Hydrogen embrittlement sensitivity of X100 pipeline steel under different pre-strain

被引:68
作者
Han, Y. D. [1 ,2 ]
Wang, R. Z. [1 ,2 ]
Wang, H. [1 ,2 ]
Xu, L. Y. [1 ,2 ,3 ]
机构
[1] Tianjin Univ, Sch Mat Sci & Engn, Tianjin 300072, Peoples R China
[2] Tianjin Key Lab Adv Joining Technol, Tianjin 300072, Peoples R China
[3] Tianjin Univ, State Key Lab Engines, Tianjin 300050, Peoples R China
基金
中国国家自然科学基金;
关键词
X100 pipeline steel; Pre-strain; Hydrogen embrittlement sensitivity; Hydrogen permeation; INDUCED CRACKING; BEHAVIOR; STRESS; MICROSTRUCTURE; TEXTURE; GROWTH; IRON;
D O I
10.1016/j.ijhydene.2019.06.054
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
In the present study, the influences of hydrogen on the mechanical properties as well as the pre-strain on the HE susceptibility of X100 pipeline steel were investigated by combining electrochemical hydrogen charging and tensile experiments. Both the yield and tensile strength decrease with the increasing hydrogen charging time no matter the values of pre-strain. When the charging time is 12 h, the yield strength and tensile strength was reduced by 3% and 9%, respectively. The longer the charging time, the stronger the HE damage of the steel. Besides, when the hydrogen charging time is same, HE sensitivity increases with the pre-strain values. When the charging time is 6 h, the HE sensitivity coefficient is 40.24% without pre-strain, and it increases to 49.26% with the pre-strain value increases to the 2%. The hydrogen effective diffusion coefficient reduces gradually with the increasing pre-strain values. The coefficient is 5.45 x 10(-7) cm(2)/s without pre-strain and it reduces to 1.21 x 10(-7) cm(2)/s with the pre-strain value increases to the 3%. When the hydrogen charging time is same, HE sensitivity increases with the pre-strain values. (C) 2019 Hydrogen Energy Publications LLC. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:22380 / 22393
页数:14
相关论文
共 29 条
[1]   Hydrogen permeation in iron at different temperatures [J].
Addach, H ;
Berçot, P ;
Rezrazi, M ;
Wery, M .
MATERIALS LETTERS, 2005, 59 (11) :1347-1351
[2]  
[Anonymous], 2004, 170812004E 2S3
[3]   The influence of chemical composition and microstructure of API linepipe steels on hydrogen induced cracking and sulfide stress corrosion cracking [J].
Carneiro, RA ;
Ratnapuli, RC ;
Lins, VD .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2003, 357 (1-2) :104-110
[4]  
Corbett KT, 2004, INT J OFFSHORE POLAR, V14, P75
[5]  
Crank J., 1979, The Mathematics of Diffusion
[6]   Effect of hydrogen concentration on strain behaviour of pipeline steel [J].
Dmytrakh, I. M. ;
Leshchak, R. L. ;
Syrotyuk, A. M. .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2015, 40 (10) :4011-4018
[7]   Evolution of the microstructure and texture of X70 pipeline steel during cold-rolling and annealing treatments [J].
Eskandari, M. ;
Mohtadi-Bonab, M. A. ;
Szpunar, J. A. .
MATERIALS & DESIGN, 2016, 90 :618-627
[8]   Effect of hydrogen and low temperature on fatigue crack growth of pipeline steels [J].
Fassina, P. ;
Brunella, M. F. ;
Lazzari, L. ;
Re, G. ;
Vergani, L. ;
Sciuccati, A. .
ENGINEERING FRACTURE MECHANICS, 2013, 103 :10-25
[9]  
Fujita FranciscoEiichi., 1985, HYDROGEN DEGRADATION, P1
[10]   Hydrogen Evolution and Absorption in an API X100 Line Pipe Steel Exposed to Near-Neutral pH Solutions [J].
Ha, Hung M. ;
Gadala, Ibrahim M. ;
Alfantazi, Akram .
ELECTROCHIMICA ACTA, 2016, 204 :18-30