The Use of Acoustic Emission to Characterize Fracture Behavior During Vickers Indentation of HVOF Thermally Sprayed WC-Co Coatings

被引:18
|
作者
Faisal, N. H. [1 ]
Steel, J. A. [1 ]
Ahmed, R. [1 ]
Reuben, R. L. [1 ]
机构
[1] Heriot Watt Univ, Dept Mech Engn, Sch Engn & Phys Sci, Edinburgh EH14 4AS, Midlothian, Scotland
关键词
acoustic emission; fracture toughness; HVOF; surface crack length; Vickers indentation; WC-12%Co coating; TOUGHNESS EVALUATION; CERMET COATINGS; MICROHARDNESS; RESISTANCE;
D O I
10.1007/s11666-009-9334-1
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
This paper describes how acoustic emission (AE) measurements can be used to supplement the mechanical information available from an indentation test. It examines the extent to which AE data can be used to replace time-consuming surface crack measurement data for the assessment of fracture toughness of brittle materials. AE is known to be sensitive to fracture events and so it was expected that features derived from the AE data may provide information on the processes (microscale and macroscale fracture events and densification) occurring during indentation. AE data were acquired during indentation tests on samples of a WC-12%Co coating of nominal thickness 300 mu m at a variety of indentation loads. The raw AE signals were reduced to three stages and three features per stage, giving nine possible indicators per indentation. Each indicator was compared with the crack profile, measured both conventionally and using a profiling method which gives the total surface crack length around the indent. A selection of the indents was also sectioned in order to make some observations on the subsurface damage. It has been found that reproducible AE signals are generated during indentation involving three distinct stages, associated, respectively, with nonradial cracking, commencement of radial cracking, and continued descent of the indenter. It has been shown that AE can give at least as good a measure of cracking processes during indentation as is possible using crack measurement after indentation.
引用
收藏
页码:525 / 535
页数:11
相关论文
共 50 条
  • [1] The Use of Acoustic Emission to Characterize Fracture Behavior During Vickers Indentation of HVOF Thermally Sprayed WC-Co Coatings
    N. H. Faisal
    J. A. Steel
    R. Ahmed
    R. L. Reuben
    Journal of Thermal Spray Technology, 2009, 18 : 525 - 535
  • [2] VICKERS INDENTATION FRACTURE TOUGHNESS OF HVOF SPRAYED WC-BASED COATINGS
    Houdkova, Sarka
    Blahova, Olga
    Zahalka, Frantisek
    Kasparova, Michaela
    CHEMICKE LISTY, 2011, 105 : S804 - S805
  • [3] Fatigue cracks in HVOF thermally sprayed WC-Co coatings
    Watanabe, S
    Tajiri, T
    Sakoda, N
    Amano, J
    JOURNAL OF THERMAL SPRAY TECHNOLOGY, 1998, 7 (01) : 93 - 96
  • [4] Fatigue cracks in HVOF thermally sprayed WC-Co coatings
    Watanabe S.
    Amano J.
    Tajiri T.
    Sakoda N.
    Journal of Thermal Spray Technology, 1998, 7 (1) : 93 - 96
  • [5] Fatigue cracks in HVOF thermally sprayed WC-Co coatings
    Watanabe S.
    Tajiri T.
    Sakoda N.
    Amano J.
    Journal of Thermal Spray Technology, 1998, 7 (1) : 93 - 96
  • [6] Effect of heat treatment on wear behavior of HVOF thermally sprayed WC-Co coatings
    Asl, Sh. Khameneh
    Sohi, M. Heydarzadeh
    Hokamoto, K.
    Uemura, M.
    WEAR, 2006, 260 (11-12) : 1203 - 1208
  • [7] Coating fracture toughness determined by Vickers indentation: an important parameter in cavitation erosion resistance of WC-Co thermally sprayed coatings
    Lima, MM
    Godoy, C
    Modenesi, PJ
    Avelar-Batista, JC
    Davison, A
    Matthews, A
    SURFACE & COATINGS TECHNOLOGY, 2004, 177 : 489 - 496
  • [8] Acoustic emission study on WC-Co thermal sprayed coatings
    Miguel, JM
    Guilemany, JM
    Mellor, BG
    Xu, YM
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2003, 352 (1-2): : 55 - 63
  • [9] Fracture Toughness of HVOF Sprayed Cermet Coatings Measured by Vickers Indentation
    Houdkova, Sarka
    Zahalka, Frantisek
    Kasparova, Michaele
    MATERIALS STRUCTURE & MICROMECHANICS OF FRACTURE, 2011, 465 : 475 - 478
  • [10] Machining of thermally sprayed WC-Co coatings
    Zhong, ZW
    MATERIALS AND MANUFACTURING PROCESSES, 2001, 16 (01) : 103 - 112