Amorphous silicon nitride deposited by hot-wire chemical vapor deposition

被引:26
作者
Liu, FZ
Ward, S
Gedvilas, L
Keyes, B
To, B
Wang, Q
Sanchez, E
Wang, SL
机构
[1] Natl Renewable Energy Lab, Golden, CO 80401 USA
[2] Appl Mat Inc, Sunnyvale, CA 94086 USA
关键词
D O I
10.1063/1.1775046
中图分类号
O59 [应用物理学];
学科分类号
摘要
High-quality amorphous silicon nitrides were deposited by hot-wire chemical vapor deposition using SiH4, NH3, and H-2 gases. These films show a high deposition rate of 5 Angstrom/s, a low processing temperature of 300 degreesC, an excellent conformal coverage, a low etching rate of 7 Angstrom/min, an index of refraction of 2.1, an optical band gap of 4.0 eV, and a high breakdown field of 3 MV/cm. The effects of hydrogen dilution, substrate temperature, chamber pressure, and filament temperature on silicon nitride film property were studied to optimize the process. We found that adding H-2 to the processing significantly enhances the silicon nitride films' properties. The N content in the film increased significantly based on the infrared measurement. Hydrogen dilution is believed to play a key role for the conformal silicon nitride film. Hydrogen dilution also improves the process in that the gas ratio of NH3/SiH4 has been greatly reduced with the assistance of the H-2 gas. With substrate temperatures varying from 23degrees to 400 degreesC, this study showed a best film at near 300 degreesC. However, a good-quality silicon nitride can be grown even if starting with a substrate at room temperature. Furthermore, we found that increasing chamber pressure and a high filament temperature result in higher deposition rate and better quality in the films. The optimized films were grown with hydrogen dilution at about 300 degreesC substrate temperature, 83 mTorr pressure, and 2100 degreesC filament temperature. (C) 2004 American Institute of Physics.
引用
收藏
页码:2973 / 2979
页数:7
相关论文
共 28 条
[1]   Characteristics of low-temperature silicon nitride (SiNx:H) using electron cyclotron resonance plasma [J].
Bae, S ;
Farber, DG ;
Fonash, SJ .
SOLID-STATE ELECTRONICS, 2000, 44 (08) :1355-1360
[2]   EFFECT OF THERMAL-TREATMENT OF PASSIVATION INTEGRITY OF CHEMICAL VAPOR-DEPOSITION SILICON-NITRIDE [J].
DOMANSKY, K ;
PETELENZ, D ;
JANATA, J .
APPLIED PHYSICS LETTERS, 1992, 60 (17) :2074-2076
[3]   Hot-wire chemical vapor deposition of high hydrogen content silicon nitride for solar cell passivation and anti-reflection coating applications [J].
Holt, JK ;
Goodwin, DG ;
Gabor, AM ;
Jiang, F ;
Stavola, M ;
Atwater, HA .
THIN SOLID FILMS, 2003, 430 (1-2) :37-40
[4]   Hydrogenation of defects in edge-defined film-fed grown aluminum-enhanced plasma enhanced chemical vapor deposited silicon nitride multicrystalline silicon [J].
Jeong, JW ;
Rosenblum, MD ;
Kalejs, JP ;
Rohatgi, A .
JOURNAL OF APPLIED PHYSICS, 2000, 87 (10) :7551-7557
[5]   Surface recombination velocity of phosphorus-diffused silicon solar cell emitters passivated with plasma enhanced chemical vapor deposited silicon nitride and thermal silicon oxide [J].
Kerr, MJ ;
Schmidt, J ;
Cuevas, A ;
Bultman, JH .
JOURNAL OF APPLIED PHYSICS, 2001, 89 (07) :3821-3826
[6]   CHEMICAL EFFECTS ON THE FREQUENCIES OF SI-H VIBRATIONS IN AMORPHOUS SOLIDS [J].
LUCOVSKY, G .
SOLID STATE COMMUNICATIONS, 1979, 29 (08) :571-576
[7]   Properties of thin film silicon nitride deposited by hot wire chemical vapor deposition using silane, ammonia, and hydrogen gas mixtures [J].
Mahan, AH ;
Dillon, AC ;
Gedvilas, LM ;
Williamson, DL ;
Perkins, JD .
JOURNAL OF APPLIED PHYSICS, 2003, 94 (04) :2360-2367
[8]   DEPOSITION OF DEVICE QUALITY, LOW H CONTENT A-SI-H BY THE HOT-WIRE TECHNIQUE [J].
MAHAN, AH ;
NELSON, BP ;
SALAMON, S ;
CRANDALL, RS .
JOURNAL OF NON-CRYSTALLINE SOLIDS, 1991, 137 :657-660
[9]  
Masuda A, 2002, MATER RES SOC SYMP P, V715, P111
[10]   SILICON-NITRIDE PRODUCED BY CATALYTIC CHEMICAL VAPOR-DEPOSITION METHOD [J].
MATSUMURA, H .
JOURNAL OF APPLIED PHYSICS, 1989, 66 (08) :3612-3617