The Fracture Toughness and Toughening Mechanism of Commercially Available Unalloyed Molybdenum and Oxide Dispersion Strengthened Molybdenum with an Equiaxed, Large Grain Structure

被引:66
作者
Cockeram, B. V. [1 ]
机构
[1] Bechtel Bettis Atom Power Lab, W Mifflin, PA 15025 USA
来源
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE | 2009年 / 40A卷 / 12期
基金
美国能源部;
关键词
CARBON ARC-CAST; TITANIUM-0.1 PCT ZIRCONIUM; REFRACTORY-METAL ALLOYS; FE-X ALLOYS; POLYCRYSTALLINE MOLYBDENUM; HARDENING MATERIAL; FLAT PRODUCTS; MICROSTRUCTURE; DUCTILITY; BEHAVIOR;
D O I
10.1007/s11661-009-9919-9
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Commercially available molybdenum and oxide dispersion strengthened (ODS) molybdenum produced by powder metallurgy (PM) methods were subjected to tensile testing, fracture toughness testing, and examination of the toughening mechanism. Both PM and ODS molybdenum have an equiaxed grain size that is larger in scale than comparable wrought products. This results in lower tensile strength and a higher tensile ductile-to-brittle transition temperature (DBTT) for PM and ODS molybdenum compared to wrought product forms. Although the grain size for PM molybdenum is large and the oxygen content is relatively high, both attributes tending to embrittle molybdenum, the transition temperature and fracture toughness values are comparable to those observed for wrought molybdenum. Crack initiation at grain boundaries and the center of grains where pores are present were observed to leave ligaments for the PM molybdenum that are similar in scale to those observed for wrought molybdenum. This is a similar toughening mechanism to the ductile laminate mechanism observed for wrought molybdenum. The larger oxide particle size for PM ODS molybdenum produces larger cracks that result in lower fracture toughness values and a higher DBTT in comparison to PM molybdenum. The impact of the grain size, grain shape, and oxide particles on the toughening mechanism and resulting properties is discussed.
引用
收藏
页码:2843 / 2860
页数:18
相关论文
共 57 条
  • [21] Ductility and fracture toughness of molybdenum with MgAl2O4 additions
    Gunter, I. M.
    Schneibel, J. H.
    Kruzic, J. J.
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2007, 458 (1-2): : 275 - 280
  • [22] Hertzberg R.W., 1983, Deformation and Fracture Mechanics of Engineering Materials, VII, P269
  • [24] JIUXING Z, 1999, INT J REFRACT MET H, V17, P405
  • [25] FRACTURE MODE TRANSITION IN POLYCRYSTALLINE MOLYBDENUM
    JOHNSON, AA
    GUPTA, SP
    KODALI, SP
    [J]. MATERIALS SCIENCE AND ENGINEERING, 1975, 18 (01): : 159 - 161
  • [26] REVIEW OF CHROMIUM, MOLYBDENUM, AND TUNGSTEN ALLOYS
    KLOPP, WD
    [J]. JOURNAL OF THE LESS-COMMON METALS, 1975, 42 (03): : 261 - 278
  • [27] Fracture toughness of molybdenum sheet under brittle-ductile transition
    Koval, AY
    Vasilev, AD
    Firstov, SA
    [J]. INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 1997, 15 (04) : 223 - 226
  • [28] Ambient- to elevated-temperature fracture and fatigue properties of Mo-Si-B alloys: Role of microstructure
    Kruzic, JJ
    Schneibel, JH
    Ritchie, RO
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2005, 36A (09): : 2393 - 2402
  • [29] GRAIN-BOUNDARY SEGREGATION AND INTERGRANULAR FRACTURE IN MOLYBDENUM
    KUMAR, A
    EYRE, BL
    [J]. PROCEEDINGS OF THE ROYAL SOCIETY OF LONDON SERIES A-MATHEMATICAL AND PHYSICAL SCIENCES, 1980, 370 (1743) : 431 - 458
  • [30] GRAIN-BOUNDARY FRACTURE IN MOLYBDENUM BICRYSTALS WITH VARIOUS (110) SYMMETRIC TILT BOUNDARIES
    KURISHITA, H
    OISHI, A
    KUBO, H
    YOSHINAGA, H
    [J]. TRANSACTIONS OF THE JAPAN INSTITUTE OF METALS, 1985, 26 (05): : 341 - 352