Effect of process parameters on the surface morphology and mechanical performance of silicon structures after deep reactive ion etching (DRIE)

被引:184
作者
Chen, KS [1 ]
Ayón, AA
Zhang, X
Spearing, SM
机构
[1] Natl Cheng Kung Univ, Dept Mech Engn, Tainan 70101, Taiwan
[2] Sony Semicond, San Antonio, TX 78245 USA
[3] MIT, Dept Elect Engn & Comp Sci, Microsyst Technol Labs, Cambridge, MA 02139 USA
[4] MIT, Dept Aeronaut & Astronaut, Cambridge, MA 02139 USA
关键词
deep reactive ion etching (DRIE); fracture strength; MEMS; plasma etching; silicon; surface morphology;
D O I
10.1109/JMEMS.2002.1007405
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
The ability to predict and control the influence of process parameters during silicon etching is vital for the success of most MEMS devices. In the case of deep reactive ion etching (DRIE) of silicon substrates, experimental results indicate that etch performance as well as surface morphology and post-etch mechanical behavior have a strong dependence on processing parameters. In order to understand the influence of these parameters, a set of experiments was designed and performed to fully characterize the sensitivity of surface morphology and mechanical behavior of silicon samples produced with different DRIE operating conditions. The designed experiment involved a matrix of 55 silicon wafers with radiused hub flexure (RHF) specimens which were etched 10 min under varying DRIE processing conditions. Data collected by interferometry, atomic force microscopy (AFM), profilometry, and scanning electron microscopy (SEM), was used to determine the response of etching performance to operating conditions. The data collected for fracture strength was analyzed and modeled by finite element computation. The data was then fitted to response surfaces to model the dependence of response variables on dry processing conditions. The results showed that the achievable anisotropy, etching uniformity, fillet radii, and surface roughness had a strong dependence on chamber pressure, applied coil and electrode power, and reactant gases flow rate. The observed post-etching mechanical behavior for specimens with high surface roughness always indicated low fracture strength. For specimens with better surface quality, there was a wider distribution in sample strength. This suggests that there are more controlling factors influencing the mechanical behavior of specimens. Nevertheless, it showed that in order to achieve high strength, fine surface quality is a necessary requisite. The mapping of the dependence of response variables on dry processing conditions produced by this systematic approach provides additional insight into the plasma phenomena involved and supplies a practical set of tools to locate and optimize robust operating conditions.
引用
收藏
页码:264 / 275
页数:12
相关论文
共 33 条
  • [1] THE PLASMA-ETCHING OF POLYSILICON WITH CF3CL/ARGON DISCHARGES .3. MODELING OF ETCHING RATE AND DIRECTIONALITY
    ALLEN, KD
    SAWIN, HH
    YOKOZEKI, A
    [J]. JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1986, 133 (11) : 2331 - 2338
  • [2] Anisotropic silicon trenches 300-500 μm deep employing time multiplexed deep etching (TMDE)
    Ayón, AA
    Zhang, X
    Khanna, R
    [J]. SENSORS AND ACTUATORS A-PHYSICAL, 2001, 91 (03) : 381 - 385
  • [3] Characterization of a time multiplexed inductively coupled plasma etcher
    Ayón, AA
    Braff, R
    Lin, CC
    Sawin, HH
    Schmidt, MA
    [J]. JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1999, 146 (01) : 339 - 349
  • [4] Ayón AA, 1999, MATER RES SOC SYMP P, V546, P51
  • [5] BAYT RL, 1997, P 33 AIAA ASME SAE A
  • [6] BOSCH R, 1994, Patent No. 4855017
  • [7] BOSCH RB, 1994, Patent No. 4784720
  • [8] CHEN CP, 1980, AM CERAM SOC BULL, V59, P469
  • [9] Controlling and testing the fracture strength of silicon on the mesoscale
    Chen, KS
    Ayon, A
    Spearing, SM
    [J]. JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2000, 83 (06) : 1476 - 1484
  • [10] Silicon strength testing for mesoscale structural applications
    Chen, KS
    Ayon, AA
    Spearing, SM
    [J]. MICROELECTROMECHANICAL STRUCTURES FOR MATERIALS RESEARCH, 1998, 518 : 123 - 130