Sulfidation properties of TiAl-2 at.% X (X=Si, Mn, Ni, Ge, Y, Zr, La and Ta) alloys at 1173 K and 1.3 Pa sulfur pressure in an H2S-H2 gas mixture

被引:11
作者
Izumi, T [1 ]
Yoshioka, T [1 ]
Hayashi, S [1 ]
Narita, T [1 ]
机构
[1] Hokkaido Univ, Grad Sch Engn, Res Grp Interface Control Engn, Kita Ku, Sapporo, Hokkaido 0608628, Japan
关键词
titanium aluminides; based on TiAl; corrosion; surface properties;
D O I
10.1016/S0966-9795(02)00005-5
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
TiAl-2 at.% X (X = Si, Mn, Ni, Ge, Y, Zr, La and Ta) alloys were sulfidized at 1173 K for 86.4 ks at a 1.3 Pa sulfur pressure in an H2S-H-2 gas mixture. The structure, phases, and compositions of the external sulfide scale and alloy surface layer were measured using EPMA and X-RD. The sulfides formed were mainly TiS, Ti3S4 and Al2S3. The alloy surface layer consisted of multi-layered structures that can be classified into three groups: group I of Mn, Ni, Y and Zr as well as TiAl binary alloy with alloy/TiAl2/TiAl3/sulfide scales; group 2 of Si and Ge with alloy/TiAl2/Ti(Al,X)(3)/sulfide scales, and group 3 of La and Ta with alloy/TiAl2/TiAl3/X-Al alloy/sulfide scales. The TiAl-2La and -2Ni alloys sulfidized faster than the TiAl, while the sulfidation amount for the TiAl-2X (X = Si, Mn, Ge, Y, Zr and Ta) alloys was almost the same as that of TiAl. The thickness of the alloy surface layer increased in the order: Ta < Si < Ni < Mn < Zr < (TiAl binary alloy) < Ge < La < Y. (C) 2002 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:353 / 360
页数:8
相关论文
共 55 条
[21]   ALUMINIDE COATINGS ON TIAL COMPOUND [J].
MABUCHI, H ;
ASAI, T ;
NAKAYAMA, Y .
SCRIPTA METALLURGICA, 1989, 23 (05) :685-689
[22]   THE OXIDATION BEHAVIOR OF GAMMA-TITANIUM ALUMINIDE ALLOYS UNDER THERMAL CYCLING CONDITIONS [J].
MCKEE, DW ;
HUANG, SC .
CORROSION SCIENCE, 1992, 33 (12) :1899-1914
[23]   The deposition of aluminide and silicide coatings on gamma-TiAl using the halide-activated pack cementation method [J].
Munro, TC ;
Gleeson, B .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1996, 27 (12) :3761-3772
[24]   Application of cast gamma TiAl for automobiles [J].
Noda, T .
INTERMETALLICS, 1998, 6 (7-8) :709-713
[25]   Oxidation of γ-TiAl intermetallic coated with electrodeposited nickel-La2O3 composite films [J].
Peng, X ;
Tang, Z ;
Li, T ;
Wu, W .
OXIDATION OF METALS, 1999, 51 (3-4) :317-331
[26]   FUNDAMENTALS OF TIAL OXIDATION - A CRITICAL-REVIEW [J].
RAHMEL, A ;
QUADAKKERS, WJ ;
SCHUTZE, M .
WERKSTOFFE UND KORROSION-MATERIALS AND CORROSION, 1995, 46 (05) :271-285
[27]   Multiphase intermetallic alloys for structural applications [J].
Sauthoff, G .
INTERMETALLICS, 2000, 8 (9-11) :1101-1109
[28]   The oxidation behavior of several Ti-Al alloys at 900°C in air [J].
Schmitz-Niederau, M ;
Schütze, M .
OXIDATION OF METALS, 1999, 52 (3-4) :225-240
[29]  
Schumacher G, 1999, MATER CORROS, V50, P162, DOI 10.1002/(SICI)1521-4176(199903)50:3<162::AID-MACO162>3.0.CO
[30]  
2-O