Characteristics of particle size distribution of deoxidation products with Mg, Zr, Al, Ca, Si/Mn and Mg/Al in Fe-10mass%Ni alloy

被引:94
作者
Ohta, Hiroki [1 ]
Suito, Hideaki [1 ]
机构
[1] Tohoku Univ, Inst Multidisciplinary Res Adv Mat, Aoba Ku, Sendai, Miyagi 9808577, Japan
关键词
deoxidation; Mg; Zr; Al; Ca; Si/Mn; Mg/Al; particle size distribution; inclusion;
D O I
10.2355/isijinternational.46.14
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
In the experiments of an Fe-10mass%Ni alloy deoxidized with Mg, Zr, Al, Ca, Mn/Si and Al/Mg at 1873 K, the characteristics of particle size distributions have been studied as a function of holding time, amount of deoxidant and order of deoxidant addition. The peak height in particle size distribution decreases and the modal value increases with increasing holding time. The width of the distribution curve is larger for Al2O3 particles and smaller for liquid CaO-Al2O3 and MnO-SiO2 particles. The number of particles increases with an increase of deoxidant for a given initial oxygen content and holding time. In the case of Al followed by Mg deoxidation, the particle size distribution is almost the same as that obtained by only Al. The size distribution in case of Mg followed by Al deoxidation is almost the same as that by only Mg.
引用
收藏
页码:14 / 21
页数:8
相关论文
共 21 条
[1]   ALUMINUM DEOXIDATION EQUILIBRIUM IN LIQUID NI-FE ALLOYS EQUILIBRATED WITH CAO-AL2O3 SLAGS [J].
CHO, SW ;
SUITO, H .
STEEL RESEARCH, 1995, 66 (06) :237-243
[2]  
DEHOFF RT, 1961, T METALL SOC AIME, V221, P975
[3]  
Fujimura H, 2001, TETSU TO HAGANE, V87, P707
[4]  
FULLMAN RL, 1953, T AM I MIN MET ENG, V197, P447
[5]   ULTRAFINE METAL PARTICLES [J].
GRANQVIST, CG ;
BUHRMAN, RA .
JOURNAL OF APPLIED PHYSICS, 1976, 47 (05) :2200-2219
[6]   Dispersion of primary inclusions of Ce2O3 and CeS in Fe-0.20 mass%C-0.02 mass%P alloy [J].
Guo, MX ;
Suito, H .
ISIJ INTERNATIONAL, 1999, 39 (07) :678-686
[7]   Influence of dissolved cerium and primary inclusion particles of Ce2O3 and CeS on solidification behavior of Fe-0.20mass%C-0.02 mass%P alloy [J].
Guo, MX ;
Suito, H .
ISIJ INTERNATIONAL, 1999, 39 (07) :722-729
[8]   Pinning of austenite grain boundary of Fe-0.09 to 0.53 mass% C-0.02 mass%P alloys by primary inclusions of Ce2O3 and CeS [J].
Guo, MX ;
Suito, H .
ISIJ INTERNATIONAL, 1999, 39 (12) :1289-1296
[9]   DETERMINATION OF OXYGEN IN IRON-ALUMINUM ALLOY BY INERT-GAS FUSION-INFRARED ABSORPTIOMETRY (REPRINTED FROM J JAPAN INST METALS, VOL 55, PG 975, 1991) [J].
INOUE, R ;
SUITO, H .
MATERIALS TRANSACTIONS JIM, 1991, 32 (12) :1164-1169
[10]   Analysis of size distributions of primary oxide inclusions in Fe-10 mass pct Ni-M (M = Si, Ti, Al, Zr, and Ce) alloy [J].
Karasev, A ;
Suito, H .
METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 1999, 30 (02) :259-270