The InP/InGaAs material system has several beneficial material properties which enable the development of high performance optical and electrical devices. However, high quality epitaxial layers with abrupt interfaces are necessary to attain the performance predicted. Several growth techniques, including metalorganic vapor phase epitaxy (MOVPE), chemical beam epitaxy (CBE), and gas source molecular-beam epitaxy (GSMBE), have been used to grow high quality layers with varying success in achieving abrupt interfaces.([1,2,3]) The difficulty in realizing abrupt interfaces arises from the As-to-P or P-to-As exchange process that occurs at heterointerfaces during the switching of the group V species. The presence of significant levels of residual As or P can degrade the interface due to the high incorporation efficiency of these molecules on the opposite terminated surface.([4]) In order to reduce residual levels of As or P, high pumping speeds, close-coupled run/vent switching, and separate hydride crackers may be necessary. ([5]) An added concern during CBE growth is the presence of residual group III molecules which can form unwanted transition layers at interfaces during subsequent growth. Formation of the poor interfaces can lead to both an increased difficulty in the fabrication of devices, if thick interfacial layers are present, and degradation of device performance due to scattering from rough interfaces. With the use of an optimized switching scheme the formation of these interfacial layers can be minimized. Several researchers have investigated the effect of switching on interfaces. A combination of growth/group III pauses as well as group V pauses, followed by the introduction of the opposite group V source prior to growth have been used.([2,3,6]) Researchers have shown varying degrees of success in reducing the extent of the interface layers, though interface layers on the order of 2-3 monolayers still remain. Tsang, et. al., has reported the best results in terms of low-temperature photoluminescence data, however, no information is available on the switching scheme used.([1]) In this paper, the effect of a simple gas switching sequence on interface abruptness during CBE growth is studied using double crystal x-ray diffraction (DCXRD), photoluminescence (PL), and scanning tunneling microscopy (STM). Optimization of the switching sequence produces monolayer abruptness for both the InP/InGaAs and the InGaAs/InP interfaces.
引用
收藏
页码:312 / 315
页数:4
相关论文
共 50 条
  • [31] SELECTIVE GROWTH OF INGAAS ON NANOSCALE INP ISLANDS
    AHOPELTO, J
    LIPSANEN, H
    SOPANEN, M
    KOLJONEN, T
    NIEMI, HEM
    APPLIED PHYSICS LETTERS, 1994, 65 (13) : 1662 - 1664
  • [32] Growth of strained InGaAs layers on InP substrates
    Okada, T
    Weatherly, GC
    McComb, DW
    JOURNAL OF APPLIED PHYSICS, 1997, 81 (05) : 2185 - 2196
  • [33] Growth and characterisation of InGaAs/InP quantum wells
    Bose, DN
    Banerji, P
    Pal, D
    PROCEEDING OF THE TENTH INTERNATIONAL WORKSHOP ON THE PHYSICS OF SEMICONDUCTOR DEVICES, VOLS I AND II, 2000, 3975 : 142 - 148
  • [34] MBE GROWTH OF INP/INGAAS MQW MODULATORS
    SCOTT, EG
    REJMANGREENE, MAZ
    JOURNAL OF CRYSTAL GROWTH, 1991, 111 (1-4) : 1076 - 1079
  • [35] Effect of growth interruption on the electrical and optical characteristics of InP/InGaAs HEMT structures
    Radhakrishnan, K
    Patrick, THK
    Zhang, PH
    Zheng, HQ
    Yoon, SF
    Raman, A
    MICROELECTRONIC ENGINEERING, 2000, 51-2 : 433 - 440
  • [36] BOND LENGTHS AT BURIED INASP/INP INTERFACES IN INP/INGAAS MULTI-QUANTUM-WELLS
    BOSCHERINI, F
    PASCARELLI, S
    LAMBERTI, C
    BORDIGA, S
    SCHIAVINI, GM
    NUCLEAR INSTRUMENTS & METHODS IN PHYSICS RESEARCH SECTION B-BEAM INTERACTIONS WITH MATERIALS AND ATOMS, 1995, 97 (1-4): : 387 - 391
  • [37] Interfaces of InGaAs/InP multi quantum wells studied by Raman spectroscopy
    Geurts, J
    Gnoth, D
    Finders, J
    Kohl, A
    Heime, K
    PHYSICA STATUS SOLIDI A-APPLIED RESEARCH, 1995, 152 (01): : 211 - 217
  • [38] HIGH-DEPTH-RESOLUTION SIMS ANALYSIS FOR INGAAS/INP INTERFACES
    GAO, Y
    ARDELEAN, I
    RENARD, D
    ROSE, B
    JIN, Y
    APPLIED SURFACE SCIENCE, 1991, 50 (1-4) : 131 - 137
  • [39] Raman scattering analysis of InGaAs/InP: Effect of rare earth (dysprosium) addition during liquid phase epitaxial growth
    Tiginyanu, IM
    Ursaki, VV
    Podor, B
    Csontos, L
    Shontya, VP
    1996 EIGHTH INTERNATIONAL CONFERENCE ON INDIUM PHOSPHIDE AND RELATED MATERIALS, 1996, : 602 - 605
  • [40] THE GROWTH OF INP/INGAAS MULTI-QUANTUM-WELL MODULATOR ARRAYS BY GAS SOURCE MBE
    SCOTT, EG
    LYONS, MH
    REJMANGREENE, MAZ
    DAVIES, GJ
    JOURNAL OF CRYSTAL GROWTH, 1990, 105 (1-4) : 249 - 253