Characterization and reactivity of Fe-[Al,B]MFI catalysts for benzene hydroxylation with N2O

被引:38
作者
Centi, G.
Perathoner, S.
Arrigo, R.
Giordano, G.
Katovic, A.
Pedula, V.
机构
[1] Univ Messina, Dept Ind Chem & Engn Mat, I-98155 Messina, Italy
[2] Univ Calabria, Dept Chem Engn & Mat, Calabria, Italy
关键词
phenol; benzene; zeolite defects; N2O; Fe/MFI; boron; aluminium;
D O I
10.1016/j.apcata.2006.03.018
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The characteristics of Fe-[B,AI]MFI catalysts prepared by changing: (i) the gel composition during the hydrothermal synthesis (Si/Al and Si/B ratio) and (ii) other synthesis aspects (silica source, use of phosphoric acid to complex iron) were studied. The samples were investigated in terms of composition, structural (X-ray diffraction (XRD), Fourier transform-IR (FT-IR)) and morphological (scanning electron microscopy (SEM)) aspects and distribution of the iron species determined by UV-vis DR spectroscopy. The results were correlated with the reactivity of these samples (phenol productivity and selectivity during benzene hydroxylation with N2O). A linear relationship was observed between Si/B ratio and phenol maximum productivity. This indicates that the main factor determining the catalytic performances is the amount of B introduced in the zeolite which in turn depends on the gel composition during hydrothermal synthesis and the preparation method. The linear relationship could be interpreted considering that the role of B is related to its easier migration from framework to extra-framework position with respect to Al and therefore easier creation of defect sites during heat treatment. These defect sites are important, because during the initial stage of the catalytic reaction, iron ions migrate to these sites creating highly active iron sites responsible of the initial increase in the phenol productivity. The presence of Al in the gel influences negatively the catalytic performances, because both Al competes with B to be introduced in the MFI structure as T atom. Furthermore, the presence of Al as T atom determines a lowering of the selectivity to phenol with respect to both carbon oxides and carbonaceous deposits formation. (c) 2006 Elsevier B.V. All rights reserved.
引用
收藏
页码:30 / 41
页数:12
相关论文
共 59 条
[1]   Isomorphous substitution in zeolites [J].
Aiello, R ;
Nagy, JB ;
Giordano, G ;
Katovic, A ;
Testa, F .
COMPTES RENDUS CHIMIE, 2005, 8 (3-4) :321-329
[2]   Selective oxidation of methane by dinitrogen monoxide on FeZSM-5 zeolites. Ab initio quantum chemical analysis [J].
Arbuznikov, AV ;
Zhidomirov, GM .
CATALYSIS LETTERS, 1996, 40 (1-2) :17-23
[3]  
ATOGUCHI T, 1997, Patent No. 09194412
[4]   Catalytic activity of Fe ions in iron-based crystalline and amorphous systems: role of dispersion, coordinative unsaturation and Al content [J].
Berlier, G ;
Ricchiardi, G ;
Bordiga, S ;
Zecchina, A .
JOURNAL OF CATALYSIS, 2005, 229 (01) :127-135
[5]   Evolution of extraframework iron species in Fe silicalite 1. Effect of Fe content, activation temperature, and interaction with redox agents [J].
Berlier, G ;
Spoto, G ;
Bordiga, S ;
Ricchiardi, G ;
Fisicaro, P ;
Zecchina, A ;
Rossetti, I ;
Selli, E ;
Forni, L ;
Giamello, E ;
Lamberti, C .
JOURNAL OF CATALYSIS, 2002, 208 (01) :64-82
[6]   The role of Al in the structure and reactivity of iron centers in Fe-ZSM-5-based catalysts: a statistically based infrared study [J].
Berlier, G ;
Zecchina, A ;
Spoto, G ;
Ricchiardi, G ;
Bordiga, S ;
Lamberti, C .
JOURNAL OF CATALYSIS, 2003, 215 (02) :264-270
[7]   Structure and reactivity of framework and extraframework iron in Fe-silicalite as investigated by spectroscopic and physicochemical methods [J].
Bordiga, S ;
Buzzoni, R ;
Geobaldo, F ;
Lamberti, C ;
Giamello, E ;
Zecchina, A ;
Leofanti, G ;
Petrini, G ;
Tozzola, G ;
Vlaic, G .
JOURNAL OF CATALYSIS, 1996, 158 (02) :486-501
[8]  
CAMBLOR MA, 1992, J CHEM SOC CHEM COMM, V7, P360
[9]   Contribution of Fe and protonic sites in calcined and steamed ZSM-5 zeolites to oxidation of benzene with N2O to phenol and selective catalytic reduction of NO with propane to nitrogen [J].
Capek, L ;
Kubánek, P ;
Wichterlova, B ;
Sobalík, Z .
COLLECTION OF CZECHOSLOVAK CHEMICAL COMMUNICATIONS, 2003, 68 (10) :1805-1818
[10]   Performances of Fe-[Al, B]MFI catalysts in benzene hydroxylation with N2O -: The role of zeolite defects as host sites for highly active iron species [J].
Centi, G ;
Perathoner, S ;
Pino, F ;
Arrigo, R ;
Giordano, G ;
Katovic, A ;
Pedulà, V .
CATALYSIS TODAY, 2005, 110 (3-4) :211-220