Influence of pre-deformation and subsequent annealing on strain hardening and anisotropy of AM30 magnesium alloy

被引:36
|
作者
Sarker, D. [1 ]
Friedman, J. [1 ]
Chen, D. L. [1 ]
机构
[1] Ryerson Univ, Dept Mech & Ind Engn, Toronto, ON M5B 2K3, Canada
基金
加拿大自然科学与工程研究理事会;
关键词
Magnesium alloy; Pre-compression; Twinning; Annealing; Recrystallization; Texture; LOW-CYCLE FATIGUE; MECHANICAL-PROPERTIES; CLIMATE-CHANGE; RARE-EARTH; RECRYSTALLIZATION BEHAVIOR; DYNAMIC RECRYSTALLIZATION; COMPRESSIVE DEFORMATION; STRETCH FORMABILITY; TENSILE DUCTILITY; HOT DEFORMATION;
D O I
10.1016/j.jallcom.2014.05.133
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
This study was aimed at evaluating the recrystallization kinetics and re-compression properties of a pre-compressed and annealed AM30 magnesium alloy with special attention to the strain hardening behavior, microstructure and texture change. Pre-compression along the extrusion direction (ED) facilitated the occurrence of {10 (1) over bar2} extension twinning due to the presence of two sets of basal textures with the c-axes aligned nearly parallel to the normal direction of the extruded plate. Most grains twinned and the c-axes of the twinned regions were rotated towards the anti-compression direction (i.e., ED) after a 4.3% pre-compression. A distinctive strain hardening stage B, characterized by an increasing strain hardening rate with a positive slope, was present. The subsequent annealing of the pre-compressed samples led to recovery, recrystallization and grain growth, and the recrystallization kinetics could be described via the Johnson-Mehl-Avrami-Kolmogorov (JMAK) model. With increasing annealing time the twins in the pre-compressed samples were observed to gradually vanish, as demonstrated by a decreased volume fraction of twins and weakened texture which became more randomly distributed. As the annealing time increased at a given temperature of 450 degrees C, the ultimate compressive strength (UCS) and the slope of strain hardening stage B decreased, while the compressive yield stress (CYS) remained nearly unchanged. With increasing annealing temperature, CYS, UCS, the extent of stage B and the slope of stage B all decreased, and the fracture strain increased. (C) 2014 Elsevier B.V. All rights reserved.
引用
收藏
页码:341 / 350
页数:10
相关论文
共 50 条
  • [31] Improved ductility of magnesium alloy sheets by pre-hardening and annealing
    He, J.
    Jiang, B.
    Yang, Q.
    Zeng, Y.
    Xia, X.
    Pan, F.
    MATERIALS SCIENCE AND TECHNOLOGY, 2015, 31 (11) : 1383 - 1387
  • [32] Effects of aluminum and copper cover tube casing on the ECAP process of AM30 magnesium alloy
    Jahadi, R.
    Sedighi, M.
    Jahed, H.
    MATERIALS AND MANUFACTURING PROCESSES, 2017, 32 (12) : 1375 - 1383
  • [33] Effect of pre-strain levels and high temperature annealing on the formability of AZ31 Mg alloy thin sheet during stretch deformation
    Wang, Lifei
    Zhang, Zhengyong
    Cao, Miao
    Zhang, Hua
    Han, Tingzhuang
    Yang, Qingshan
    Wang, Hongxia
    Cheng, Weili
    MATERIALS RESEARCH EXPRESS, 2019, 6 (08):
  • [34] The Effects of Pre-strain and Subsequent Annealing on the Yielding Behavior in a Rolled Magnesium Alloy AZ31
    Zhixiang Long
    Tianmo Liu
    Jiejun He
    Yin Zhang
    Fusheng Pan
    Journal of Materials Engineering and Performance, 2015, 24 : 16 - 23
  • [35] The Effects of Pre-strain and Subsequent Annealing on the Yielding Behavior in a Rolled Magnesium Alloy AZ31
    Long, Zhixiang
    Liu, Tianmo
    He, Jiejun
    Zhang, Yin
    Pan, Fusheng
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2015, 24 (01) : 16 - 23
  • [36] Improving the anisotropy of rolled Mg-3Al-1Zn alloy by pre-strain and annealing
    Long, Zhixiang
    Liu, Tianmo
    Wu, Yonggang
    Zhang, Yin
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2014, 616 : 240 - 245
  • [37] Dependence of compressive deformation on pre-strain and loading direction in an extruded magnesium alloy: Texture, twinning and de-twinning
    Sarker, D.
    Chen, D. L.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2014, 596 : 134 - 144
  • [38] Influence of pre-strain and heat treatment on subsequent deformation behavior of extruded AZ31 Mg alloy
    Chen, Hong-bing
    Liu, Tian-mo
    Lu, Li-wei
    He, Jie-jun
    Zhai, Yan-bo
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2015, 25 (11) : 3604 - 3610
  • [39] Effect of annealing treatments on strain rate sensitivity and anisotropy in a magnesium alloy processed by severe rolling
    del Valle, J. A.
    Ruano, O. A.
    THERMEC 2009, PTS 1-4, 2010, 638-642 : 1524 - 1529
  • [40] Effect of pre-deformation on microstructure characteristics, texture evolution and deformation mechanism of AZ31 magnesium alloy
    Li, Yuyu
    Yang, Bowen
    Han, Tingzhuang
    Chu, Zhibing
    Tuo, Leifeng
    Xue, Chun
    Yang, Qianhua
    Zhao, Xiaodong
    Gao, Hong
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 845