Linear and non-linear rheological characterization of photo-oxidative degraded LDPE

被引:23
作者
Rolon-Garrido, Victor H. [1 ]
Wagner, Manfred H. [1 ]
机构
[1] TU Berlin, Berlin Inst Technol, Chair Polymer Engn Polymer Phys, D-10623 Berlin, Germany
关键词
Rheology; MSF model; Strain hardening; Low-density polyethylene; Polymer melts; Photo-oxidative degradation; LOW-DENSITY POLYETHYLENE; ELECTRON-BEAM IRRADIATION; CONCENTRATED POLYMER SYSTEMS; UNIVERSAL TESTING PLATFORM; STRESS FUNCTION MODEL; GURP-PALMEN-PLOT; MOLECULAR-STRUCTURE; ELONGATIONAL VISCOSITY; MELT RHEOLOGY; DEFORMATION-BEHAVIOR;
D O I
10.1016/j.polymdegradstab.2013.11.014
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Sheets of low-density polyethylene (LDPE) were photo-oxidatively treated in the presence of air. Characterization methods include solvent extraction method and rheology in the melt state by shear and uniaxial extensional experiments. For photo-oxidation, a xenon lamp was used to irradiate the samples for times between 1 day and 6 weeks. Linear viscoelasticity is strongly affected by increasing photo-oxidation due to crosslinking of LDPE, as corroborated by gel fraction. For samples which were degraded for up to three days, negligible gel content was found and the non-linear parameters f(max) and beta of the Molecular Stress Function (MSF) model indicate that the induced increase in strain hardening is due to the formation of long-chain branching, which is overcoming chain scission. Further degradation leads the parameter f(max) to increase to values outside the experimental window, while the parameter beta was found to correlate with the gel content and with the trend followed by the strain hardening index. The competition between chain scission and crosslinking could also be followed in linear viscoelasticity by the change in activation energy and in the loss angle delta. From the constitutive analysis, it is noticed that, within the experimental window, time-deformation separability is confirmed for all samples, independent of the degree of photo-oxidation. It is demonstrated that the sensitivity of theological characterization with respect to structural modifications, when combined with constitutive analysis, can be used to elucidate the effects of photo-degradation on LDPE. (C) 2013 Elsevier Ltd. All rights reserved.
引用
收藏
页码:136 / 145
页数:10
相关论文
共 65 条
[61]  
Winter H.H., 2007, IRIS DEV
[62]  
Winter HH, 1997, ADV POLYM SCI, V134, P165
[63]   Strain hardening behavior in elongational viscosity for binary blends of linear polymer and crosslinked polymer [J].
Yamaguchi, M ;
Miyata, H .
POLYMER JOURNAL, 2000, 32 (02) :164-170
[64]   Enhanced strain hardening in elongational viscosity for HDPE/crosslinked HDPE blend. II. Processability of thermoforming [J].
Yamaguchi, M ;
Suzuki, K .
JOURNAL OF APPLIED POLYMER SCIENCE, 2002, 86 (01) :79-83
[65]   Characterization to the weathering extent of LLDPE/LDPE thin film [J].
Zhao, BY ;
Yi, XW ;
Li, RY ;
Zhu, PF ;
Hu, KA .
JOURNAL OF APPLIED POLYMER SCIENCE, 2003, 88 (01) :12-16