Evolution of surface morphology in laser-dressed alumina grinding wheel material

被引:16
作者
Harimkar, Sandip P. [1 ]
Dahotre, Narendra B. [1 ]
机构
[1] Univ Tennessee, Dept Mat Sci & Engn, Knoxville, TN 37996 USA
关键词
D O I
10.1111/j.1744-7402.2006.02097.x
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
An approach to laser dressing of alumina grinding wheels is proposed based on solidification microstructures associated with rapid cooling rates obtained in laser surface processing. Laser dressing of alumina grinding wheels forms surface microstructures characterized by multifaceted grains that are expected to facilitate the micro-scale material removal during precision machining. A detailed investigation of variation of grain size and melt depth with laser fluence is conducted. The results are correlated with calculated cooling rates derived from a thermal model. In addition, based on microscopic observations, the formation of surface grains by stacking of individual multifaceted grains formed during laser dressing is suggested.
引用
收藏
页码:375 / 381
页数:7
相关论文
共 23 条
[11]   Variation of structure with input energy during laser surface engineering of ceramic coatings on aluminum alloys [J].
Kadolkar, P ;
Dahotre, NB .
APPLIED SURFACE SCIENCE, 2002, 199 (1-4) :222-233
[12]   Morphological modification in laser-dressed alumina grinding wheel material for microscale grinding [J].
Khangar, A ;
Dahotre, NB .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2005, 170 (1-2) :1-10
[13]   Microstructure and microtexture in laser-dressed alumina grinding wheel material [J].
Khangar, AA ;
Kenik, EA ;
Dahotre, NB .
CERAMICS INTERNATIONAL, 2005, 31 (04) :621-629
[14]   The evolution of microstructure in a laser clad TiB-Ti composite coating [J].
Kooi, BJ ;
Pei, YT ;
De Hosson, JTM .
ACTA MATERIALIA, 2003, 51 (03) :831-845
[15]  
Kurz W., 1998, FUNDAMENTALS SOLIDIF
[16]   Laser surface engineering of a magnesium alloy with Al+Al2O3 [J].
Majumdar, JD ;
Chandra, BR ;
Mordike, BL ;
Galun, R ;
Manna, I .
SURFACE & COATINGS TECHNOLOGY, 2004, 179 (2-3) :297-305
[17]   GRINDING MECHANISMS AND STRENGTH DEGRADATION FOR CERAMICS [J].
MALKIN, S ;
RITTER, JE .
JOURNAL OF ENGINEERING FOR INDUSTRY-TRANSACTIONS OF THE ASME, 1989, 111 (02) :167-174
[18]   Laser surface engineering of copper with chromium for enhanced wear resistance [J].
Manna, I ;
Majumdar, JD ;
Chatterjee, UK ;
Nath, AK .
SCRIPTA MATERIALIA, 1996, 35 (03) :405-410
[19]   EFFECTS OF SINGLE-PASS LASER HEAT-TREATMENT ON EROSION BEHAVIOR OF CAST IRONS [J].
MOLIAN, PA ;
BALDWIN, M .
WEAR, 1987, 118 (03) :319-327
[20]  
NICOLAS G, 1997, APPL SURF SCI, V110, P289