Thermoelectric properties of the p-type Bi2Te3-Sb2Te3-Sb2Se3 alloys fabricated by mechanical alloying and hot pressing

被引:77
|
作者
Kim, HC
Oh, TS [1 ]
Hyun, DB
机构
[1] Hongik Univ, Dept Met Engn & Mat Sci, Seoul 121791, South Korea
[2] Korea Inst Sci & Technol, Div Mat Sci & Technol, Seoul 136791, South Korea
关键词
alloys; chalcogenides; electrical properties; thermal conductivity;
D O I
10.1016/S0022-3697(99)00269-3
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
The p-type (100 - x)% Bi2Te3-x% Sb2Te3 (75 less than or equal to x less than or equal to 85) and 20% Bi2Te3-(80 - y)% Sb2Te3-gamma% Sb2Se3 (0 less than or equal to gamma less than or equal to 7) alloys were fabricated by mechanical alloying and hot pressing, and their thermoelectric properties were characterized. Among the hot-pressed (100 - x)% Bi2Te3-x% Sb2Te3 alloys, the 20% Bi2Te3-80% Sb2Te3 alloy exhibited a maximum figure-of-merit of 3.05 x 10(-3)/K. The Seebeck coefficient and the electrical resistivity of the hot-pressed 20% Bi2Te3-(80 - gamma) Sb2Te3-gamma% Sb2Se3 alloys increased with increasing the Sb2Se3 content due to the reduction of the hole concentration. The figure-of-merit of the hot-pressed 20% Bi2Te3-(80 - gamma)% Sb2Te3-gamma% Sb2Se3 alloys decreased from 3.05 x 10(-3)/K to 2.5 x 10(-3)/K with increasing the Sb2Se3 content up to 7 mol%, because the increment of the electrical resistivity was much larger than the decrement of the thermal conductivity and the increment of the Seebeck coefficient. (C) 2000 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:743 / 749
页数:7
相关论文
共 50 条
  • [1] Thermoelectric properties of p-type (Bi,Sb)2Te3 alloys fabricated by the hot pressing method
    Kim, HJ
    Kim, HC
    Hyun, DB
    Oh, TS
    METALS AND MATERIALS INTERNATIONAL, 1998, 4 (01) : 75 - 81
  • [2] Thermoelectric properties of p-type (Bi,Sb)2Te3 alloys fabricated by the hot pressing method
    Hee-Jeong Kim
    Hang-Chong Kim
    Dow-Bin Hyun
    Tae-Sung Oh
    Metals and Materials, 1998, 4 : 75 - 81
  • [3] EFFECTS OF GROWTH RATE ON THERMOELECTRIC PROPERTIES OF BI2TE3-SB2TE3-SB2SE3 PSEUDOTERNARY ALLOYS
    YIM, WM
    FITZKE, EV
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1968, 115 (05) : 556 - &
  • [4] THERMOELECTRIC PROPERTIES OF PARA TYPE BI2TE3-SB2TE3-SB2SE3 ALLOYS AND TYPE BI2TE3-BI2SE3 ALLOYS IN TEMPERATURE-RANGE 300 TO 600 K
    IMAMUDDIN, M
    DUPRE, A
    PHYSICA STATUS SOLIDI A-APPLICATIONS AND MATERIALS SCIENCE, 1972, 10 (02): : 415 - +
  • [5] Phase transformation and thermoelectric properties of p-type (Bi2Te3)0.25(Sb2Te3)0.75 prepared by mechanical alloying and hot pressing
    Fan, X. A.
    Yang, J. Y.
    Chen, R. G.
    Zhu, W.
    Bao, S. Q.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2006, 438 : 190 - 193
  • [6] ELECTRICAL AND THERMOELECTRICAL PROPERTIES OF UNDOPED BI2TE3-SB2TE3 AND BI2TE3-SB2TE3-SB2SE3 SINGLE-CRYSTALS
    JEON, HW
    HA, HP
    HYUN, DB
    SHIM, JD
    JOURNAL OF PHYSICS AND CHEMISTRY OF SOLIDS, 1991, 52 (04) : 579 - 585
  • [7] Thermoelectric properties of p-type 25%Bi2Te3+75%Sb2Te3 alloys manufactured by rapid solidification and hot pressing
    Kim, TS
    Kim, IS
    Kim, TK
    Hong, SJ
    Chun, BS
    MATERIALS SCIENCE AND ENGINEERING B-SOLID STATE MATERIALS FOR ADVANCED TECHNOLOGY, 2002, 90 (1-2): : 42 - 46
  • [9] Thermoelectric properties of p-type (Bi2Te3)x(Sb2Te3)1-x prepared via bulk mechanical alloying and hot pressing
    Yang, J
    Aizawa, T
    Yamamoto, A
    Ohta, T
    JOURNAL OF ALLOYS AND COMPOUNDS, 2000, 309 (1-2) : 225 - 228
  • [10] Thermoelectric Properties of Bi2Te3-Sb2Te3-Sb2Se3 Pseudo-Ternary Alloys in the Temperature Range 77 to 300 degrees K
    Yim, W. M.
    Fitzke, E. V.
    Rosi, F. D.
    JOURNAL OF MATERIALS SCIENCE, 1966, 1 (01) : 52 - 65