Scratch behavior of aluminum anodized in oxalic acid: Effect of anodizing potential

被引:45
作者
Choudhary, R. K. [1 ]
Mishra, P. [1 ]
Kain, V. [1 ]
Singh, K. [1 ]
Kumar, S. [2 ]
Chakravartty, J. K. [1 ]
机构
[1] Bhabha Atom Res Ctr, Mat Grp, Bombay 400085, Maharashtra, India
[2] Bhabha Atom Res Ctr, Post Irradiat Examinat Div, Bombay 400085, Maharashtra, India
关键词
Aluminum; Anodizing; Oxalic acid; Scratch resistance; POROUS ALUMINA; OXIDE-FILMS; ANODIZATION PARAMETERS; MECHANICAL-PROPERTIES; VOLUME EXPANSION; FABRICATION; OXIDATION; COATINGS; GENERATION; CORROSION;
D O I
10.1016/j.surfcoat.2015.10.042
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Commercial purity aluminum sheets were anodized at 10-30 V in 10% oxalic acid solution at room temperature. The anodized specimens were tested for its resistance against scratch damage using a microscratch adhesion tester operated in the progressive mode. The specimens were studied also for crystal structure, chemical composition, surface morphology, surface topography, microhardness and electrical resistivity by X-ray diffractometty, energy dispersive X-ray spectroscopy, field emission scanning electron microscopy, stylus based surface profilometer, Vickers microhardness tester and four point probe method, respectively. Microscratch test results showed improved adhesion of the anodic aluminum oxide coating with the untransformed bulk, as the anodizing potential decreased. During scratch test, the specimens showed formation of cohesive cracks at a load of 1 N. Energy dispersive X-ray analysis showed that the concentration of oxygen increased marginally on increasing the anodizing potential. Field emission scanning electron microscopy showed comparatively less porous microstructure of the anodized specimens for anodizing conducted at potential 20 V or lower. The results of profilometry showed formation of smooth coating surface at potentials lower than 25 V. Microhardness test showed increased hardness of the anodized aluminum with increasing anodizing potential. The electrical resistivity of anodized aluminum was in the range of 10(6)-10(9) Omega.cm. X-ray diffraction measurements indicated amorphous structure of the so obtained aluminum oxide coating. (C) 2015 Elsevier B.V. All rights reserved.
引用
收藏
页码:135 / 147
页数:13
相关论文
共 53 条
[1]   Porous and mesh alumina formed by anodization of high purity aluminum films at low anodizing voltage [J].
Abd-Elnaiem, Alaa M. ;
Mebed, A. M. ;
El-Said, Waleed Ahmed ;
Abdel-Rahim, M. A. .
THIN SOLID FILMS, 2014, 570 :49-56
[2]  
Abd-Elnaiem AM, 2013, INT J ELECTROCHEM SC, V8, P10515
[3]  
Alaba O.A., 2012, ADV MAT LETT, V3, P273
[4]   Mechanical properties of barrier-type anodic alumina films using nanoindentation [J].
Alcalá, G ;
Mato, S ;
Skeldon, P ;
Thompson, GE ;
Mann, AB ;
Habazaki, H ;
Shimizu, K .
SURFACE & COATINGS TECHNOLOGY, 2003, 173 (2-3) :293-298
[5]  
Araoyinbo A.O., 2010, International Journal of Mechanical and Materials Engineering, V5, P53
[6]   Influence of porosity on Young's modulus and Poisson's ratio in alumina ceramics [J].
Asmani, M ;
Kermel, C ;
Leriche, A ;
Ourak, M .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2001, 21 (08) :1081-1086
[7]   Asymmetric alumina membranes electrochemically formed in oxalic acid solution [J].
Bocchetta, P ;
Sunseri, C ;
Bottino, A ;
Capannelli, G ;
Chiavarotti, G ;
Piazza, S ;
Di Quarto, F .
JOURNAL OF APPLIED ELECTROCHEMISTRY, 2002, 32 (09) :977-985
[8]   Enhancing aluminum corrosion resistance by two-step anodizing process [J].
Bouchama, L. ;
Azzouz, N. ;
Boukrnouche, N. ;
Chopart, J. P. ;
Daltin, A. L. ;
Bouznit, Y. .
SURFACE & COATINGS TECHNOLOGY, 2013, 235 :676-684
[9]   Aluminium corrosion in hydrochloric acid solutions and the effect of some organic inhibitors [J].
Branzoi, V ;
Golgovici, F ;
Branzoi, F .
MATERIALS CHEMISTRY AND PHYSICS, 2003, 78 (01) :122-131
[10]   An overview of the potential of quantitative coating adhesion measurement by scratch [J].
Bull, SJ ;
Berasetegui, EG .
TRIBOLOGY INTERNATIONAL, 2006, 39 (02) :99-114