Effect of Mn addition on the precipitation and corrosion behaviour of 22% Cr economical duplex stainless steel after isothermal aging at 800 °C

被引:10
作者
Feng, Zaiqiang [1 ]
Yang, Yinhui [2 ]
Wang, Jia [3 ]
机构
[1] North China Univ Water Resources & Elect Power, Sch Mech Engn, Zhengzhou 450045, Peoples R China
[2] Kunming Univ Sci & Technol, Sch Mat Sci & Engn, Kunming 650093, Peoples R China
[3] Tongji Univ, Sch Mat Sci & Engn, Shanghai 200092, Peoples R China
基金
中国国家自然科学基金;
关键词
Metals and alloys; Intermetallics; Microstructure; Precipitation; Corrosion; SIGMA-PHASE PRECIPITATION; MECHANICAL-PROPERTIES; MICROSTRUCTURAL STABILITY; PITTING CORROSION; RESISTANCE; 800-DEGREES-C; CHLORIDE; CAST; ENVIRONMENTS; PARAMETERS;
D O I
10.1016/j.jallcom.2017.01.031
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The microstructural and corrosion behaviour of Fe-22Cr-1.9Ni-2.3Mo-0.2N-xMn low nickel type duplex stainless steel (DSS) with Mn contents ranging from 4.3 to 9.7 wt% were studied after aging treatment at 800 degrees C lasting from 30 to 930 min. The corrosion behaviour was investigated in 3.5 wt% NaCI solution by measurements of potentiodynamic polarisation and electrochemical impedance spectroscopy. The microstructural analysis shows that the sigma precipitates mainly nucleated along gamma/delta phase boundaries and grew into the adjacent delta-ferrite by prolonging the aging time, having the same eutectoid structures as commercial high-Ni DSS. At high Mn contents, the growth rate of a precipitates was initially high with aging times from 30 to 150 min, but decreased gradually up to 930 min with more Mn participation. A Mn content of 4.3 wt% brought only about a 150 mV pitting potential (E-b) drop for the aged specimens, while further addition of Mn significantly lowered E-b at the early stage of aging with more aging-induced a precipitates. The metastable pit nucleation resistance decreased with Mn content from 4.3 to 6.9 wt% and was suppressed by a higher Mn addition of 9.7 wt% for aging treatments from 150 to 930 min. The pits mainly initiated along gamma/delta boundaries and within delta ferrite, then propagated around a precipitates with increasing aging time, and more Mn gives rise to both the number and size of pits in the early stage of aging treatment. The charge transfer resistance (Rt) depends strongly on the existence of defects caused by the a precipitates, while increasing Mn content slightly decreases the passive film resistance (Rfilm) in specimens aged from 60 to 930 min. (C) 2017 Elsevier B.V. All rights reserved.
引用
收藏
页码:334 / 344
页数:11
相关论文
共 50 条
  • [21] The effect of copper addition on the corrosion resistance of cast duplex stainless steel
    Lopes Ferreira de Lima, Hillane Mirelle
    Maior Tavares, Sergio Souto
    Martins, Marcelo
    Araujo, Walney Silva
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2019, 8 (02): : 2107 - 2119
  • [22] EFFECT OF Ce ON THE MICROSTRUCTURE AND PROPERTIES OF 27Cr-4Mo-2Ni SUPER-FERRITIC STAINLESS STEEL WITH 800 °C AGING
    Yang, Guang
    Zhao, Chenglin
    Li, Dejun
    Liao, Xiangwei
    Li, Yang
    Sun, Shen
    MATERIALI IN TEHNOLOGIJE, 2024, 58 (03): : 403 - 411
  • [23] Effect of Aging on the Corrosion Resistance of 2209 Duplex Stainless Steel Weldments
    Donghoon Kang
    Nohoon Kim
    Haewoo Lee
    Metals and Materials International, 2019, 25 : 740 - 750
  • [24] Investigation on the Corrosion Behavior of Lean Duplex Stainless Steel 2404 after Aging within the 650-850 °C Temperature Range
    Zanotto, Federica
    Grassi, Vincenzo
    Balbo, Andrea
    Zucchi, Fabrizio
    Monticelli, Cecilia
    METALS, 2019, 9 (05)
  • [25] Study of the effect of sigma phase precipitation on the sliding wear and corrosion behaviour of duplex stainless steel AISI 2205
    del Abra-Arzola, J. L.
    Garcia-Renteria, M. A.
    Cruz-Hernandez, V. L.
    Garcia-Guerra, J.
    Martinez-Landeros, V. H.
    Falcon-Franco, L. A.
    Curiel-Lopez, F. F.
    WEAR, 2018, 400 : 43 - 51
  • [26] Influence of Isothermal Aging on the Embrittlement of 00Cr25Ni7Mo4N Super Duplex Stainless Steel
    Wang, Xiaofeng
    Chen, Weiqing
    STEEL RESEARCH INTERNATIONAL, 2009, 80 (10) : 779 - 784
  • [27] Effect of Short-Time Aging on the Pitting Corrosion Behavior of a Novel Lean Duplex Stainless Steel 2002
    Sun, Tian-Yi
    Guo, Yan-Jun
    Jiang, Yi-Ming
    Li, Jin
    ACTA METALLURGICA SINICA-ENGLISH LETTERS, 2019, 32 (06) : 755 - 763
  • [28] Effect of ageing on precipitation and impact energy of 2101 economical duplex stainless steel
    Zhang Wei
    Jiang Laizhu
    Hu Jincheng
    Song Hongmei
    MATERIALS CHARACTERIZATION, 2009, 60 (01) : 50 - 55
  • [29] 22Cr High-Mn-N Low-Ni Economical Duplex Stainless Steels
    Jiang Da-wei
    Ge Chang-sheng
    Zhao Xiang-juan
    Li Jun
    Shi Lu-lu
    Xiao Xue-shan
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2012, 19 (02) : 50 - 56
  • [30] Effect of Thermal Aging Conditions on the Corrosion Properties and Hardness of a Duplex Stainless Steel
    May, Jose Eduardo
    Caldas de Souza, Carlos Alberto
    de Paula Nascente, Pedro Augusto
    Soares, Paulo
    Lepienski, Carlos Mauricio
    Kuri, Sebastiao Elias
    MATERIALS RESEARCH-IBERO-AMERICAN JOURNAL OF MATERIALS, 2010, 13 (04): : 431 - 436