Effect of SiO2 Content on the Extended Creep Behavior of SiO2-Based Wood-Inorganic Composites Derived via the Sol-Gel Process Using the Stepped Isostress Method

被引:8
作者
Hung, Ke-Chang [1 ]
Wu, Jyh-Horng [1 ]
机构
[1] Natl Chung Hsing Univ, Dept Forestry, Taichung 402, Taiwan
关键词
SiO2-based wood-inorganic composites; sol-gel process; creep behavior; stepped isostress method; activation volume; PREDICTION; RESISTANCE; FIBERS; METHACRYLATE; COMBINATION; DECAY;
D O I
10.3390/polym10040409
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
In this study, methyltrimethoxysilane (MTMOS) was used as a reagent to prepare SiO2-based wood-inorganic composites (WICSiO2) via the sol-gel process, and subsequently, the extended creep behaviors of WICSiO2 with weight percent gains (WPGs) of 10%, 20%, and 30% were estimated using the stepped isostress method (SSM). The results revealed that the density of all samples ranged from 426 to 513 kg/m(3), and no significant difference in the modulus of elasticity (MOE) was noted among all of the samples (10.5-10.7 GPa). However, the MOR of WICSiO2 with a WPG of 20% (102 MPa) was significantly greater than that of untreated wood (87 MPa). In addition, according to the result using the SSM, the SSM-predicted creep master curve fitted well with the experimental data for the untreated wood and WICSiO2. This result demonstrated that the SSM could be a useful method to evaluate long-term creep behaviors of wood and WICSiO2. Furthermore, the activation volume (V*) of the specimens was calculated from the linear slope of Eyring plots, and the resulting V* of all of the WICSiO2 (0.754-0.842 nm(3)) was lower than that of untreated wood (0.856 nm(3)). On the other hand, the modulus reduction of untreated wood showed 39%, 45%, 48%, and 51% at 5, 15, 30, and 50 years, respectively. In contrast, the modulus reduction of the WICSiO2 with a WPG of 10% decreased to 25%, 31%, 35%, and 38% at 5, 15, 30, and 50 years, respectively. Similar trends were also observed for other WICSiO2 with different WPGs. Of these, the WICSiO2 with a WPG of 20% exhibited the lowest reduction in time-dependent modulus (31%) over a 50-year period. Accordingly, the creep resistance of the wood could be effectively enhanced under the MTMOS treatment.
引用
收藏
页数:12
相关论文
共 42 条
  • [1] Accelerated creep testing of polymers using the stepped isothermal method
    Achereiner, Frederic
    Engelsing, Kurt
    Bastian, Martin
    Heidemeyer, Peter
    [J]. POLYMER TESTING, 2013, 32 (03) : 447 - 454
  • [2] Accelerated creep testing for aramid fibres using the stepped isothermal method
    Alwis, K. G. N. C.
    Burgoyne, C. J.
    [J]. JOURNAL OF MATERIALS SCIENCE, 2008, 43 (14) : 4789 - 4800
  • [3] ASTM, 2009, D790 ASTM
  • [4] ASTM, 2006, D1037 ASTM
  • [5] Accessibility of hydroxyl groups in anhydride modified wood as measured by deuterium exchange and saponification
    Beck, Greeley
    Strohbusch, Sarah
    Larnoy, Erik
    Militz, Holger
    Hill, Callum
    [J]. HOLZFORSCHUNG, 2018, 72 (01) : 17 - 23
  • [6] Temperature effects on creep behavior of continuous fiber GMT composites
    Dasappa, Prasad
    Lee-Sullivan, Pearl
    Xiao, Xinran
    [J]. COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2009, 40 (08) : 1071 - 1081
  • [7] Dong X., 2016, APPL CATAL B-ENVIRON, V1, P56
  • [8] Findley WN., 1976, CREEP RELAXATION NON
  • [9] Silane nanofilm formation by sol-gel processes for promoting adhesion of waterborne and solvent-borne coatings to wood surface
    Gholamiyan, Hadi
    Tarmian, Asghar
    Ranjbar, Zahra
    Abdulkhani, Ali
    Azadfallah, Mohammad
    Mai, Carsten
    [J]. HOLZFORSCHUNG, 2016, 70 (05) : 429 - 437
  • [10] Accelerated and real-time creep and creep-rupture results for aramid fibers
    Giannopoulos, Ioannis P.
    Burgoyne, Chris J.
    [J]. JOURNAL OF APPLIED POLYMER SCIENCE, 2012, 125 (05) : 3856 - 3870