Compressive properties of zone-directionally solidified β-NiAl and its off-eutectic alloys with chromium and tungsten

被引:11
作者
Asthana, R
Tiwari, R
Tewari, SN
机构
[1] Univ Wisconsin Stout, Mfg Engn Technol Dept, Menomonie, WI 54751 USA
[2] Texas Instruments Inc, 300 MM CMP Proc Team, Dallas, TX 75243 USA
[3] Cleveland State Univ, Dept Chem Engn, Cleveland, OH 44115 USA
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2002年 / 336卷 / 1-2期
关键词
zone-directional solidification; nickel aluminide; chromium alloying; tungsten alloying; compressive strength; fracture;
D O I
10.1016/S0921-5093(01)01919-0
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The ordered intermetallic compound beta-NiAl and its pseudo-binary off-eutectic alloys with 1 at.% tungsten and 9.7 at.% chromium were directionally solidified (DS) in the 'floating-zone' mode, and tested for compressive strength and fracture behavior in the temperature range 300-800 K. The dual-phase structures created by the DS of ternary NiAl alloys led to improvements in both the compressive strength and the ductility. The room-temperature (300 K) 0.2% compressive yield strength (CYS) of DS NiAl(W) (623 MPa) is larger than the CYS of DS NiAl(Cr) (565 MPa) and DS NiAl (435 MPa). The CYS of the three alloys dropped with increasing test temperature, and at 800 K, the CYS values for the three materials were comparable (356, 315 and 344 MPa for NiAl, NiAl(W) and NiAl(Cr), respectively). All the DS alloys exhibited greater than near-zero ductility of polycrystalline beta-NiAl at room-temperature, with the fracture strain being the largest for the DS NiAl(Cr) (16.6%), followed by DS NiAl(W) (9.8%) and DS NiAl (7.33%). The strength and ductility data and fractography of test specimens suggest that ductile-phase toughening and second-phase strengthening are responsible for the observed improvements in the ductility and strength of NiAl. Limited tensile tests on the DS NiAl and DS NiAl(Cr) indicate that the CYS is greater than the tensile yield strength. (C) 2002 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:99 / 109
页数:11
相关论文
共 23 条
  • [1] CORRELATION OF DEFORMATION MECHANISMS WITH THE TENSILE AND COMPRESSIVE BEHAVIOR OF NIAL AND NIAL(ZR) INTERMETALLIC ALLOYS
    BOWMAN, RR
    NOEBE, RD
    RAJ, SV
    LOCCI, IE
    [J]. METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1992, 23 (05): : 1493 - 1508
  • [2] MICROSTRUCTURES FROM A DIRECTIONALLY SOLIDIFIED NIAL-CR EUTECTIC DEFORMED AT ROOM-TEMPERATURE
    CHEN, XF
    JOHNSON, DR
    OLIVER, BF
    [J]. SCRIPTA METALLURGICA ET MATERIALIA, 1994, 30 (08): : 975 - 980
  • [3] THE EFFECTS OF CHROMIUM ON NIAL INTERMETALLIC ALLOYS .1. MICROSTRUCTURES AND MECHANICAL-PROPERTIES
    COTTON, JD
    NOEBE, RD
    KAUFMAN, MJ
    [J]. INTERMETALLICS, 1993, 1 (01) : 3 - 20
  • [4] THE EFFECT OF IRON, GALLIUM AND MOLYBDENUM ON THE ROOM-TEMPERATURE TENSILE DUCTILITY OF NIAL
    DAROLIA, R
    LAHRMAN, D
    FIELD, R
    [J]. SCRIPTA METALLURGICA ET MATERIALIA, 1992, 26 (07): : 1007 - 1012
  • [5] DESTEFANI JD, 1989, ADV MATER PROCESS, V2, P37
  • [6] THE ROLE OF MICROSTRUCTURE ON STRENGTH AND DUCTILITY OF HOT-EXTRUDED MECHANICALLY ALLOYED NIAL
    DOLLAR, M
    DYMEK, S
    HWANG, SJ
    NASH, P
    [J]. METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1993, 24 (09): : 1993 - 2000
  • [7] THE EFFECT OF ALLOYING ON SLIP SYSTEMS IN (001) ORIENTED NIA1 SINGLE-CRYSTALS
    FIELD, RD
    LAHRMAN, DF
    DAROLIA, R
    [J]. ACTA METALLURGICA ET MATERIALIA, 1991, 39 (12): : 2961 - 2969
  • [8] GUHA S, 1989, HIGH TEMPERATURE ORD, V133, P633
  • [9] THE FRACTURE-RESISTANCE OF DIRECTIONALLY SOLIDIFIED DUAL-PHASE NIAL REINFORCED WITH REFRACTORY-METALS
    HEREDIA, FE
    HE, MY
    LUCAS, GE
    EVANS, AG
    DEVE, HE
    KONITZER, D
    [J]. ACTA METALLURGICA ET MATERIALIA, 1993, 41 (02): : 505 - 511
  • [10] HIRANO T, 1993, STRUCTURAL INTERMETALLICS, P437