Mechanical behavior of additive manufactured, powder-bed laser-fused materials

被引:762
作者
Mower, Todd M. [1 ]
Long, Michael J. [1 ]
机构
[1] MIT, Lincoln Lab, Lexington, MA 02420 USA
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2016年 / 651卷
关键词
Aluminum alloys; Titanium alloys; Stainless steel alloys; Powder-bed fusion; Cyclic fatigue; STAINLESS-STEEL; FATIGUE PERFORMANCE; TI-6AL-4V; MICROSTRUCTURE; PARTS; SLM;
D O I
10.1016/j.msea.2015.10.068
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Mechanical behavior of four metallic alloys fabricated with layered, laser-heated methods of additive manufacturing (AM) was compared to that of similar alloys produced with conventional methods (wrought and machined). AM materials were produced by a leading commercial service provider, as opposed to incorporating material specimens produced by unique or specially-adapted equipment. The elastic moduli were measured in flexure, stress-strain characteristics were measured in tensile deformation, and fatigue strengths were measured in fully reversed bending. The effects of fabrication orientation, surface polishing, and hot isostatic pressing upon mechanical behavior were studied. The fatigue strengths exhibited by SLM AlSi10Mg and DMLS Ti6AI4V in the as-fabricated condition proved to be significantly inferior to that of conventional material. These lower fatigue strengths are a consequence of multiple fatigue cracks initiating at surface defects, internal voids and microcracks, and growing simultaneously during cyclic loading. Measured fatigue strengths of DMLS 316L and 17-4PH approached those of corresponding wrought materials when subjected to principal stresses aligned with the build planes. When cyclic stresses were applied across the build planes of the DMLS stainless steels, fatigue fractures often developed prematurely by separation of material. Post-processing the DMIS Ti6Al4V and SS316L with hot isostatic pressure elevated the fatigue strength significantly. Measurements of surface roughness with an optical profilometer, examinations of the material microstructures, and fractography contribute to an understanding of the mechanical of the additive materials. (C) 2015 The Authors. Published by Elsevier B.V.
引用
收藏
页码:198 / 213
页数:16
相关论文
共 38 条
[1]  
Aboulkhair Nesma T., 2014, Addit. Manuf., V1-4, P77, DOI DOI 10.1016/J.ADDMA.2014.08.001
[2]   Direct selective laser sintering of metals [J].
Agarwala, Mukesh ;
Bourell, David ;
Beaman, Joseph ;
Marcus, Harris ;
Barlow, Joel .
RAPID PROTOTYPING JOURNAL, 1995, 1 (01) :26-36
[3]  
[Anonymous], J MAT RES TECHNOL
[4]  
[Anonymous], 2011, MAT PROP DEV STAND M
[5]  
ASTM International. F2792, 2012, F2792 ASTM INT
[6]  
Boucher F., 2010, P 56 ANN M ORTH RES
[7]  
Brandi E., 2008, P EUR INT C RAP PROT
[8]   Microstructure of additive layer manufactured Ti-6Al-4V after exceptional post heat treatments [J].
Brandl, Erhard ;
Greitemeier, Daniel .
MATERIALS LETTERS, 2012, 81 :84-87
[9]   Additive manufactured AlSi10Mg samples using Selective Laser Melting (SLM): Microstructure, high cycle fatigue, and fracture behavior [J].
Brandl, Erhard ;
Heckenberger, Ulrike ;
Holzinger, Vitus ;
Buchbinder, Damien .
MATERIALS & DESIGN, 2012, 34 :159-169
[10]   High Power Selective Laser Melting (HP SLM) of Aluminum Parts [J].
Buchbinder, D. ;
Schleifenbaum, H. ;
Heidrich, S. ;
Meiners, W. ;
Bueltmann, J. .
LASERS IN MANUFACTURING 2011: PROCEEDINGS OF THE SIXTH INTERNATIONAL WLT CONFERENCE ON LASERS IN MANUFACTURING, VOL 12, PT A, 2011, 12 :271-278