Assessment of geopolymer composites durability at one year age

被引:64
作者
Aygormez, Yurdakul [1 ]
Canpolat, Orhan [1 ]
Al-mashhadani, Mukhallad M. [2 ]
机构
[1] Yildiz Tech Univ, Civil Engn Dept, Davutpasa Campus, Istanbul, Turkey
[2] Istanbul Gelisim Univ, Civil Engn Dept, Avcilar Campus, Istanbul, Turkey
来源
JOURNAL OF BUILDING ENGINEERING | 2020年 / 32卷
关键词
Geopolymer; Colemanite; Metakaolin; Freezing-thawing; Hydrochloric acid; ASH-BASED GEOPOLYMER; CEMENT-BASED MATERIALS; FREEZE-THAW RESISTANCE; FLY-ASH; ACID ATTACK; SLAG CONCRETE; SILICA FUME; METAKAOLIN; BEHAVIOR; WASTE;
D O I
10.1016/j.jobe.2020.101453
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
Geopolymers are important alternative materials for use in support of recycling and sustainability, and one of the most important properties is durability. While many studies perform durability tests 28 days after production, we carried out durability tests on a mixture of geopolymers starting 365 days after production. In this case, other conditions that occur until durability conditions are applied are taken into consideration. The geopolymer mixture consisted of metakaolin (90% by wt.) and boron waste colemanite (10% by wt.). The study investigated heat and wet-dry curing methods and polyolefin and polyamide fibre ratios (0.5, 1.0, and 1.5% by vol.) on durability. Durability issues related to concrete, such as long-term exposure to hydrochloric acid, freeze-thaw cycles, and abrasion were recorded. Results show that polyamide fibres provide better results than polyolefin fibres, the optimum polyamide fibre ratio was 1%, and the wet-dry curing method increased geopolymerisation more than heat curing. The Si-O-Al bonds were found to be stronger after wet-dry curing. All durability studies showed that the compact structure of the geopolymers withstood the durability tests performed one year after production. Scanning electron microscopy (SEM) analysis supports these results.
引用
收藏
页数:9
相关论文
共 54 条
  • [1] Chemical durability of superabsorbent polymer (SAP) based geopolymer mortars (GPMs)
    Afridi, Suleman
    Sikandar, Muhammad Ali
    Waseem, Muhammad
    Nasir, Hasan
    Naseer, Amjad
    [J]. CONSTRUCTION AND BUILDING MATERIALS, 2019, 217 : 530 - 542
  • [2] Mechanical and microstructural characterization of fiber reinforced fly ash based geopolymer composites
    Al-mashhadani, Mukhallad M.
    Canpolat, Orhan
    Aygormez, Yurdakul
    Uysal, Mucteba
    Erdem, Savas
    [J]. CONSTRUCTION AND BUILDING MATERIALS, 2018, 167 : 505 - 513
  • [3] Durability evaluation of geopolymer and conventional concretes
    Albitar, M.
    Ali, M. S. Mohamed
    Visintin, P.
    Drechsler, M.
    [J]. CONSTRUCTION AND BUILDING MATERIALS, 2017, 136 : 374 - 385
  • [4] Alexander M., 2013, PERFORMANCE CEMENT B, V10, P462
  • [5] Resistance of chemically-activated high phosphorous slag content cement against freeze-thaw cycles
    Allahverdi, Ali
    Abadi, Mohammad Mandi Bahri Rasht
    Hossain, Khandaker M. Anwar
    Lachemi, Mohamed
    [J]. COLD REGIONS SCIENCE AND TECHNOLOGY, 2014, 103 : 107 - 114
  • [6] Effectiveness of surface coatings in improving concrete durability
    Almusallam, AA
    Khan, FM
    Dulaijan, SU
    Al-Amoudi, OSB
    [J]. CEMENT & CONCRETE COMPOSITES, 2003, 25 (4-5) : 473 - 481
  • [7] Alkaline activation of metakaolin and calcium hydroxide mixtures: influence of temperature, activator concentration and solids ratio
    Alonso, S
    Palomo, A
    [J]. MATERIALS LETTERS, 2001, 47 (1-2) : 55 - 62
  • [8] [Anonymous], 1994, 1 INT C ALK CEM CONC
  • [9] [Anonymous], 2018, 4 INT C GREEN DES MA
  • [10] [Anonymous], 2016, STANDARD TEST METHOD, P1