Benchmarks for finite element analysis of creep continuum damage mechanics

被引:64
作者
Becker, AA
Hyde, TH
Sun, W
Andersson, P
机构
[1] Univ Nottingham, Sch Mech Mat Mfg Engn & Management, Nottingham NG7 2RD, England
[2] SAQ Kontroll AB Technol, SE-10029 Stockholm, Sweden
关键词
creep; finite element analysis; continuum damage mechanics;
D O I
10.1016/S0927-0256(02)00247-1
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Creep rupture life can be predicted using a continuum damage mechanics approach incorporated within a finite element (FE) formulation. The rate of change of a damage parameter, omega, ranging from omega = 0 (no damage) to omega = 1 (100% damage), is computed within each element, until failure occurs in the material cross-section. The main difficulty in the numerical formulation arises due to the very small time steps needed as the damage parameter increases to 1. This paper presents the results of a number of benchmark tests involving the FE analysis of creep continuum damage mechanics that can be used to verify the FE solutions. Two independent FE codes are used; an in-house code (FE-DAMAGE) and a commercial code (ABAQUS) in which a user-subroutine (UMAT) is incorporated. The results of a series of tests used to represent uniaxial, biaxial, triaxial and multi-material creep and damage behaviour are presented. (C) 2002 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:34 / 41
页数:8
相关论文
共 17 条
[1]  
[Anonymous], 1980, CREEP ANAL
[2]  
Becker A. A., 1994, FE DAMAGE USERS MANU
[3]   NUMERICAL-ANALYSIS OF CREEP IN COMPONENTS [J].
BECKER, AA ;
HYDE, TH ;
XIA, L .
JOURNAL OF STRAIN ANALYSIS FOR ENGINEERING DESIGN, 1994, 29 (03) :185-192
[4]  
BECKER AA, 1993, R0027 NAFEMS
[5]  
BECKER AA, 1999, R0065 NAFEMS, V5
[6]   CONTINUUM DAMAGE MECHANICS .1. GENERAL CONCEPTS [J].
CHABOCHE, JL .
JOURNAL OF APPLIED MECHANICS-TRANSACTIONS OF THE ASME, 1988, 55 (01) :59-64
[7]  
CHAMBERS AC, 1993, CREEP AND FRACTURE OF ENGINEERING MATERIALS AND STRUCTURES, P421
[8]   CONTINUUM DAMAGE MECHANICS MODELING OF HIGH-TEMPERATURE DEFORMATION AND FAILURE IN A PIPE WELDMENT [J].
HALL, FR ;
HAYHURST, DR .
PROCEEDINGS OF THE ROYAL SOCIETY OF LONDON SERIES A-MATHEMATICAL PHYSICAL AND ENGINEERING SCIENCES, 1991, 433 (1888) :383-403
[9]  
HINTON E, 1987, P06 NAFEMS
[10]   Creep continuum damage constitutive equations for the base, weld and heat-affected zone materials of a service-aged 1/2Cr1/2Mo1/4V:21/4Cr1Mo multipass weld at 640 degrees C [J].
Hyde, TH ;
Sun, W ;
Becker, AA ;
Williams, JA .
JOURNAL OF STRAIN ANALYSIS FOR ENGINEERING DESIGN, 1997, 32 (04) :273-285