Role of compression direction on recrystallization behavior and texture evolution during hot deformation of extruded ZK60 magnesium alloy

被引:75
作者
Hadadzadeh, Amir [1 ]
Wells, Mary A. [1 ]
Shaha, Sugrib Kumar [1 ]
Jahed, Hamid [1 ]
Williams, Bruce W. [2 ]
机构
[1] Univ Waterloo, Mech & Mechatron Engn Dept, 200 Univ Ave West, Waterloo, ON N2L 3G1, Canada
[2] Nat Resources Canada, 183 Longwood Rd South,2nd Floor,Room 223A, Hamilton, ON L8P 0A5, Canada
基金
加拿大自然科学与工程研究理事会;
关键词
ZK60 magnesium alloy; Extruded rod; Texture; Microstructure; Hot deformation; MECHANICAL-PROPERTIES; DYNAMIC RECRYSTALLIZATION; PROCESSING MAPS; MICROSTRUCTURAL EVOLUTION; TEMPERATURE DEFORMATION; PLASTIC-DEFORMATION; HEAT-TREATMENT; STRAIN-RATE; MG ALLOY; AZ31;
D O I
10.1016/j.jallcom.2017.01.236
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Hot deformation behavior of as-extruded ZK60 magnesium alloy was investigated using uniaxial hot compression tests over the temperature range of 300-450 degrees C under strain rates of 0.001-1.0 s(-1) using a Gleeble((R)) 3500 available at the University of Waterloo. In order to take in account the effect of initial texture and microstructure on the hot deformation behavior of the alloy, compression tests were conducted in both the extrusion and radial directions (designated as ED and RD, respectively). The as received alloy exhibited an inhomogeneous microstructure featured by unrecrystallized elongated grains stretched along the extrusion direction, surrounded by equiaxed grains, with a typical fiber texture. Visual observation of the hot compressed samples showed that deformation along the radial direction led to pronounced anisotropic flow which reduced by increasing the deformation temperature or decreasing the strain rate. Processing maps determined from the compression tests predicted possible dynamic recrystallization (DRX) for both directions, specifically over the temperature regime of 400-450 degrees C which was confirmed by microstructural studies. It was observed that DRX grain size for both deformation directions is very close under identical deformation conditions; however, the final texture was strongly dependent on the deformation direction. While a weak and close to random texture was developed after deformation along the extrusion direction (ED), RD samples exhibited either similar texture to, the starting texture or a sharper texture. Such a behavior was attributed to the initial texture and DRX mechanism. (C) 2017 Published by Elsevier B.V.
引用
收藏
页码:274 / 289
页数:16
相关论文
共 74 条
[1]   Crystallographic texture evolution of three wrought magnesium alloys during equal channel angular extrusion [J].
Agnew, SR ;
Mehrotra, P ;
Lillo, TM ;
Stoica, GM ;
Liaw, PK .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2005, 408 (1-2) :72-78
[2]   Plastic anisotropy and the role of non-basal slip in magnesium alloy AZ31B [J].
Agnew, SR ;
Duygulu, Ö .
INTERNATIONAL JOURNAL OF PLASTICITY, 2005, 21 (06) :1161-1193
[3]   Texture evolution of five wrought magnesium alloys during route A equal channel angular extrusion: Experiments and simulations [J].
Agnew, SR ;
Mehrotra, P ;
Lillo, TM ;
Stoica, GM ;
Liaw, PK .
ACTA MATERIALIA, 2005, 53 (11) :3135-3146
[4]   Dynamic recrystallization during high temperature deformation of magnesium [J].
Al-Samman, T. ;
Gottstein, G. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2008, 490 (1-2) :411-420
[5]   Deformation conditions and stability of the basal texture in magnesium [J].
Al-Samman, Talal ;
Gottstein, Guenter .
THERMEC 2006, PTS 1-5, 2007, 539-543 :3401-+
[6]   Hot deformation and processing maps of extruded ZE41A magnesium alloy [J].
Anbuselvan, S. ;
Ramanathan, S. .
MATERIALS & DESIGN, 2010, 31 (05) :2319-2323
[7]  
[Anonymous], 2013, E11213 ASTM INT
[8]   Influence of grain size on the compressive deformation of wrought Mg-3Al-1Zn [J].
Barnett, MR ;
Keshavarz, Z ;
Beer, AG ;
Atwell, D .
ACTA MATERIALIA, 2004, 52 (17) :5093-5103
[9]   A critical analysis of plastic flow behaviour in axisymmetric isothermal and Gleeble compression testing [J].
Bennett, C. J. ;
Leen, S. B. ;
Williams, E. J. ;
Shipway, P. H. ;
Hyde, T. H. .
COMPUTATIONAL MATERIALS SCIENCE, 2010, 50 (01) :125-137
[10]   Low cycle fatigue and mechanical properties of magnesium alloy Mg-6Zn-1Y-0.6Ce-0.6Zr at different temperatures [J].
Canadija, Marko ;
Guo, Xuefeng ;
Lanc, Domagoj ;
Yang, Wenpeng ;
Brnic, Josip .
MATERIALS & DESIGN, 2014, 59 :287-295