Ba2+Co-doped Zn2SiO4: Mn phosphor particles prepared by spray pyrolysis process

被引:40
作者
Kang, YC [1 ]
Lim, MA
Park, HD
Han, M
机构
[1] Korea Res Inst Chem Technol, Adv Mat Div, Yusung Gu 305600, Daejeon, South Korea
[2] Chungnam Natl Univ, Dept Chem Engn, Taejon 305764, South Korea
关键词
D O I
10.1149/1.1523416
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
Green-emitting Zn2SiO4:Mn phosphor particles having a spherical shape, high brightness, and short decay time were prepared by large-scale spray pyrolysis. The morphological control was attempted by using artificial colloidal solution obtained by adding the fumed silica particles to the aqueous solution. The particles prepared from the colloidal solution had a spherical and filled morphology even after post-treatment. To reduce the decay time of Zn2SiO4:Mn particles prepared by spray pyrolysis, barium was introduced as a codoping material. The effects of barium codopant concentration on the crystal structure, morphology, and luminescence properties such as luminescence intensity and decay time of Zn2SiO4:Mn particles were investigated. Zn2SiO4:Mn phosphor particles containing 0.1 mol % of barium codopant had a higher photoluminescence (PL) intensity and shorter decay time than the nonco-doped ones. The influence of post-treatment temperature on the decay time and PL intensities of Zn2SiO4:Mn particles was also investigated. The particles post-treated at 1145degreesC had the maximum PL intensity, which was 107% of that of the commercial product. Although the decay time of the optimized particles was similar to that of the commercial product (5.5 ms), that of prepared particles tended to be short with increasing post- treatment temperature. (Minimum decay time obtained was 4.5 ms.) (C) 2002 The Electrochemical Society.
引用
收藏
页码:H7 / H11
页数:5
相关论文
共 16 条
  • [1] MN-2+ CONCENTRATION-EFFECT ON THE OPTICAL-PROPERTIES OF ZN2SIO4MN PHOSPHORS
    BARTHOU, C
    BENOIT, J
    BENALLOUL, P
    MORELL, A
    [J]. JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1994, 141 (02) : 524 - 528
  • [2] REFINEMENT OF ZINC SILICATE PHOSPHOR SYNTHESIS
    CHANG, IF
    BROWNLOW, JW
    SUN, TI
    WILSON, JS
    [J]. JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1989, 136 (11) : 3532 - 3536
  • [3] Zn2SiO4:Mn phosphor particles prepared by spray pyrolysis using a filter expansion aerosol generator
    Kang, YC
    Park, SB
    [J]. MATERIALS RESEARCH BULLETIN, 2000, 35 (07) : 1143 - 1151
  • [4] Kang YC., 2001, J. Inf. Disp, V2, P57, DOI [10.1080/15980316.2018.12035738, DOI 10.1080/15980316.2018.12035738]
  • [5] KOIKE J, 1997, 3 INT C SCI TECHN DI, P13
  • [6] One-step synthesis for Zn2SiO4:Mn particles 0.3-1.3 μm in size with spherical morphology and non-aggregation
    Lenggoro, IW
    Iskandar, F
    Mizushima, H
    Xia, B
    Okuyama, K
    Kijima, N
    [J]. JAPANESE JOURNAL OF APPLIED PHYSICS PART 2-LETTERS, 2000, 39 (10B): : L1051 - L1053
  • [7] CONTROL OF MORPHOLOGY OF ZN2SIO4 BY HYDROTHERMAL PREPARATION
    LI, QH
    KOMARNENI, S
    ROY, R
    [J]. JOURNAL OF MATERIALS SCIENCE, 1995, 30 (09) : 2358 - 2363
  • [8] Li QH, 1997, 3 INT C SCI TECHN DI, P21
  • [9] Gd2O3:Eu phosphor particles prepared from the polymeric precursors in spray pyrolysis
    Lim, MA
    Kang, YC
    Park, HD
    [J]. JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2001, 148 (12) : H171 - H175
  • [10] GREEN PHOSPHORS FOR LARGE PLASMA TV SCREENS
    MORELL, A
    ELKHIATI, N
    [J]. JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1993, 140 (07) : 2019 - 2022