Insights into the stress corrosion cracking of solution annealed alloy 690 in simulated pressurized water reactor primary water under dynamic straining

被引:80
作者
Kuang, Wenjun [1 ]
Song, Miao [1 ]
Was, Gary S. [1 ]
机构
[1] Univ Michigan, Dept Nucl Engn & Radiol Sci, Ann Arbor, MI 48109 USA
关键词
Nickel alloy; STEM; Grain boundary diffusion; Stress-corrosion cracking; Grain boundary migration; NI-BASE ALLOYS; INTERNAL OXIDATION; INTERGRANULAR OXIDATION; 304-STAINLESS-STEEL; INITIATION; MECHANISM; BEHAVIOR; CR; DIFFUSION; MIGRATION;
D O I
10.1016/j.actamat.2018.04.002
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The intergranular attack near both stagnant and active stress corrosion crack (SCC) tips of solution annealed alloy 690 were characterized after constant extension rate tensile tests in simulated pressurized water reactor (PWR) primary water containing 18cc H-2/kg H2O. In both cracks, an intergranular oxide, composed of NiO and Cr2O3, was observed beyond the crack tip with an adjacent Cr depleted grain boundary migration zone. The stagnant crack has a compact Cr2O3 covering the crack tip and the adjacent grain boundary migration zone is deep and free of oxidation, while the active crack has porous penetrative oxide extending into the migration zone. The ability to form a compact Cr2O3 film at the crack tip is important to the IGSCC resistance and may be dictated by the efficiency of Cr diffusion up the migrated grain boundary. When a compact Cr2O3 film does not form at the crack tip, the Cr depleted grain boundary migration zone is subject to penetrative oxidation via the inward diffusion of oxygen, making the zone susceptible to crack propagation. Thus, even a high Cr content cannot guarantee the immunity of a Ni base alloy to SCC during dynamic straining. (C) 2018 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:321 / 333
页数:13
相关论文
共 61 条
[1]  
Andresen P.L., 2009, 14 INT C ENV DEGR MA
[2]  
Andresen P.L., 2013, P 16 INT C ENV DEGR
[3]   Dependence of Stress Corrosion Cracking of Alloy 690 on Temperature, Cold Work, and Carbide Precipitation-Role of Diffusion of Vacancies at Crack Tips [J].
Arioka, K. ;
Yamada, T. ;
Miyamoto, T. ;
Terachi, T. .
CORROSION, 2011, 67 (03)
[4]   Degradation of Alloy 690 After Relatively Short Times [J].
Arioka, Koji ;
Staehle, Roger W. ;
Yamada, T. ;
Miyamoto, T. ;
Terachi, T. .
CORROSION, 2016, 72 (10) :1252-1268
[5]   MECHANISM FOR DIFFUSION INDUCED GRAIN-BOUNDARY MIGRATION [J].
BALLUFFI, RW ;
CAHN, JW .
ACTA METALLURGICA, 1981, 29 (03) :493-500
[6]   The effect of residual stress on the Preferential Intergranular Oxidation of Alloy 600 [J].
Bertali, G. ;
Scenini, F. ;
Burke, M. G. .
CORROSION SCIENCE, 2016, 111 :494-507
[7]   Pourbaix diagrams for the ternary system of iron-chromium-nickel [J].
Beverskog, B ;
Puigdomenech, I .
CORROSION, 1999, 55 (11) :1077-1087
[8]  
Boursier J., 2003, 11 INT S ENV DEGR MA
[9]  
Bruemmer S. M., 2014, M2LW14OR0404023
[10]  
Bruemmer S. M., 2010, MRS P, V1264