The effect of thermal cycling on metal-ceramic bond strength

被引:34
|
作者
Fischer, Jens [1 ]
Zbaeren, Christoph [1 ]
Stawarczyk, Bogna [1 ]
Haemmerle, Christoph H. F. [1 ]
机构
[1] Univ Zurich, Clin Fixed & Removable Prosthodont & Dent Mat Sci, Ctr Dent & Oral Med, CH-8032 Zurich, Switzerland
关键词
Metal-ceramic technique; Metal-ceramic bond strength; Dental alloys; Crack initiation test; Thermal cycling; OF-THE-LITERATURE; LEAST; 3; YEARS; COMPLICATION RATES; OBSERVATION PERIOD; FLEXURAL STRENGTH; IN-VITRO; PORCELAIN; TITANIUM; GOLD; SYSTEMS;
D O I
10.1016/j.jdent.2009.03.014
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objectives: The aim was to evaluate the effect of thermal cycling on the metal-ceramic bond strength. Methods: Four different noble metal alloys were used. Specimens for the crack initiation test according to ISO 9693 were prepared to assess metal-ceramic bond strength (n = 10). The metal substrates were either air-borne particle abraded or polished prior to veneering. Bond strength was measured after veneering or after 6000 thermal cycles. With one alloy in addition long-term thermal cycling with 15,000 and 50,000 cycles was carried out. Statistical analysis was performed with one-way ANOVA followed by a post hoc Bonferroni test. Results: Polished metal substrates showed a significantly lower bond strength compared to the air-borne particle abraded substrates. Treatment with 6000 thermal cycles did not significantly reduce the bond strength. Long-term thermal cycling resulted in an exponential decrease of bond strength for both polished and air-borne particle abraded specimens. Conclusions: Air-borne particle abrasion significantly increases metal-ceramic bond strength. Thermal cycling of metal-ceramic composites results in an exponential decrease of bond strength. The crack initiation test is a sensitive method for assessing the metal-ceramic bond strength. (C) 2009 Elsevier Ltd. All rights reserved.
引用
收藏
页码:549 / 553
页数:5
相关论文
共 50 条
  • [1] CORRELATION BETWEEN METAL-CERAMIC BOND STRENGTH AND COEFFICIENT OF LINEAR THERMAL EXPANSION DIFFERENCE
    Lopes, Stella Crosara
    Pagnano, Valeria Oliveira
    Domingos de Almeida Rollo, Joao Manuel
    Leal, Monica Barbosa
    Bezzon, Osvaldo Luiz
    JOURNAL OF APPLIED ORAL SCIENCE, 2009, 17 (02) : 122 - 128
  • [2] Comparative evaluation of bond strength of various metal-ceramic restorations
    Korkmaz, Turan
    Asar, Volkan
    MATERIALS & DESIGN, 2009, 30 (03) : 445 - 451
  • [3] Simplified Acid Treatment Technique in Cobalt-Chromium Alloys: Effect on Bond Strength Metal-Ceramic
    Sobreiro, Michelli Menezes
    Macedo, Ana Paula
    Bezzon, Osvaldo Luiz
    Pagnano, Valeria Oliveira
    MATERIALS RESEARCH-IBERO-AMERICAN JOURNAL OF MATERIALS, 2021, 24 (06):
  • [4] Effect of different air-abrasion particles on metal-ceramic bond strength
    Kulunk, Tolga
    Kurt, Murat
    Ural, Cagri
    Kulunk, Safak
    Baba, Seniha
    JOURNAL OF DENTAL SCIENCES, 2011, 6 (03) : 140 - 146
  • [5] Effect of layered manufacturing techniques, alloy powders, and layer thickness on metal-ceramic bond strength
    Ekren, Orhun
    Ozkomur, Ahmet
    Ucar, Yurdanur
    JOURNAL OF PROSTHETIC DENTISTRY, 2018, 119 (03) : 481 - 487
  • [6] A study on metal-ceramic thermal expansion compatibility
    Miculescu, Marian
    Branzei, Mihai
    Miculescu, Florin
    Meghea, Daniela
    Bane, Marin
    ADVANCED MATERIALS AND STRUCTURES V, 2014, 216 : 85 - 90
  • [7] Effect of pretreatments on the metal-ceramic bonding strength of a Pd-Ag alloy
    Li, Bo-hua
    Ye, Jian-tao
    Liao, Juan-kun
    Zhuang, Pei-lin
    Zhang, Yi-ping
    Li, Jie-yin
    JOURNAL OF DENTISTRY, 2014, 42 (03) : 319 - 328
  • [8] Effect of surface treatments on the bond strength of veneering ceramic to zirconia
    Korkmaz, Fatih Mehmet
    Bagis, Bora
    Turgut, Sedanur
    Ates, Sabit Melih
    Ayaz, Elif Aydogan
    JOURNAL OF APPLIED BIOMATERIALS & FUNCTIONAL MATERIALS, 2015, 13 (01): : 17 - 27
  • [9] Influence of cast surface finishing process on metal-ceramic bond strength
    Mehulic, Ketij
    Laus-Sosic, Martina
    Schauperl, Zdravko
    Vojvodic, Denis
    Stefancic, Sanja
    MEDICINSKI GLASNIK, 2009, 6 (02) : 235 - 242
  • [10] Metal-ceramic bond strength between a feldspathic porcelain and a Co-Cr alloy fabricated with Direct Metal Laser Sintering technique
    Dimitriadis, Konstantinos
    Spyropoulos, Konstantinos
    Papadopoulos, Triantafillos
    JOURNAL OF ADVANCED PROSTHODONTICS, 2018, 10 (01) : 25 - 31