On microstructure and corrosion behaviour of AlSi10Mg alloy with low surface roughness fabricated by direct metal laser sintering

被引:58
|
作者
Fathi, P. [1 ]
Rafieazad, M. [1 ]
Duan, X. [1 ]
Mohammadi, M. [2 ]
Nasiri, A. M. [1 ]
机构
[1] Mem Univ Newfoundland, Fac Engn & Appl Sci, St John, NF A1B 3X5, Canada
[2] Univ New Brunswick, MAMCE, Fredericton, NB E3B 5A3, Canada
基金
加拿大自然科学与工程研究理事会;
关键词
Additive manufacturing (AM); Direct metal laser sintering (DMLS); AlSi10Mg; Surface roughness; Corrosion; Microstructure; A356; ALUMINUM-ALLOY; MECHANICAL-PROPERTIES; PITTING CORROSION; PROCESS PARAMETERS; ENERGY DENSITY; HEAT-TREATMENT; RESISTANCE; PRODUCTS; TEXTURE;
D O I
10.1016/j.corsci.2019.05.032
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this study, in-depth microstructure and electrochemical properties of highly smoothed AlSi10Mg parts fabricated through direct-metal-laser-sintering are reported. The samples with the lowest surface roughness were characterized by having a periodic large and small melt pools (MPs) pattern in their upskin layers. Consequently, a noticeably coarser eutectic-Si network, Al-dendrite and grain size formed along the larger MPs' borders, rationalized by their slower solidification rate. Such microstructural features were found to control/deteriorate the electrochemical performance of the as-printed samples than their surface roughness. An improved electrochemical stability for the samples that experience the fastest solidification rate along their MP-boundaries was revealed.
引用
收藏
页码:126 / 145
页数:20
相关论文
共 50 条
  • [1] On microstructure and early stage corrosion performance of heat treated direct metal laser sintered AlSi10Mg
    Rafieazad, Mehran
    Mohammadi, Mohsen
    Nasiri, Ali M.
    ADDITIVE MANUFACTURING, 2019, 28 : 107 - 119
  • [2] Corrosion in laser powder bed fusion AlSi10Mg alloy
    Laieghi, Hossein
    Kvvssn, Varma
    Butt, Muhammad Muteeb
    Ansari, Peyman
    Salamci, Metin U.
    Patterson, Albert E.
    Salamci, Elmas
    ENGINEERING REPORTS, 2024, 6 (10)
  • [3] Effect of surface roughness on corrosion fatigue performance of AlSi10Mg alloy produced by Selective Laser Melting (SLM)
    Leon, Avi
    Aghion, Eli
    MATERIALS CHARACTERIZATION, 2017, 131 : 188 - 194
  • [4] Effect of Direct Aging on Corrosion Behavior of AlSi10Mg Alloy Fabricated by Laser Powder Bed Fusion
    Zhang, Zhen
    Zhao, Zhanyong
    Li, Xiaofeng
    Wang, Beibei
    Bai, Peikang
    ACTA METALLURGICA SINICA-ENGLISH LETTERS, 2024, 37 (02) : 266 - 282
  • [5] Achieving low surface roughness AlSi10Mg_200C parts using direct metal laser sintering
    Mohammadi, Mohsen
    Asgari, Hamed
    ADDITIVE MANUFACTURING, 2018, 20 : 23 - 32
  • [6] Low Surface Roughness Additively Manufactured AlSi10Mg: The Impacts on Corrosion and Water Repellency Properties
    Fathi, P.
    Mohammadi, M.
    Nasiri, A. M.
    TMS 2020 149TH ANNUAL MEETING & EXHIBITION SUPPLEMENTAL PROCEEDINGS, 2020, : 309 - 320
  • [7] Size dependence of microstructure of AlSi10Mg alloy fabricated by selective laser melting
    Takata, Naoki
    Kodaira, Hirohisa
    Suzuki, Asuka
    Kobashi, Makoto
    MATERIALS CHARACTERIZATION, 2018, 143 : 18 - 26
  • [8] Anti-corrosion and wear resistance properties of AlSi10Mg alloy and SiC/AlSi10Mg composites fabricated by selective laser melting
    Ding, Xueping
    Zhang, Qi
    Zhou, Yinying
    Guo, Yaoqi
    Tang, Min
    Gong, Yuan
    CAILIAO GONGCHENG-JOURNAL OF MATERIALS ENGINEERING, 2024, 52 (10): : 97 - 105
  • [9] Comparing microstructure and hardness of direct metal laser sintered AlSi10Mg alloy between different planes
    Ghasri-Khouzani, M.
    Peng, H.
    Attardo, R.
    Ostiguy, P.
    Neidig, J.
    Billo, R.
    Hoelzle, D.
    Shankar, M. R.
    JOURNAL OF MANUFACTURING PROCESSES, 2019, 37 : 274 - 280
  • [10] A review on the fatigue behaviour of AlSi10Mg alloy fabricated using laser powder bed fusion technique
    Raja, A.
    Cheethirala, Srinivasa Rakesh
    Gupta, Pallavi
    Vasa, Nilesh J.
    Jayaganthan, R.
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2022, 17 : 1013 - 1029