Behavior of Alkali-Activated Metakaolin Pastes Blended with Quartz Powder Exposed to Seawater Attack

被引:40
作者
Rashad, Alaa M. [1 ]
Ouda, Ahmed S. [2 ,3 ]
Sadek, Dina M. [1 ]
机构
[1] Housing & Bldg Natl Res Ctr, Bldg Mat Res & Qual Control Inst, Cairo 11511, Egypt
[2] Housing & Bldg Natl Res Ctr, Raw Bldg Mat Technol & Proc Res Inst, Cairo 11511, Egypt
[3] Tabuk Univ, Univ Coll Taimaa, Tabuk 71491, Saudi Arabia
关键词
Geopolymers; Quartz powder; Durability; Seawater; Strength deterioration ratio; CEMENTITIOUS MATERIALS; ELEVATED-TEMPERATURES; GEOPOLYMERS; DURABILITY; SLAG; STRENGTH; MORTARS;
D O I
10.1061/(ASCE)MT.1943-5533.0002335
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
The purpose of this work is to investigate the resistance of alkali-activated metakaolin (AAMK) paste specimens blended with different amounts of quartz powder (QP) against different environmental conditions. Metakaolin (MK) was partially substituted with QP at levels of 10, 20, 30, and 40%, by weight. After initial curing, specimens were exposed to different conditions including air, potable fresh water, and seawater up to 12 months. Compressive strength before exposure as well as strength deterioration ratio (SDR) after exposure were determined. The mineralogical compositions for selected mixtures before and after exposure to seawater attack were identified by X-ray diffraction (XRD) and thermogravimetric analysis (TGA) and compared with those cured in lab air. The microstructure and morphology were identified using scanning electron microscopy (SEM). The results showed that the incorporation of QP in MK-based geopolymers seemed as promising candidates for marine structure applications. (C) 2018 American Society of Civil Engineers.
引用
收藏
页数:8
相关论文
共 50 条
[21]   Wear behavior in pastes of alkali-activated materials: Influence of precursor and alkali solution [J].
Shagnay, S. ;
Velasco, F. ;
del Campo, A. ;
Torres-Carrasco, M. .
TRIBOLOGY INTERNATIONAL, 2020, 147
[22]   Effect of Waste Ceramic Powder on the Properties of Alkali-Activated Slag and Fly Ash Pastes Exposed to High Temperature [J].
Zhang, Gui-Yu ;
Bae, Sung-Chul ;
Lin, Run-Sheng ;
Wang, Xiao-Yong .
POLYMERS, 2021, 13 (21)
[23]   Sulfuric acid degradation of alkali-activated metakaolin cements supplemented with brucite [J].
Gevaudan, Juan Pablo ;
Craun, Zoey ;
Srubar, Wil V. .
CEMENT & CONCRETE COMPOSITES, 2021, 121
[24]   Copper mine tailings and metakaolin as precursors for sustainable alkali-activated mortars [J].
Mobili, Alessandra ;
Blasi, Elisa ;
Maqbool, Qaisar ;
Tittarelli, Francesca .
JOURNAL OF BUILDING ENGINEERING, 2025, 103
[25]   Microstructural Changes Induced by CO2 Exposure in Alkali-Activated Slag/Metakaolin Pastes [J].
Bernal, Susan A. .
FRONTIERS IN MATERIALS, 2016, 3
[26]   An investigation of using seawater as mixing water for alkali-activated slag pastes [J].
Rashad, Alaa M. ;
Khalil, Mervat H. .
INNOVATIVE INFRASTRUCTURE SOLUTIONS, 2022, 7 (02)
[27]   The effect of matrix composition and calcium content on the sulfate durability of metakaolin and metakaolin/slag alkali-activated mortars [J].
Alcamand, Himad A. ;
Borges, Paulo H. R. ;
Silva, Flavio A. ;
Trindade, Ana Carolina C. .
CERAMICS INTERNATIONAL, 2018, 44 (05) :5037-5044
[28]   An initial study on the effect of nano-zirconium on the behavious of alkali-activated slag cement subjected to seawater attack [J].
Rashad, Alaa M. ;
Eessaa, Ashraf K. ;
Khalil, Mervat H. ;
Mohamed, O. A. .
CONSTRUCTION AND BUILDING MATERIALS, 2023, 370
[29]   Effect of ceramic waste powder on alkali-activated slag pastes cured in hot weather after exposure to elevated temperature [J].
Rashad, Alaa M. ;
Essa, Ghada M. F. .
CEMENT & CONCRETE COMPOSITES, 2020, 111
[30]   Thermomechanical performance of blended metakaolin-GGBS alkali-activated foam concrete [J].
Samson, Gabriel ;
Cyr, Martin ;
Gao, Xiao Xiao .
CONSTRUCTION AND BUILDING MATERIALS, 2017, 157 :982-993