Effects of Sample and Indenter Configurations of Nanoindentation Experiment on the Mechanical Behavior and Properties of Ductile Materials

被引:22
作者
Koloor, Seyed Saeid Rahimian [1 ]
Karimzadeh, Atefeh [1 ]
Tamin, Mohd Nasir [1 ]
Abd Shukor, Mohd Hamdi [2 ]
机构
[1] Univ Teknol Malaysia, Fac Mech Engn, Dept Appl Mech & Design, Computat Solid Mech Lab, Johor Baharu 81310, Malaysia
[2] Univ Malaya, Ctr Adv Mfg & Mat Proc, Kuala Lumpur 50603, Malaysia
关键词
aluminum; 1100; nanoindentation test; indentation plane orientation; indenter edge-tip radius; indentation depth; finite element simulation; FINITE-ELEMENT; GRAIN-BOUNDARY; INSTRUMENTED INDENTATION; NANO-INDENTATION; SPHERICAL INDENTATION; FRACTURE-TOUGHNESS; LENGTH SCALES; SIZE; PLASTICITY; TILT;
D O I
10.3390/met8060421
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The nanoindentation test is frequently used as an alternate method to obtain the mechanical properties of ductile materials. However, due to the lack of information about the effects of the sample and indenter physical configurations, the accuracy of the extracted material properties in nanoindentation tests requires further evaluation that has been considered in this study. In this respect, a demonstrator ductile material, aluminum 1100, was tested using the Triboscope nanoindenter system with the Berkovich indenter. A 3D finite element simulation of the nanoindentation test was developed and validated through exact prediction of the structural response with measured data. The validated model was then employed to examine the effects of various test configurations on the load-displacement response of the sample material. These parameters were the different indenter edge-tip radii, different indentation depths, different sample tilts, and different friction conditions between the indenter and the material surface. Within the range of the indenter edge-tip radii examined, the average elastic modulus and hardness were 78.34 +/- 14.58 and 1.6 +/- 0.24 GPa, respectively. The different indentation depths resulted in average values for the elastic modulus and hardness of 77.03 +/- 6.54 and 1.58 +/- 0.17 GPa, respectively. The uneven surface morphology, as described by the inclination of the local indentation plane, indicated an exponential increase in the extracted values of elastic modulus and hardness, ranging from 71.83 and 1.47 GPa (for the reference case, theta = 0 degrees) to 243.39 and 5.05 GPa at theta = 12 degrees. The mechanical properties that were obtained through nanoindentation on the surface with 6 degrees tilt or higher were outside the range for aluminum properties. The effect of friction on the resulting mechanical response and the properties of the material was negligible.
引用
收藏
页数:18
相关论文
共 50 条
[41]   Nanoindentation measurements of mechanical properties and creep behavior of Niutitang formation shale rocks, China [J].
Wang, Jianfeng ;
Niu, Jungang ;
Yang, Chao ;
Jiang, Wenmin ;
Li, Yun ;
Zheng, Yijun ;
Liao, Yuhong ;
Feng, Dingyu ;
Peng, Ping'an ;
Xiong, Yongqiang .
FRONTIERS IN EARTH SCIENCE, 2025, 13
[42]   Mechanical properties of superhard materials synthesised at various pressure-temperature conditions investigated by nanoindentation [J].
Richter, Asta ;
Smith, Roger ;
Dubrovinskaia, Natalia ;
McGee, Edward .
HIGH PRESSURE RESEARCH, 2006, 26 (02) :99-109
[43]   Mechanical properties of 2D materials: A review on molecular dynamics based nanoindentation simulations [J].
Patra, Lokanath ;
Pandey, Ravindra .
MATERIALS TODAY COMMUNICATIONS, 2022, 31
[44]   Numerical study of interfacial crack growth effects on nanoindentation mechanical properties in presence of pre-existing defect [J].
Pejman, Reza ;
Salehi, S. Hassan ;
Salehi, Manouchehr .
THIN SOLID FILMS, 2013, 545 :408-413
[45]   Effects of indenter radius and temperature on mechanical capacities of crystalline Cu/Cu50Ta50 metallic glasses multilayers during nanoindentation [J].
Nguyen, Van-Ha ;
Tran, Anh-Son ;
Chu, Van-Tuan ;
Doan, Dinh-Quan ;
Pham, Anh-Vu ;
Nguyen, Van-Thoai ;
Hoang, Van-Han ;
Vu, Hong-Son ;
Pham, The-Tan .
PHYSICA SCRIPTA, 2025, 100 (03)
[46]   Mechanical properties and deformation behavior of amorphous nickel-phosphorous films measured by nanoindentation test [J].
Shou-Yi Chang ;
Yu-Shuien Lee ;
Hsiang-Long Hsiao ;
Ting-Kui Chang .
Metallurgical and Materials Transactions A, 2006, 37 :2939-2945
[47]   Corrosion behavior and mechanical properties of Q450 steel investigated using nanoindentation technology [J].
Wei, Yu ;
Zhang, Chuntao ;
Zhu, Hongjie ;
An, Renbing .
Construction and Building Materials, 2025, 491
[48]   Effects of Ion Irradiation and Temperature on Mechanical Properties of GaN Single Crystals under Nanoindentation [J].
Dong, Zhaohui ;
Zhang, Xiuyu ;
Li, Jiling ;
Peng, Shengyuan ;
Wan, Qiang ;
Xue, Jianming ;
Yi, Xin .
MATERIALS, 2023, 16 (24)
[49]   Investigation of the Effects of Environmental Fatigue on the Mechanical Properties of GFRP Composite Constituents Using Nanoindentation [J].
Gonabadi, H. ;
Oila, A. ;
Yadav, A. ;
Bull, S. .
EXPERIMENTAL MECHANICS, 2022, 62 (04) :585-602
[50]   Effects of surface roughness and maximum load on the mechanical properties of cancellous bone measured by nanoindentation [J].
Donnelly, E ;
Baker, SP ;
Boskey, AL ;
van der Meulen, MCH .
JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART A, 2006, 77A (02) :426-435