Performance improvement of a two-stage GM cryocooler by use of Er(Ni0.075Co0.925)2 magnetic regenerator material

被引:18
作者
Trevisani, L
Kuriyama, T
Negrini, F
Okamura, T
Ohtani, Y
Okamura, M
Fabbri, M
机构
[1] Univ Bologna, Dept Elect Engn, I-40136 Bologna, Italy
[2] Toshiba Co Ltd, Power & Ind Syst Res & Dev Ctr, Yokohama, Kanagawa 2300045, Japan
[3] Tokyo Inst Technol, Dept Energy Sci, Yokohama, Kanagawa 2268502, Japan
[4] Toshiba Co Ltd, Mat & Components Dev Dept, Yokohama, Kanagawa 2350032, Japan
关键词
GM cryocooler; regenerator; magnetic regenerator material;
D O I
10.1016/S0011-2275(02)00101-7
中图分类号
O414.1 [热力学];
学科分类号
摘要
A newly developed magnetic regenerator material Er(Ni0.075Co0.925)(2), having high specific heat at temperatures from 10 to 20 K, has been tested inside the second regenerator of a two-stage GM cryocooler. Different working conditions have been examined: four Er(Ni0.075Co0.925)(2)/Pb material ratios, three displacer reciprocating speeds, and two cryocooler stroke lengths. In the best working conditions, the experimental results show a cooling power improvement up to 15% over the whole temperature range from 10 to 20 K compared to that of the same GM cryocooler employing only lead. (C) 2002 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:653 / 657
页数:5
相关论文
共 5 条
[1]  
ACKERMAN RA, 1997, CRYOGENIC REGENERATI, P148
[2]  
KE G, 1994, ADV CRYOG ENG, V40, P639
[3]  
Kuriyama T, 1990, Adv Cryog Eng, V35, P1261, DOI [10.1007/978-1-4613-0639-9_150, DOI 10.1007/978-1-4613-0639-9_150]
[4]  
Satoh T, 1996, ADV CRYOG ENG, P1631
[5]  
WALKER G, 1983, CRYOCOOLERS 2, P33