Microtensile bond strength analysis of adhesive systems to Er:YAG and Er,Cr:YSGG laser-treated dentin

被引:30
|
作者
Ramos, Thaysa Monteiro [1 ]
Ramos-Oliveira, Thayanne Monteiro [1 ]
Moretto, Simone Goncalves [1 ]
de Freitas, Patricia Moreira [1 ]
Esteves-Oliveira, Marcella [2 ]
Eduardo, Carlos de Paula [1 ]
机构
[1] Univ Sao Paulo, Sch Dent, Dept Restorat Dent, Special Lab Lasers Dent LELO, BR-05508000 Sao Paulo, Brazil
[2] Rhein Westfal TH Aachen, Dept Operat Dent Periodontol & Prevent Dent ZPP, D-52074 Aachen, Germany
基金
巴西圣保罗研究基金会;
关键词
Dentin; Er:YAG laser; Er; Cr:YSGG laser; SEM; Microtensile bond strength; ER-YAG-LASER; SELF-ETCHING PRIMER; BUR-CUT; CAVITY PREPARATION; WATER STORAGE; SURFACE; RESIN; ACID; ENAMEL; MICROLEAKAGE;
D O I
10.1007/s10103-012-1261-6
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
The aim of this in vitro study was to evaluate the effect of different surface treatments (control, diamond bur, erbium-doped yttrium aluminum garnet (Er:YAG) laser, and erbium, chromium:yttrium-scandium-gallium-garnet (Er,Cr:YSGG) laser) on sound dentin surface morphology and on microtensile bond strength (mu TBS). Sixteen dentin fragments were randomly divided into four groups (n = 4), and different surface treatments were analyzed by scanning electron microscopy. Ninety-six third molars were randomly divided into eight groups (n = 12) according to type of surface treatment and adhesive system: G1 = Control + Clearfil SE Bond (SE); G2 = Control + Single Bond (SB); G3 = diamond bur (DB) + SE; G4 = DB + SB, G5 = Er:YAG laser (2.94 mu m, 60 mJ, 2 Hz, 0.12 W, 19.3 J/cm(2)) + SE; G6 = Er:YAG + SB, G7 = Er,Cr:YSGG laser (2.78 mu m, 50 mJ, 30 Hz, 1.5 W, 4.5 J/cm(2)) + SE; and G8 = Er,Cr:YSGG + SB. Composite blocks were bonded to the samples, and after 24-h storage in distilled/deionized water (37 A degrees C), stick-shaped samples were obtained and submitted to mu TBS test. Bond strength values (in megapascal) were analyzed by two-way ANOVA and Tukey tests (alpha = 0.05). G1 (54.69 A +/- 7.8 MPa) showed the highest mean, which was statistically significantly higher than all the other groups (p < 0.05). For all treatments, SE showed higher bond strength than SB, except only for Er,Cr:YSGG treatment, in which the systems did not differ statistically from each other. Based on the irradiation parameters considered in this study, it can be concluded that Er:YAG and Er,Cr:YSGG irradiation presented lower values than the control group; however, their association with self-etching adhesive does not have a significantly negative effect on sound dentin (mu TBS values of > 20 MPa).
引用
收藏
页码:565 / 573
页数:9
相关论文
共 50 条
  • [41] Enhancement of Bonding to Enamel and Dentin Prepared by Er,Cr:YSGG Laser
    Obeidi, Ali
    McCracken, Michael S.
    Liu, Perng-Ru
    Litaker, Mark S.
    Beck, Preston
    Rahemtulla, Firoz
    LASERS IN SURGERY AND MEDICINE, 2009, 41 (06) : 454 - 462
  • [42] Microtensile Strength of Resin Cement Bond to Indirect Composite Treated by Different Output Powers of Er:YAG Laser
    Garshasbzadeh, Nazanin Zeinab
    Mirzaie, Mansoreh
    Yassini, Esmaeil
    Shahabi, Sima
    Benedicenti, Stefano
    Angiero, Francesca
    Chiniforush, Nasim
    MICROSCOPY RESEARCH AND TECHNIQUE, 2016, 79 (04) : 328 - 333
  • [43] Research on pulsed Er,Cr:YSGG laser ablation of dentin
    Chen, Chong
    Li, Yongliang
    2024 8TH INTERNATIONAL CONFERENCE ON BIOMEDICAL ENGINEERING AND APPLICATIONS, ICBEA 2024, 2024, : 213 - 219
  • [44] Influence of Different Pulse Durations of Er:YAG Laser Based on Variable Square Pulse Technology on Microtensile Bond Strength of a Self-Etch Adhesive to Dentin
    Baraba, Anja
    Dukic, Walter
    Chieffi, Nicoletta
    Ferrari, Marco
    Anic, Ivica
    Miletic, Ivana
    PHOTOMEDICINE AND LASER SURGERY, 2013, 31 (03) : 116 - 124
  • [45] Micromorphology and adhesive performance of Er:YAG laser-treated dentin of primary teeth
    Simon Flury
    Tamara Koch
    Anne Peutzfeldt
    Adrian Lussi
    Lasers in Medical Science, 2012, 27 : 529 - 535
  • [46] Dentin Bond Strength: Influence of Er:YAG and Nd:YAG Lasers
    Ribeiro, Carolina Ferraz
    de Paiva Goncalves, Sergio Eduardo
    Kazue Yui, Karen Cristina
    Borges, Alessandra Buehler
    Barcellos, Daphne Camara
    Brayner, Ricardo
    INTERNATIONAL JOURNAL OF PERIODONTICS & RESTORATIVE DENTISTRY, 2013, 33 (03) : 373 - 377
  • [47] Influence of Er: Cr: YSGG laser on adhesive strength and microleakage of dentin bonded to resin composite. In-vitro study
    Vohra, Fahim
    Alghamdi, Abdullah
    Aldakkan, Mohammed
    Alharthi, Sultan
    Alturaigi, Osama
    Alrabiah, Mohammed
    Al-Aali, Khulud Abdulrahman
    Alrahlah, Ali
    Naseem, Mustafa
    Abduliabbar, Tariq
    PHOTODIAGNOSIS AND PHOTODYNAMIC THERAPY, 2018, 23 : 342 - 346
  • [48] Microtensile bond strength of an etch-and-rinse adhesive to enamel and dentin after Er:YAG laser pretreatment with different pulse durations
    Esra Firat
    Sevil Gurgan
    Norbert Gutknecht
    Lasers in Medical Science, 2012, 27 : 15 - 21
  • [49] Microtensile bond strength of an etch-and-rinse adhesive to enamel and dentin after Er:YAG laser pretreatment with different pulse durations
    Firat, Esra
    Gurgan, Sevil
    Gutknecht, Norbert
    LASERS IN MEDICAL SCIENCE, 2012, 27 (01) : 15 - 21
  • [50] Shear bond strength of self-etching adhesive systems to Er:YAG-laser-prepared dentin
    Brulat, Nathalie
    Rocca, Jean-Paul
    Leforestier, Eric
    Fiorucci, Gilbert
    Nammour, Samir
    Bertrand, Marie-France
    LASERS IN MEDICAL SCIENCE, 2009, 24 (01) : 53 - 57