摘要
Conventionally produced high pressure die-cast (HPDC) components are not considered to be heat treatable because gases entrapped during the die-casting process expand during solution treatment causing unacceptable surface blistering. Components may also become dimensionally unstable. Both these effects prevent the heat treatment of die-castings as these phenomena are detrimental to the visual appearance, mechanical properties and utilisation of the component. Recent work has revealed a process window in which HPDC aluminium alloys that are capable of responding to age hardening may be successfully heat treated without encountering these problems. As a result, improvements of greater than 100% in the tensile properties are possible, when compared with the as-cast condition. The new heat treatment schedules are described for HPDC parts of different size and shape, the role of chemistry on ageing is discussed and microstructural development during heat treatment examined.
引用
收藏
页码:351 / 358
页数:8
相关论文
共 50 条
  • [31] HARD INCLUSIONS IN PRESSURE DIE-CASTING
    LIPHARDT, WF
    DIE CASTING ENGINEER, 1987, 31 (04): : 42 - &
  • [32] On the Use of Conformal Cooling in High-Pressure Die-Casting and Semisolid Casting
    Jarfors, Anders E. W.
    Sevastopol, Ruslan
    Seshendra, Karamchedu
    Zhang, Qing
    Steggo, Jacob
    Stolt, Roland
    TECHNOLOGIES, 2021, 9 (02)
  • [33] Studies on Flow Characteristics at High-Pressure Die-Casting
    Schneiderbauer, S.
    Pirker, S.
    Chimani, C.
    Kretz, R.
    3RD INTERNATIONAL CONFERENCE ON ADVANCES IN SOLIDIFICATION PROCESSES, 2012, 27
  • [35] PRESSURE DIE-CASTING AND MANAGEMENT - REPORT ON THE 9TH INTERNATIONAL PRESSURE DIE-CASTING EXHIBIT, BASEL
    MALLE, K
    WERKSTATTSTECHNIK ZEITSCHRIFT FUR INDUSTRIELLE FERTIGUNG, 1980, 70 (12): : 803 - 805
  • [36] STUDIES ON FLOW CHARACTERISTICS AT HIGH-PRESSURE DIE-CASTING
    Chimani, Christian. M.
    Kretz, Richard
    Schneiderbauer, Simon
    Puttinger, Stefan
    Pirker, Stefan
    LIGHT METALS 2012, 2012, : 443 - 447
  • [37] Failures of dies for die-casting of aluminium alloys
    Kosec, B.
    METALURGIJA, 2008, 47 (01): : 51 - 55
  • [38] BASIC METALLURGY OF THE MAGNESIUM DIE-CASTING ALLOYS
    KAPLAN, HI
    DIE CASTING ENGINEER, 1986, 30 (06): : 44 - 49
  • [39] Failures of dies for die-casting of aluminium alloys
    Faculty of Natural Sciences and Engineering, University of Ljubljana, Ljubljana, Slovenia
    Metalurgija, 2008, 1 (51-55):
  • [40] MODERN DIE-CASTING MACHINES FOR ZINC ALLOYS
    CHIVERS, ARL
    METALL, 1975, 29 (09): : 938 - 941