Analysis of Factors Affecting Free Surface Vortex Formation during Steel Teeming

被引:27
|
作者
Li, Hong-Xia [1 ]
Wang, Qiang [1 ,2 ]
Jiang, Jia-Wei [1 ]
Lei, Hong [1 ]
Guo, Zhan-Cheng [2 ]
He, Ji-Cheng [1 ]
机构
[1] Northeastern Univ, Key Lab Electromagnet Proc Mat, Minist Educ, Shenyang 110819, Peoples R China
[2] Univ Sci & Technol Beijing, State Key Lab Adv Met, Beijing 100083, Peoples R China
基金
中国国家自然科学基金;
关键词
clean steel; inclusions; vortex; steel teeming; BATH-TUB VORTEX; DRAINING OPERATIONS; LADLE; SIMULATION;
D O I
10.2355/isijinternational.ISIJINT-2015-096
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
To suppress slag entrapment by vortexes during steel teeming, and to improve steel cleanliness, key factors affecting free surface vortex formation have been analyzed in this study. It was found that Coriolis forces have little effect on vortex formation. The initial tangential disturbance is the main factor for vortex formation. And when the nozzle position is central or eccentric, the effects of initial tangential velocity, nozzle diameter on the critical height are different. Physical properties of liquid steel have a small effect on the critical height. A formula for calculating the height was discussed.
引用
收藏
页码:94 / 102
页数:9
相关论文
共 50 条
  • [1] Mechanism Analysis of Free-Surface Vortex Formation during Steel Teeming
    Li, Hong-Xia
    Wang, Qiang
    Lei, Hong
    Jiang, Jia-Wei
    Guo, Zhan-Cheng
    He, Ji-Cheng
    ISIJ INTERNATIONAL, 2014, 54 (07) : 1592 - 1600
  • [2] FORMATION MECHANISM AND INFLUENCE FACTORS OF SINK VORTEX DURING LADLE TEEMING
    Tang Haiyan
    Liang Yongchang
    ACTA METALLURGICA SINICA, 2016, 52 (05) : 519 - 528
  • [3] Suppression Mechanism and Method of Vortex During Steel Teeming Process in Ladle
    Wang Qiang
    Wang Lianyu
    Li Hongxia
    Jiang Jiawei
    Zhu Xiaowei
    Guo Zhancheng
    He Jicheng
    ACTA METALLURGICA SINICA, 2018, 54 (07) : 959 - 968
  • [4] Factors affecting surface roughness of low carbon resulfurized free cutting steel
    Imanami, Yuta
    Tomita, Kunikazu
    Nishimura, Kimihiro
    JFE Technical Report, 2018, (23): : 43 - 48
  • [5] Suppression and Control of Vortex Formation Caused by Boundary Disturbance during Ladle Teeming Process
    Wang, Ziming
    Li, Yue
    Sun, Benchen
    Zhou, Xiaobin
    Yue, Qiang
    STEEL RESEARCH INTERNATIONAL, 2024, 95 (08)
  • [6] Formation and Influencing Factors of Free Surface Vortex in a Barrel with a Central Orifice at Bottom
    Hai-feng Li
    Hong-xun Chen
    Zheng Ma
    Yi Zhou
    Journal of Hydrodynamics, 2009, 21 : 238 - 244
  • [7] FORMATION AND INFLUENCING FACTORS OF FREE SURFACE VORTEX IN A BARREL WITH A CENTRAL ORIFICE AT BOTTOM
    Li Hai-feng
    Chen Hong-xun
    Ma Zheng
    Zhou Yi
    JOURNAL OF HYDRODYNAMICS, 2009, 21 (02) : 238 - 244
  • [9] Optimizing Design of Vortex Suppression Utilizing Static Electromagnetic Field during Steel Teeming from Ladle
    He, Ming
    Ma, Shuai
    Zhao, Lijia
    Zhu, Xiaowei
    Jiang, Zhouhua
    Wang, Qiang
    STEEL RESEARCH INTERNATIONAL, 2023, 94 (01)
  • [10] LIBERATION OF GASES AND FORMATION OF SKIN BLOWHOLES DURING TEEMING AND SOLIDIFICATION OF KILLED STEEL INGOTS
    VOLKER, W
    TECHNISCHE MITTEILUNGEN KRUPP FORSCHUNGSBERICHTE, 1968, 26 (3-4): : 95 - &