Tailoring electrolyte enables high-voltage Ni-rich NCM cathode against aggressive cathode chemistries for Li-ion batteries

被引:50
作者
Cheng, Fangyuan [1 ]
Zhang, Xiaoyu [1 ]
Wei, Peng [1 ]
Sun, Shixiong [1 ]
Xu, Yue [1 ]
Li, Qing [1 ]
Fang, Chun [1 ]
Han, Jiantao [1 ]
Huang, Yunhui [1 ]
机构
[1] Huazhong Univ Sci & Technol, Sch Mat Sci & Engn, State Key Lab Mat Proc & Die & Mould Technol, Wuhan 430074, Peoples R China
基金
中国国家自然科学基金; 中国博士后科学基金;
关键词
Li-ion batteries; Electrolyte additives; Cathode-electrolyte-interface; High-voltage; Ni-rich NCM; LITHIUM-ION; PERFORMANCE; MECHANISM; DEGRADATION; STABILITY;
D O I
10.1016/j.scib.2022.10.007
中图分类号
O [数理科学和化学]; P [天文学、地球科学]; Q [生物科学]; N [自然科学总论];
学科分类号
07 ; 0710 ; 09 ;
摘要
The LiNi0.8Co0.1Mn0.1O2 (Ni-rich NCM) cathode materials suffer from electrochemical performance degradation upon cycling due to detrimental cathode interface reactions and irreversible surface phase transition when operating at a high voltage (>= 4.5 V). Herein, a traditional carbonate electrolyte with lithium difluoro(oxalato)borate (LiDFOB) and tris(trimethylsilyl)phosphate (TMSP) as dual additives that can preferentially oxidize and decompose to form a stable F, B and Si-rich cathode-electrolyte interphase (CEI) that effectively inhibits continual electrolyte decomposition, transition metal dissolves, surface phase transition and gas generation. In addition, TMSP also removes trace H2O/HF in the electrolyte to increase the electrolyte stability. Owing to the synergistic effect of LiDFOB and TMSP, the Li/ LiNi0.8Co0.1Mn0.1O2 half cells exhibit the capacity retention 76.3% after 500 cycles at a super high voltage of 4.7 V, the graphite/LiNi0.8Co0.1Mn0.1O2 full cells exhibit high capacity retention of 82.8% after 500 cycles at 4.5 V, and Li/LiNi0.8Co0.1Mn0.1O2 pouch cells exhibit high capacity retention 94% after 200 cycles at 4.5 V. This work is expected to provide an effective electrolyte optimizing strategy compatible with high energy density lithium-ion battery manufacturing systems. (c) 2022 Science China Press. Published by Elsevier B.V. and Science China Press. All rights reserved.
引用
收藏
页码:2225 / 2234
页数:10
相关论文
共 46 条
[1]   Future generations of cathode materials: an automotive industry perspective [J].
Andre, Dave ;
Kim, Sung-Jin ;
Lamp, Peter ;
Lux, Simon Franz ;
Maglia, Filippo ;
Paschos, Odysseas ;
Stiaszny, Barbara .
JOURNAL OF MATERIALS CHEMISTRY A, 2015, 3 (13) :6709-6732
[2]   Cross Talk between Transition Metal Cathode and Li Metal Anode: Unraveling Its Influence on the Deposition/Dissolution Behavior and Morphology of Lithium [J].
Betz, Johannes ;
Brinkmann, Jan-Paul ;
Noelle, Roman ;
Luerenbaum, Constantin ;
Kolek, Martin ;
Stan, Marian Cristian ;
Winter, Martin ;
Placke, Tobias .
ADVANCED ENERGY MATERIALS, 2019, 9 (21)
[3]   A Cobalt- and Manganese-Free High-Nickel Layered Oxide Cathode for Long-Life, Safer Lithium-Ion Batteries [J].
Cui, Zehao ;
Xie, Qiang ;
Manthiram, Arumugam .
ADVANCED ENERGY MATERIALS, 2021, 11 (41)
[4]   Ultrasonic Scanning to Observe Wetting and "Unwetting" in Li-Ion Pouch Cells [J].
Deng, Zhe ;
Huang, Zhenyu ;
Shen, Yue ;
Huang, Yunhui ;
Ding, Han ;
Luscombe, Aidan ;
Johnson, Michel ;
Harlow, Jessie E. ;
Gauthier, Roby ;
Dahn, Jeff R. .
JOULE, 2020, 4 (09) :2017-2029
[5]   The Impact of Electrolyte Composition on Parasitic Reactions in Lithium Ion Cells Charged to 4.7 V Determined Using Isothermal Microcalorimetry [J].
Downie, L. E. ;
Hyatt, S. R. ;
Dahn, J. R. .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2016, 163 (02) :A35-A42
[6]   Non-flammable electrolyte enables Li-metal batteries with aggressive cathode chemistries [J].
Fan, Xiulin ;
Chen, Long ;
Borodin, Oleg ;
Ji, Xiao ;
Chen, Ji ;
Hou, Singyuk ;
Deng, Tao ;
Zheng, Jing ;
Yang, Chongyin ;
Liou, Sz-Chian ;
Amine, Khalil ;
Xu, Kang ;
Wang, Chunsheng .
NATURE NANOTECHNOLOGY, 2018, 13 (08) :715-+
[7]   Scavenging Materials to Stabilize LiPF6-Containing Carbonate-Based Electrolytes for Li-Ion Batteries [J].
Han, Jung-Gu ;
Kim, Koeun ;
Lee, Yongwon ;
Choi, Nam-Soon .
ADVANCED MATERIALS, 2019, 31 (20)
[8]   Why is tris(trimethylsilyl) phosphite effective as an additive for high-voltage lithium-ion batteries? [J].
Han, Young-Kyu ;
Yoo, Jaeik ;
Yim, Taeeun .
JOURNAL OF MATERIALS CHEMISTRY A, 2015, 3 (20) :10900-10909
[9]   Multifunctional electrolyte additive for improved interfacial stability in Ni-rich layered oxide full-cells [J].
Hieu Quang Pham ;
Mirolo, Marta ;
Tarik, Mohamed ;
El Kazzi, Mario ;
Trabesinger, Sigita .
ENERGY STORAGE MATERIALS, 2020, 33 :216-229
[10]   Evolution of the Solid-Electrolyte Interphase on Carbonaceous Anodes Visualized by Atomic-Resolution Cryogenic Electron Microscopy [J].
Huang, William ;
Attia, Peter M. ;
Wang, Hansen ;
Renfrew, Sara E. ;
Jin, Norman ;
Das, Supratim ;
Zhang, Zewen ;
Boyle, David T. ;
Li, Yuzhang ;
Bazant, Martin Z. ;
McCloskey, Bryan D. ;
Chueh, William C. ;
Cui, Yi .
NANO LETTERS, 2019, 19 (08) :5140-5148