Influence of the Crack Spacing in the Coating Layer on the Progress of Interfacial Debonding in Galvannealed Steel Pulled in Tension

被引:2
作者
Iwamoto, Sohei [1 ]
Ochiai, Shojiro [1 ]
Okuda, Hiroshi [1 ]
机构
[1] Kyoto Univ, Grad Sch Engn, Sakyo Ku, Kyoto 6068501, Japan
基金
日本学术振兴会;
关键词
finite element analysis; galvannealed steel; coating; cracking; spalling; interface; MULTIPLE-CRACKING; STRESS-ANALYSIS; STRAIN; STRENGTH; FRACTURE; FRAGMENTATION; MECHANISMS;
D O I
10.2355/isijinternational.49.431
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The coefficient of thermal expansion of the coating layer of the hot-dipped galvannealed steels is higher than that of the substrate steel. Accordingly, the coating layer shows multiple cracking during cooling due to the thermally induced stress. When tensile stress is applied externally on the coated steels, the coating layer exhibits further multiple cracking perpendicular to the tensile direction. As a result, the coating layer is multiply-cracked both in tensile and sample width directions. Under such existent cracks, the coating layer is spalled due to the interfacial debonding induced by the buckling of the coating layer in the sample width direction. In the present work, the influences of the crack spacing in the tensile direction and that in the sample width direction on the spalling process of the coating layer were studied with the finite element stress analysis. The results of analysis showed that (a) the larger the crack spacing of the coating layer in the tensile direction, the more occurs the interfacial debonding and (b) the crack spacing in the tensile direction affects especially on the initial spalling behavior; the larger the spacing, the more the spalling is enhanced. On the other hand, the crack spacing in the sample width direction affects only slightly on the initial spalling behavior, while the larger the spacing, the larger becomes the debonding area in the later stage.
引用
收藏
页码:431 / 438
页数:8
相关论文
共 24 条
[1]   Effect of microstructure on fracture mechanisms in galvannealed coatings [J].
Alpas, AT ;
Inagaki, J .
ISIJ INTERNATIONAL, 2000, 40 (02) :172-181
[2]   Analysis of brittle coating fragmentation under uniaxial tension for Weibull strength distributions [J].
Andersons, J ;
Handge, UA ;
Sokolov, IM ;
Blumen, A .
EUROPEAN PHYSICAL JOURNAL B, 2000, 17 (02) :261-268
[3]   RELAXATION OF STRESSES BY CRACKS IN INTERMETALLIC COATINGS - APPLICATION TO GALVANIZING [J].
FOCT, J .
SCRIPTA METALLURGICA ET MATERIALIA, 1993, 28 (01) :127-132
[4]   THE CRACKING AND DECOHESION OF THIN-FILMS ON DUCTILE SUBSTRATES [J].
HU, MS ;
EVANS, AG .
ACTA METALLURGICA, 1989, 37 (03) :917-925
[5]  
IOST A, 1993, J MATER SCI LETT, V12, P1340, DOI 10.1007/BF00241701
[6]  
Iwamoto S, 2005, TETSU TO HAGANE, V91, P335
[7]   Analysis of buckling and interfacial debonding of galvannealed coating layer on steel substrates under applied tensile strain [J].
Iwamoto, Sohei ;
Ochiai, Shojiro ;
Okuda, Hiroshi ;
Inoue, Tadanobu .
ISIJ INTERNATIONAL, 2007, 47 (06) :930-934
[8]   Analysis of Group-buckling and -debonding Behaviors of Galvannealed Coating Layer on Steel Substrates under Applied Tensile Strain [J].
Iwamoto, Sohei ;
Ochia, Shojiro ;
Okuda, Hiroshi .
ISIJ INTERNATIONAL, 2009, 49 (01) :139-145
[9]   Finite Element Analysis of the Interfacial Debonding of the Galvannealed Coating Layer with High Tensile Strength Steel Substrates [J].
Iwamoto, Sohei ;
Ochiai, Shojiro ;
Okuda, Hiroshi .
ISIJ INTERNATIONAL, 2009, 49 (01) :119-123
[10]   INTERFACIAL LAYER DEVELOPMENT IN HOT-DIP GALVANNEAL COATINGS ON INTERSTITIAL-FREE (IF) STEEL [J].
JORDAN, CE ;
GOGGINS, KM ;
MARDER, AR .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1994, 25 (10) :2101-2109