Microtensile bond strength analysis of adhesive systems to Er:YAG and Er,Cr:YSGG laser-treated dentin

被引:30
作者
Ramos, Thaysa Monteiro [1 ]
Ramos-Oliveira, Thayanne Monteiro [1 ]
Moretto, Simone Goncalves [1 ]
de Freitas, Patricia Moreira [1 ]
Esteves-Oliveira, Marcella [2 ]
Eduardo, Carlos de Paula [1 ]
机构
[1] Univ Sao Paulo, Sch Dent, Dept Restorat Dent, Special Lab Lasers Dent LELO, BR-05508000 Sao Paulo, Brazil
[2] Rhein Westfal TH Aachen, Dept Operat Dent Periodontol & Prevent Dent ZPP, D-52074 Aachen, Germany
基金
巴西圣保罗研究基金会;
关键词
Dentin; Er:YAG laser; Er; Cr:YSGG laser; SEM; Microtensile bond strength; ER-YAG-LASER; SELF-ETCHING PRIMER; BUR-CUT; CAVITY PREPARATION; WATER STORAGE; SURFACE; RESIN; ACID; ENAMEL; MICROLEAKAGE;
D O I
10.1007/s10103-012-1261-6
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
The aim of this in vitro study was to evaluate the effect of different surface treatments (control, diamond bur, erbium-doped yttrium aluminum garnet (Er:YAG) laser, and erbium, chromium:yttrium-scandium-gallium-garnet (Er,Cr:YSGG) laser) on sound dentin surface morphology and on microtensile bond strength (mu TBS). Sixteen dentin fragments were randomly divided into four groups (n = 4), and different surface treatments were analyzed by scanning electron microscopy. Ninety-six third molars were randomly divided into eight groups (n = 12) according to type of surface treatment and adhesive system: G1 = Control + Clearfil SE Bond (SE); G2 = Control + Single Bond (SB); G3 = diamond bur (DB) + SE; G4 = DB + SB, G5 = Er:YAG laser (2.94 mu m, 60 mJ, 2 Hz, 0.12 W, 19.3 J/cm(2)) + SE; G6 = Er:YAG + SB, G7 = Er,Cr:YSGG laser (2.78 mu m, 50 mJ, 30 Hz, 1.5 W, 4.5 J/cm(2)) + SE; and G8 = Er,Cr:YSGG + SB. Composite blocks were bonded to the samples, and after 24-h storage in distilled/deionized water (37 A degrees C), stick-shaped samples were obtained and submitted to mu TBS test. Bond strength values (in megapascal) were analyzed by two-way ANOVA and Tukey tests (alpha = 0.05). G1 (54.69 A +/- 7.8 MPa) showed the highest mean, which was statistically significantly higher than all the other groups (p < 0.05). For all treatments, SE showed higher bond strength than SB, except only for Er,Cr:YSGG treatment, in which the systems did not differ statistically from each other. Based on the irradiation parameters considered in this study, it can be concluded that Er:YAG and Er,Cr:YSGG irradiation presented lower values than the control group; however, their association with self-etching adhesive does not have a significantly negative effect on sound dentin (mu TBS values of > 20 MPa).
引用
收藏
页码:565 / 573
页数:9
相关论文
共 45 条
[1]   Bond Strengths of One-Step Self-Etch Adhesives to Laser-Irradiated and Bur-Cut Dentin After Water Storage and Thermocycling [J].
Akin, Gulsah E. ;
Herguner-Siso, Seyda ;
Ozcan, Mutlu ;
Ozel-Bektas, Ozden ;
Akin, Hakan .
PHOTOMEDICINE AND LASER SURGERY, 2012, 30 (04) :214-221
[2]   Adhesion to Er:YAG laser-prepared dentin after long-term water storage and thermocycling [J].
Amaral, F. L. B. ;
Colucci, V. ;
Souza-Gabriel, A. E. ;
Chinelatti, M. A. ;
Palma-Dibb, R. G. ;
Corona, S. A. M. .
OPERATIVE DENTISTRY, 2008, 33 (01) :51-58
[3]  
[Anonymous], 2007, P 1 INT WORKSH EV BA
[4]  
Anusavice, 2003, PHILLIPS SCI DENT MA, P394
[5]   Adhesives bonded to erbium:yttrium-aluminum-garnet laser-irradiated dentin: transmission electron microscopy, scanning electron microscopy and tensile bond strength analyses [J].
Bastos Ramos, Andreia Cristina ;
Esteves-Oliveira, Marcella ;
Arana-Chavez, Victor E. ;
Eduardo, Carlos de Paula .
LASERS IN MEDICAL SCIENCE, 2010, 25 (02) :181-189
[6]   Morphology of resin-dentin interfaces after Er,Cr:YSGG laser and acid etching preparation and application of different bonding systems [J].
Beer, Franziska ;
Buchmair, Alfred ;
Koerpert, Wolfram ;
Marvastian, Leila ;
Wernisch, Johann ;
Moritz, Andreas .
LASERS IN MEDICAL SCIENCE, 2012, 27 (04) :835-841
[7]   Current aspects on bonding effectiveness and stability in adhesive dentistry [J].
Cardoso, M. V. ;
Neves, A. de Almeida ;
Mine, A. ;
Coutinho, E. ;
Van Landuyt, K. ;
De Munck, J. ;
Van Meerbeek, B. .
AUSTRALIAN DENTAL JOURNAL, 2011, 56 :31-44
[8]  
Cardoso MV, 2008, J ADHES DENT, V10, P25
[9]   Adhesion of composite luting cement to Er: YAG-laser-treated dentin [J].
Carrieri, Teresa C. D. ;
de Freitas, Patricia M. ;
Navarro, Ricardo S. ;
Eduardo, Carlos de P. ;
Mori, Matsuyoshi .
LASERS IN MEDICAL SCIENCE, 2007, 22 (03) :165-170
[10]   Bond Strength of Adhesive Systems to Er, Cr:YSGG Laser-Irradiated Dentin [J].
Carvalho, Adriana Oliveira ;
Reis, Andre Figueiredo ;
de Oliveira, Marcelo Tavares ;
de Freitas, Patricia Moreira ;
Correa Aranha, Ana Cecilia ;
Eduardo, Carlos de Paula ;
Giannini, Marcelo .
PHOTOMEDICINE AND LASER SURGERY, 2011, 29 (11) :747-752