The Use of Acoustic Emission to Characterize Fracture Behavior During Vickers Indentation of HVOF Thermally Sprayed WC-Co Coatings

被引:18
|
作者
Faisal, N. H. [1 ]
Steel, J. A. [1 ]
Ahmed, R. [1 ]
Reuben, R. L. [1 ]
机构
[1] Heriot Watt Univ, Dept Mech Engn, Sch Engn & Phys Sci, Edinburgh EH14 4AS, Midlothian, Scotland
关键词
acoustic emission; fracture toughness; HVOF; surface crack length; Vickers indentation; WC-12%Co coating; TOUGHNESS EVALUATION; CERMET COATINGS; MICROHARDNESS; RESISTANCE;
D O I
10.1007/s11666-009-9334-1
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
This paper describes how acoustic emission (AE) measurements can be used to supplement the mechanical information available from an indentation test. It examines the extent to which AE data can be used to replace time-consuming surface crack measurement data for the assessment of fracture toughness of brittle materials. AE is known to be sensitive to fracture events and so it was expected that features derived from the AE data may provide information on the processes (microscale and macroscale fracture events and densification) occurring during indentation. AE data were acquired during indentation tests on samples of a WC-12%Co coating of nominal thickness 300 mu m at a variety of indentation loads. The raw AE signals were reduced to three stages and three features per stage, giving nine possible indicators per indentation. Each indicator was compared with the crack profile, measured both conventionally and using a profiling method which gives the total surface crack length around the indent. A selection of the indents was also sectioned in order to make some observations on the subsurface damage. It has been found that reproducible AE signals are generated during indentation involving three distinct stages, associated, respectively, with nonradial cracking, commencement of radial cracking, and continued descent of the indenter. It has been shown that AE can give at least as good a measure of cracking processes during indentation as is possible using crack measurement after indentation.
引用
收藏
页码:525 / 535
页数:11
相关论文
共 50 条
  • [21] Characterization and residual stresses of WC-Co thermally sprayed coatings
    Santana, Y. Y.
    Renault, P. O.
    Sebastiani, M.
    La Barbera, J. G.
    Lesage, J.
    Bemporad, E.
    Le Bourhis, E.
    Puchi-Cabrera, E. S.
    Staia, M. H.
    SURFACE & COATINGS TECHNOLOGY, 2008, 202 (18): : 4560 - 4565
  • [22] The effect of spraying temperature on the corrosion and wear behavior of HVOF thermal sprayed WC-Co coatings
    Azizpour, M. Jalali
    Tolouei-Rad, M.
    CERAMICS INTERNATIONAL, 2019, 45 (11) : 13934 - 13941
  • [23] Elevated temperature wear behavior of thermally sprayed WC-Co/nanodiamond composite coatings
    Nieto, Andy
    Kim, Jaekang
    Penkov, Oleksiy V.
    Kim, Dae-Eun
    Schoenung, Julie M.
    SURFACE & COATINGS TECHNOLOGY, 2017, 315 : 283 - 293
  • [24] Microstructure Characterization and Abrasive Wear Performance of HVOF Sprayed WC-Co Coatings
    Wang, Hongtao
    Ji, Gangchang
    Chen, Qinyu
    Du, Xuefei
    Fu, Wei
    MANUFACTURING PROCESS TECHNOLOGY, PTS 1-5, 2011, 189-193 : 707 - 710
  • [25] Sliding wear behaviour of conventional and nanostructured HVOF sprayed WC-Co coatings
    Shipway, PH
    McCartney, DG
    Sudaprasert, T
    WEAR, 2005, 259 : 820 - 827
  • [26] Improving the performance of HVOF sprayed WC-Co Coatings using Statistical Design
    Wu, Wen-Tung
    Jean, Ming-Der
    Lin, Jeng-Der
    ADVANCED MANUFACTURING TECHNOLOGY, PTS 1-3, 2011, 314-316 : 284 - +
  • [27] Fatigue and deformation of HVOF sprayed WC-Co coatings and hard chrome plating
    Ibrahim, A.
    Berndt, C. C.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2007, 456 (1-2): : 114 - 119
  • [28] Plasma and HVOF sprayed WC-Co coatings as hard chrome replacement solution
    Hazra, S.
    Sabiruddin, K.
    Bandyopadhyay, P. P.
    SURFACE ENGINEERING, 2012, 28 (01) : 37 - 43
  • [29] An improved Vickers indentation fracture toughness model to assess the quality of thermally sprayed coatings
    Faisal, N. H.
    Ahmed, R.
    Prathuru, A. K.
    Spence, S.
    Hossain, M.
    Steel, J. A.
    ENGINEERING FRACTURE MECHANICS, 2014, 128 : 189 - 204
  • [30] Acoustic emission analysis of Vickers indentation fracture of cermet and ceramic coatings
    Faisal, N. H.
    Ahmed, R.
    MEASUREMENT SCIENCE AND TECHNOLOGY, 2011, 22 (12)