Corrosion behavior of 2205 duplex stainless steel in NaCl solutions containing sulfide ions

被引:44
作者
Xiao, Ying [1 ]
Tang, Junlei [1 ]
Wang, Yingying [2 ]
Lin, Bing [1 ]
Nie, Zhen [4 ]
Li, Yunfei [5 ]
Normand, Bernard [6 ]
Wang, Hu [3 ]
机构
[1] Southwest Petr Univ, Sch Chem & Chem Engn, Chengdu 610500, Peoples R China
[2] Jianghan Univ, Key Lab Optoelect Chem Mat & Devices, Minist Educ, Wuhan, Peoples R China
[3] Southwest Petr Univ, Sch Mat Sci & Engn, Chengdu 610500, Peoples R China
[4] CNPC, Res Inst Petr Explorat & Dev, Beijing 100083, Peoples R China
[5] Xinjiang Oilfield Co, 2 Oil Prod Plant Xinjiang Oilfield Co, Karamay 834008, Xinjiang, Peoples R China
[6] Univ Lyon, MATEIS UMR CNRS 5510, INSA Lyon, Bat L de Vinci,21 Ave Jean Capelle, F-69621 Villeurbanne, France
关键词
Duplex stainless steel; PH; Chloride; Sulfide; Pitting corrosion; ELECTROCHEMICAL-BEHAVIOR; PASSIVE FILMS; PITTING CORROSION; CHLORIDE; RESISTANCE; H2S; CRACKING; PH; TEMPERATURE; CHROMIUM;
D O I
10.1016/j.corsci.2022.110240
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The corrosion behavior of 2205 duplex stainless steel (DSS) in sulfide-containing NaCl solutions at different pH values are investigated. In 0.8 g/L NaCl solutions, the 2205 DSS pitting corrosion resistance increased with Na2S addition. The pH has significant effects on the corrosion mechanism of 2205 DSS in a 35 g/L NaCl solution with sulfide. In 35 g/L NaCl solutions, addition of Na2S can improve pitting resistance of 2205 DSS at pH 11.5, but the Na2S addition promotes pitting corrosion at pH 9, 7 and 4. At pH 7, the pitting corrosion resistance of 2205 DSS is the worst with sulfide.
引用
收藏
页数:17
相关论文
共 47 条
[11]   The beneficial galvanic effect of the constituent phases in 2205 duplex stainless steel on the passive films formed in a 3.5% NaCl solution [J].
Cheng, Xuequn ;
Wang, Yi ;
Dong, Chaofang ;
Li, Xiaogang .
CORROSION SCIENCE, 2018, 134 :122-130
[12]   Cooling rate effect on vacuum brazed joint properties for 2205 duplex stainless steels [J].
Chiu, LH ;
Hsieh, WC ;
Wu, CH .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2003, 354 (1-2) :82-91
[13]   COAL LIQUIDS DISTILLATION TOWER CORROSION - CHLORIDE ANALYSIS OF SOLVENT REFINED COAL PROCESS SAMPLES [J].
DAVIS, BH ;
THOMAS, GA ;
SAGUES, AA ;
JEWITT, CH ;
BAUMERT, KL .
FUEL PROCESSING TECHNOLOGY, 1983, 8 (01) :77-93
[14]   A comparative H2S corrosion study of 304L and 316L stainless steels in acidic media [J].
Davoodi, A. ;
Pakshir, M. ;
Babaiee, M. ;
Ebrahimi, G. R. .
CORROSION SCIENCE, 2011, 53 (01) :399-408
[15]   The electrochemical behaviour of 316L austenitic stainless steel in Cl- containing environment under different H2S partial pressures [J].
Ding, Jinhui ;
Zhang, Lei ;
Lu, Minxu ;
Wang, Jing ;
Wen, Zhibin ;
Hao, Wenhui .
APPLIED SURFACE SCIENCE, 2014, 289 :33-41
[16]   In situ study of selective dissolution of duplex stainless steel 2205 by electrochemical scanning tunnelling microscopy [J].
Femenia, M ;
Pan, J ;
Leygraf, C ;
Luukkonen, P .
CORROSION SCIENCE, 2001, 43 (10) :1939-1951
[17]   Effects of cold work and sensitization treatment on the corrosion resistance of high nitrogen stainless steel in chloride solutions [J].
Fu, Yao ;
Wu, Xinqiang ;
Han, En-Hou ;
Ke, Wei ;
Yang, Ke ;
Jiang, Zhouhua .
ELECTROCHIMICA ACTA, 2009, 54 (05) :1618-1629
[18]   Passivation model of 316 stainless steel in simulated cooling water and the effect of sulfide on the passive film [J].
Ge, HH ;
Zhou, DD ;
Wu, WQ .
APPLIED SURFACE SCIENCE, 2003, 211 (1-4) :321-334
[19]   A statistical study on the effect of annealing temperature on pitting corrosion resistance of 2205 duplex stainless steel [J].
Gholami, M. ;
Hoseinpoor, M. ;
Moayed, M. H. .
CORROSION SCIENCE, 2015, 94 :156-164
[20]  
Gong M, 2009, CORROS PROT MATER, V30, P473