Microstructure and dielectric properties of CCTO glass-ceramic prepared by the melt-quenching method

被引:11
作者
Aliabadi, Tahere Nazari [1 ]
Alizadeh, Parvin [1 ]
机构
[1] Tarbiat Modares Univ, Dept Mat Sci & Engn, Tehran 14115143, Iran
关键词
Glass; Glass-ceramic; CaCu3Ti4O12; Dielectric properties; ENERGY-STORAGE PROPERTIES; CACU3TI4O12; CERAMICS; CRYSTALLIZATION BEHAVIOR; SIO2-PBO-CAO-ZRO2-TIO2-(B2O3-K2O); IMPROVEMENT; CONSTANT; DENSITY; GROWTH;
D O I
10.1016/j.ceramint.2019.06.182
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In this work, CaCu3Ti4O12 (CCTO) glass-ceramic was prepared by using the melt-quenching method followed by a two-step heat treatment. The prepared glass frits with the chemical composition of 24SiO(2)-65PbO-3K(2)O-7B(2)O(3)-1ZnO (wt. %) were mixed with 32, 34 and 38 wt % of CCTO including 14.03 CaO-29.66 CuO-56.31 TiO2 (wt. %) and melted at 1070-1090 degrees C. The glass with 32 wt % of CCTO, which was XRD amorphous, was selected as the final composition. The heat treatment conditions were found to be 6 and 2 h at 468 degrees C and 830 degrees C, respectively. The faceted crystals of CCTO, two solid-solution of (Pb1-xCax)TiO3, and CaTiO(SiO4) were formed in the glassy matrix during the crystallization based on the studies related to XRD, SEM, EDS, and elemental mapping in the glass-ceramic. The measured dielectric constant of the glass was 16.3 at 1 MHz, which reached 41.2 after the heat treatment process, and the value of the tans increased from 4.6x10(-5) to 0.012.
引用
收藏
页码:19316 / 19322
页数:7
相关论文
共 43 条
[1]   A Short Review on Copper Calcium Titanate (CCTO) Electroceramic: Synthesis, Dielectric Properties, Film Deposition, and Sensing Application [J].
Ahmadipour, Mohsen ;
Ain, Mohd Fadzil ;
Ahmad, Zainal Arifin .
NANO-MICRO LETTERS, 2016, 8 (04) :291-311
[2]  
[Anonymous], J AM CERAM SOC
[3]  
[Anonymous], J MYANMAR ACAD ARTS
[4]   The dielectric properties of the rutile form of T1O2 [J].
Berberich, LJ ;
Bell, ME .
JOURNAL OF APPLIED PHYSICS, 1940, 11 (10) :681-692
[5]   Control of grain boundary in alumina doped CCTO showing colossal permittivity by core-shell approach [J].
De Almeida-Didry, Sonia ;
Nomel, Meledje Martin ;
Autret, Cecile ;
Honstettre, Christophe ;
Lucas, Anthony ;
Pacreau, Francois ;
Gervais, Francois .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2018, 38 (09) :3182-3187
[6]   Co-doping effects of A-site Y3+ and B-site Al3+ on the microstructures and dielectric properties of CaCu3Ti4O12 ceramics [J].
Du, Guoping ;
Wei, Fangbin ;
Li, Wang ;
Chen, Nan .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2017, 37 (15) :4653-4659
[7]   The role of PbO on crystallization in PbO-SrO-TiO2-SiO2 glass [J].
Duan, Fei .
JOURNAL OF NON-CRYSTALLINE SOLIDS, 2010, 356 (43) :2286-2288
[8]   Density, surface tension, and viscosity of PbO-B2O3-SiO2 glass melts [J].
Fujino, S ;
Hwang, CW ;
Morinaga, K .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2004, 87 (01) :10-16
[9]   Low temperature sintering of CCTO using P2O5 as a sintering aid [J].
Goswami, Sudipta ;
Sen, A. .
CERAMICS INTERNATIONAL, 2010, 36 (05) :1629-1631
[10]   A review on the dielectric materials for high energy-storage application [J].
Hao, Xihong .
JOURNAL OF ADVANCED DIELECTRICS, 2013, 3 (01)