On the mechanics of mother-of-pearl: A key feature in the material hierarchical structure

被引:756
作者
Barthelat, F.
Tang, H.
Zavattieri, P. D.
Li, C. -M.
Espinosa, H. D. [1 ]
机构
[1] Northwestern Univ, Dept Mech Engn, Evanston, IL 60208 USA
[2] GM Res & Dev Ctr, Warren, MI 48090 USA
基金
美国国家科学基金会;
关键词
biological material; microstructures; mechanical testing; strengthening and mechanisms; finite elements;
D O I
10.1016/j.jmps.2006.07.007
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Mother-of-pearl, also known as nacre, is the iridescent material which forms the inner layer of seashells from gastropods and bivalves. It is mostly made of microscopic ceramic tablets densely packed and bonded together by a thin layer of biopolymer. The hierarchical microstructure of this biological material is the result of millions of years of evolution, and it is so well organized that its strength and toughness are far superior to the ceramic it is made of. In this work the structure of nacre is described over several length scales. The tablets were found to have wavy surfaces, which were observed and quantified using various experimental techniques. Tensile and shear tests performed on small samples revealed that nacre can withstand relatively large inelastic strains and exhibits strain hardening. In this article we argue that the inelastic mechanism responsible for this behavior is sliding of the tablets on one another accompanied by transverse expansion in the direction perpendicular to the tablet planes. Three dimensional representative volume elements, based on the identified nacre microstructure and incorporating cohesive elements with a constitutive response consistent with the interface material and nanoscale features were numerically analyzed. The simulations revealed that even in the absence of nanoscale hardening mechanism at the interfaces, the microscale waviness of the tablets could generate strain hardening, thereby spreading the inelastic deformation and suppressing damage localization leading to material instability. The formation of large regions of inelastic deformations around cracks and defects in nacre are believed to be an important contribution to its toughness. In addition, it was shown that the tablet junctions (vertical junctions between tablets) strengthen the microstructure but do not contribute to the overall material hardening. Statistical variations within the microstructure were found to be beneficial to hardening and to the overall mechanical stability of nacre. These results provide new insights into the microstructural features that make nacre tough and damage tolerant. Based on these findings, some design guidelines for composites mimicking nacre are proposed. (c) 2006 Elsevier Ltd. All rights reserved.
引用
收藏
页码:306 / 337
页数:32
相关论文
共 36 条
  • [1] BARTHELAT F, 2006, UNPUB MICROSCOPIC OR
  • [2] Mechanical properties of nacre constituents and their impact on mechanical performance
    Barthelat, Francois
    Li, Chun-Ming
    Comi, Claudia
    Espinosa, Horacio D.
    [J]. JOURNAL OF MATERIALS RESEARCH, 2006, 21 (08) : 1977 - 1986
  • [3] The nacre protein perlucin nucleates growth of calcium carbonate crystals
    Blank, S
    Arnoldi, M
    Khoshnavaz, S
    Treccani, L
    Kuntz, M
    Mann, K
    Grathwohl, G
    Fritz, M
    [J]. JOURNAL OF MICROSCOPY-OXFORD, 2003, 212 : 280 - 291
  • [4] Nanoscale morphology and indentation of individual nacre tablets from the gastropod mollusc Trochus niloticus
    Bruet, BJF
    Qi, HJ
    Boyce, MC
    Panas, R
    Tai, K
    Frick, L
    Ortiz, C
    [J]. JOURNAL OF MATERIALS RESEARCH, 2005, 20 (09) : 2400 - 2419
  • [5] Computational modelling of impact damage in brittle materials
    Camacho, GT
    Ortiz, M
    [J]. INTERNATIONAL JOURNAL OF SOLIDS AND STRUCTURES, 1996, 33 (20-22) : 2899 - 2938
  • [6] CURREY JD, 1977, PROC R SOC SER B-BIO, V196, P443, DOI 10.1098/rspb.1977.0050
  • [7] CURREY JD, 1974, J ZOOL, V173, P395
  • [8] A grain level model for the study of failure initiation and evolution in polycrystalline brittle materials. Part I: Theory and numerical implementation
    Espinosa, HD
    Zavattieri, PD
    [J]. MECHANICS OF MATERIALS, 2003, 35 (3-6) : 333 - 364
  • [9] A grain level model for the study of failure initiation and evolution in polycrystalline brittle materials. Part II: Numerical examples
    Espinosa, HD
    Zavattieri, PD
    [J]. MECHANICS OF MATERIALS, 2003, 35 (3-6) : 365 - 394
  • [10] Model for the robust mechanical behavior of nacre
    Evans, AG
    Suo, Z
    Wang, RZ
    Aksay, IA
    He, MY
    Hutchinson, JW
    [J]. JOURNAL OF MATERIALS RESEARCH, 2001, 16 (09) : 2475 - 2484