cBN-Al2O3 composites in NaCl environment under high pressure and high temperature conditions

被引:4
作者
Chu, Dongliang [1 ]
Ma, Hongan [1 ]
Wang, Jian [1 ]
Zhang, Zhuangfei [2 ]
Shen, Weixia [2 ]
Jia, Xiaopeng [1 ]
机构
[1] Jilin Univ, Coll Phys, State Key Lab Superhard Mat, Changchun, Jilin, Peoples R China
[2] Zhengzhou Univ, Sch Phys & Engn, Minist Educ, Key Lab Mat Phys, Zhengzhou, Henan, Peoples R China
基金
中国国家自然科学基金;
关键词
cBN-Al2O3; composites; NaCl environment; HPHT; Thermogravimetric analysis; Vickers hardness; CBN; AL;
D O I
10.1016/j.ceramint.2019.05.215
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
A series of experiments of cubic boron nitride (cBN)-Al2O3 composites was conducted in NaCl environment under a pressure of 5 GPa at 1200-1650 degrees C using a Chinese multi-anvil high-pressure apparatus. The oxidation resistance of cBN-Al2O3 composites reached 1300 degrees C, which was 200 degrees C higher than that of raw cBN powder. The porosity was estimated by the content of NaCl impurities in cBN-Al2O3 composites. The content of NaCl impurity increases with increasing temperature and decreases with increasing Al2O3 level under high pressure and high temperature conditions. cBN + 30 vol% Al2O3 sintered at 5 GPa and 1200 degrees C shows no NaCl impurity, and the Vickers hardness of the sample is 21.6 GPa which is half of cBN +10 vol% Al.
引用
收藏
页码:16792 / 16796
页数:5
相关论文
共 50 条
  • [31] Effect of High-Energy Milling and Sintering Temperature on the Properties of Al2O3-WC-Co Composites
    Azevedo, Heytor V. S. B.
    Raimundo, Rafael A.
    Silva, David D. S.
    Morais, Luis M. F.
    Costa, Francine A.
    Macedo, Daniel A.
    Cavalcante, Danielle G. L.
    Gomes, Uilame U.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2021, 30 (02) : 1504 - 1512
  • [32] Effect of cBN content and additives on sliding and surface fatigue wear of spark plasma sintered Al2O3-cBN composites
    Kumar, Rahul
    Antonov, Maksim
    Klimczyk, Piotr
    Mikli, Valdek
    Gomon, Dmitri
    WEAR, 2022, 494-495
  • [34] PROCESSING AND HIGH-TEMPERATURE DEFORMATION OF AL2O3 FIBER-REINFORCED NIALFE MATRIX COMPOSITES
    LIU, C
    JENG, SM
    YANG, JM
    AMATO, RA
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1995, 191 (1-2): : 49 - 59
  • [35] Wetting of MgO and α-Al2O3 by molten Mg: a model of droplet with high vapor pressure
    Fujii, Hidetoshi
    Izutani, Shun
    JOURNAL OF MATERIALS SCIENCE, 2012, 47 (24) : 8387 - 8394
  • [36] High temperature oxidation behaviour of Al2O3/Al composite coating on γ-TiAl
    Xu, Y.
    Liang, W.
    Miao, Q.
    Jiang, Q.
    Ren, B.
    Yao, Z.
    Zhang, P.
    Wei, D.
    SURFACE ENGINEERING, 2015, 31 (05) : 354 - 360
  • [37] Preparation and Properties of β-SiAlON-cBN Composites Using Y2O3, B2O3 and Al as Additives
    He, Chao
    Shi, Xiaofei
    Yue, Xinyan
    Wang, Jianjun
    Ru, Hongqiang
    HIGH-PERFORMANCE CERAMICS VIII, 2014, 602-603 : 380 - 383
  • [38] Synthesis of an (Al3BC + Al2O3)/Al composite with high stiffness and attractive high-temperature tensile properties
    Hu, Jingyi
    Gao, Tong
    Li, Mengyu
    Liu, Xiangfa
    MATERIALS RESEARCH LETTERS, 2024, 12 (05): : 355 - 362
  • [39] Microstructure and properties of large bulk Al2O3/ZrO2 (Y2O3) composites prepared by SHS under high gravity
    W. Y. Liu
    Z. M. Zhao
    L. Zhang
    L. Wang
    International Journal of Self-Propagating High-Temperature Synthesis, 2009, 18 (3) : 180 - 185
  • [40] A Comparative Study of High Temperature Corrosion of Al2O3, SiO2 and Al2O3–SiO2 Forming Alloys in a Na2SO4–NaCl Atmosphere
    Toto Sudiro
    Tomonori Sano
    Shoji Kyo
    Osamu Ishibashi
    Masaharu Nakamori
    Kazuya Kurokawa
    Oxidation of Metals, 2013, 80 : 589 - 597