wells, Mary A.
    Esmaeili, Shahrzad
    JOURNAL OF ALLOYS AND COMPOUNDS, 2022, 906
  • [8] Phase Composition and Microstructure of High Strength AA6xxx Aluminium Alloys with Nickel Additions
    Shurkin, Pavel
    Scamans, Geoff
    Barekar, Nilam
    Hou, Longgang
    Subroto, Tungky
    Barbatti, Carla
    MATERIALS TRANSACTIONS, 2023, 64 (02) : 398 - 405
  • [9] A thermomechanical process for grain refinement in precipitation hardening AA6xxx aluminum alloys
    Esmaeili, S.
    Lloyd, D. J.
    Jin, H.
    MATERIALS LETTERS, 2011, 65 (06) : 1028 - 1030
  • [10] Material characterisation of anodising effects on small fatigue crack nucleation in AA7XXX alloys
    Main, B.
    Jiang, L.
    Marceau, R. K. W.
    Barter, S.
    MATERIALIA, 2024, 33