Role of butter layer in low-cycle fatigue behavior of modified 9Cr and CrMoV dissimilar rotor welded joint

被引:42
|
作者
Wu, Qingjun [1 ,2 ]
Lu, Fenggui [1 ,2 ]
Cui, Haichao [1 ,2 ]
Liu, Xia [3 ]
Wang, Peng [3 ]
Tang, Xinhua [1 ,2 ]
机构
[1] Shanghai Jiao Tong Univ, Sch Mat Sci & Engn, Shanghai 200240, Peoples R China
[2] Shanghai Jiao Tong Univ, Shanghai Key Lab Mat Laser Proc & Modificat, Shanghai 200240, Peoples R China
[3] Shanghai Turbine Plant Shanghai Elect Power Gener, Shanghai 200240, Peoples R China
关键词
Low-cycle fatigue behavior; Butter layer; Dissimilar welded joint; Fracture location; Softening behavior; LOW-ALLOY STEEL; AUSTENITIC STAINLESS-STEEL; STRENGTH LOW-ALLOY; GAS TUNGSTEN ARC; MECHANICAL-PROPERTIES; CREEP-FATIGUE; MICROSTRUCTURE CHARACTERISTICS; STEAM; TEMPERATURE; BEAM;
D O I
10.1016/j.matdes.2014.02.022
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The present work aims at studying the role of butter layer (BL) in low-cycle fatigue (LCF) behavior of modified 9Cr steel and CrMoV steel dissimilar welded joint. The significant difference of the chemical composition of base metals (BMs) makes it a challenge to achieve sound welded joint. Therefore, buttering was considered to obtain a transition layer between the dissimilar steels. The LCF tests of two kinds of specimens without and with butter layer were performed applying strain-controlled cyclic load with different axial strain amplitudes. The test results indicated that the number of cycles at higher strain amplitudes of welded joint without butter layer was greatly higher than that of the joint with butter layer, while the fatigue lifetime to crack initiation (2N(f)) became closer to each other at low and middle strain amplitudes. The failure was in the tempered heat affected zone (HAZ) at the CrMoV side for specimens without BL, while the fracture occurred at the tempered HAZ in the BL for specimens with BL. The microstructure details of BM, BL, HAZ and weld metals (WMs) were revealed by optical microscopy (OM). It was found that the tempered martensite was major microstructure for welded joint and much more carbides were observed in tempered HAZ than other parts due to the repeated tempering. Microhardness test indicated a softest zone existing tempered HAZ of BL and also there was a softer zone in tempered HAZ at the CrMoV side due to repeated tempering during welding and post weld heat treatment (PWHT). And scanning electron microscopy (SEM) was applied to observe the fractography. It was indicated that the fatigue crack initiation occurred from the specimen surface and all specimens were ductile-brittle mixed fractures. It is deemed that the softening behavior in BL caused by twice tempering correspondingly decreased the LCF lifetime at higher strain amplitudes. So suitable welding parameters and heat treatment processes became a key measure to ensure LCF property without losing other properties for welded joint with BL. (C) 2014 Elsevier Ltd. All rights reserved.
引用
收藏
页码:165 / 175
页数:11
相关论文
共 50 条
  • [21] Failure competition behavior of 9Cr/617 dissimilar welded joint during LCF test at elevated temperature
    Wang, Yaqi
    Shao, Chendong
    Cui, Haichao
    Fan, Manjie
    Ma, Ninshu
    Lu, Fenggui
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2020, 773
  • [22] Prevention of carbon migration in 9% Cr/CrMoV dissimilar welded joint by adding tungsten inert gas overlaying layer
    Kai Ding
    Hui-jun Ji
    Xia Liu
    Peng Wang
    Quan-liang Zhang
    Xiao-hong Li
    Yu-lai Gao
    Journal of Iron and Steel Research International, 2018, 25 : 847 - 853
  • [23] Prevention of carbon migration in 9% Cr/CrMoV dissimilar welded joint by adding tungsten inert gas overlaying layer
    Ding, Kai
    Ji, Hui-jun
    Liu, Xia
    Wang, Peng
    Zhang, Quan-liang
    Li, Xiao-hong
    Gao, Yu-lai
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2018, 25 (08) : 847 - 853
  • [24] High cycle fatigue property and lifetime modeling of CrMoV and NiCrMoV dissimilar steel welded joint
    Wang, Zhipeng
    Zhu, Mingliang
    Xuan, Fuzhen
    Hanjie Xuebao/Transactions of the China Welding Institution, 2024, 45 (07): : 67 - 73
  • [25] Effects of weld geometry and HAZ property on low-cycle fatigue behavior of welded joint
    Tsutsumi, Seiichiro
    Fincato, Riccardo
    Luo, Pengjun
    Sano, Moe
    Umeda, Toshihiro
    Kinoshita, Tomohiro
    Tagawa, Tetsuya
    INTERNATIONAL JOURNAL OF FATIGUE, 2022, 156
  • [26] Investigation on the weakest zone in toughness of 9Cr/NiCrMoV dissimilar welded joint and its enhancement
    Xia Liu
    Zhipeng Cai
    Xionglin Deng
    Fenggui Lu
    Journal of Materials Research, 2017, 32 : 3117 - 3127
  • [27] Investigation on the weakest zone in toughness of 9Cr/NiCrMoV dissimilar welded joint and its enhancement
    Liu, Xia
    Cai, Zhipeng
    Deng, Xionglin
    Lu, Fenggui
    JOURNAL OF MATERIALS RESEARCH, 2017, 32 (16) : 3117 - 3127
  • [28] High cycle fatigue behavior of a dissimilar metal welded joint in ultra-supercritical steam turbine rotor
    Wang, Wen-Ke
    Xu, Zhen-Zhen
    Zhu, Bo
    Zhang, Xiao-Fan
    Zhong, Jie
    Zhang, Jian-Xun
    MATERIALS RESEARCH EXPRESS, 2020, 7 (01)
  • [29] Enhanced Galvanic Corrosion Phenomenon in the Welded Joint of NiCrMoV Steel by Low-Cycle Fatigue Behavior
    Weng, S.
    Huang, Y. H.
    Xuan, F. Z.
    Zheng, S. L.
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2019, 166 (12) : C270 - C283
  • [30] Anomalous residual austenite formation in root of welding layers of 9% Cr/CrMoV dissimilar welded joint
    Ding, Kai
    Ji, Hui-jun
    Zhang, Quan-liang
    Liu, Xia
    Wang, Peng
    Li, Xiao-hong
    Zhang, Ling
    Gao, Yu-lai
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2018, 25 (08) : 839 - 846