共 50 条
A new interpretation of SAXS peaks in sulfonated poly(ether ether ketone) (sPEEK) membranes for fuel cells
被引:46
|作者:
Mendil-Jakani, H.
[1
]
Lopez, I. Zamanillo
[1
]
Legrand, P. M.
[1
]
Mareau, V. H.
[1
]
Gonon, L.
[1
]
机构:
[1] CEA Grenoble, CEA CNRS UJF, SPrAM, UMR 5819, F-38054 Grenoble 9, France
关键词:
X-RAY-SCATTERING;
CONDUCTING MEMBRANES;
ANGLE;
NAFION;
IONOMERS;
POLYELECTROLYTES;
MORPHOLOGY;
TRANSPORT;
D O I:
10.1039/c4cp00710g
中图分类号:
O64 [物理化学(理论化学)、化学物理学];
学科分类号:
070304 ;
081704 ;
摘要:
The structure of a commercial sulfonated poly(ether ether ketone) (sPEEK) membrane was analyzed by Small-Angle X-Ray Scattering (SAXS) for different water uptakes obtained after immersion in liquid water at various temperatures. For low membrane swelling, the SAXS profile displays only a wide-angle peak in the 0.2-0.3 angstrom(-1) region. As the membrane swells, two supplementary correlation peaks arise and shift towards small angles, which are the signature of a structural evolution of the membrane, whereas the wide angle peak remains stable. The SAXS spectra of sPEEK membranes can thus display three correlation peaks simultaneously. Therefore we propose a new interpretation of these SAXS spectra which conclude that the two small angle peaks are attributed to the so-called matrix and ionomer peaks and the wide-angle peak is ascribed to the mean separation distance between sulfonic acid groups grafted onto the polymer backbone. This peak attribution implies that the sPEEK nano-phase separation is triggered by an immersion in hot water (ionomer peak apparition). Our new peak attribution was confirmed by studying the impact of temperature, electron density contrast and ionic exchange capacity.