Contact deformation of TiN coatings on metallic substrates

被引:36
作者
Jayaram, V. [1 ]
Bhowmick, S.
Xie, Z. -H.
Math, S.
Hoffman, M.
Biswas, S. K.
机构
[1] Indian Inst Sci, Dept Met, Bangalore 560012, Karnataka, India
[2] Univ New S Wales, Sch Mat Sci & Engn, Sydney, NSW 2052, Australia
[3] Indian Inst Sci, Dept Engn Mech, Bangalore 560012, Karnataka, India
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2006年 / 423卷 / 1-2期
关键词
thin films; columnar coatings; TiN; indentation; modeling;
D O I
10.1016/j.msea.2005.09.123
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Recent developments in the contact deformation and fracture of columnar TiN coatings are reviewed. It is shown that columnar films display two regimes of responses: one dominated by columnar sliding at a critical shear stress which is determined substantially by the residual stress in the film, and the other, more damaging response, characterized by fracture. The transition to cracking modes of response is aided by a soft substrate and a thick film and can be understood from a relative comparison of the driving forces for the different modes by analytically simulating the response of an elastic bi-layer to Hertzian loading. The above comparison suggests that the relative success of columnar films, vis-A-vis amorphous or equi-axed films, is probably due to the existence of this relatively benign mode of columnar shear. The implications for optimal coating design are also discussed. (c) 2006 Elsevier B.V. All rights reserved.
引用
收藏
页码:8 / 13
页数:6
相关论文
共 23 条
[1]   ANALYSIS OF ELASTIC AND PLASTIC-DEFORMATION ASSOCIATED WITH INDENTATION TESTING OF THIN-FILMS ON SUBSTRATES [J].
BHATTACHARYA, AK ;
NIX, WD .
INTERNATIONAL JOURNAL OF SOLIDS AND STRUCTURES, 1988, 24 (12) :1287-1298
[2]   Contact damage in TiN coatings on steel [J].
Bhowmick, S ;
Kale, AN ;
Jayaram, V ;
Biswas, SK .
THIN SOLID FILMS, 2003, 436 (02) :250-258
[3]   Fracture mode transitions during indentation of columnar TiN coatings on metal [J].
Bhowmick, S ;
Bhide, R ;
Hoffman, M ;
Jayaram, V ;
Biswas, SK .
PHILOSOPHICAL MAGAZINE, 2005, 85 (25) :2927-2945
[4]   Deconvolution of fracture properties of TiN films on steels from nanoindentation load-displacement curves [J].
Bhowmick, S ;
Jayaram, V ;
Biswas, SK .
ACTA MATERIALIA, 2005, 53 (08) :2459-2467
[5]   Nature of contact deformation of TiN films on steel [J].
Bhowmick, S ;
Xie, ZH ;
Hoffman, M ;
Jayaram, V ;
Biswas, SK .
JOURNAL OF MATERIALS RESEARCH, 2004, 19 (09) :2616-2624
[6]  
Buckle H., 1973, The science of hardness testing and its research applications, P453
[7]   THE MECHANICAL-PROPERTIES OF WEAR-RESISTANT COATINGS .2. EXPERIMENTAL STUDIES AND INTERPRETATION OF HARDNESS [J].
BURNETT, PJ ;
RICKERBY, DS .
THIN SOLID FILMS, 1987, 148 (01) :51-65
[8]   SURFACE SOFTENING IN SILICON BY ION-IMPLANTATION [J].
BURNETT, PJ ;
PAGE, TF .
JOURNAL OF MATERIALS SCIENCE, 1984, 19 (03) :845-860
[9]   THE MECHANICAL-PROPERTIES OF WEAR-RESISTANT COATINGS .1. MODELING OF HARDNESS BEHAVIOR [J].
BURNETT, PJ ;
RICKERBY, DS .
THIN SOLID FILMS, 1987, 148 (01) :41-50
[10]   Degradation of TiN coatings under cyclic loading [J].
Cairney, JM ;
Tsukano, R ;
Hoffman, MJ ;
Yang, M .
ACTA MATERIALIA, 2004, 52 (11) :3229-3237