Effect of heat treatment on fatigue crack initiation of laser powder bed fusion stainless steel 316L

被引:15
作者
Zhang, Meng [1 ]
Sun, Chen-Nan [2 ]
Zhang, Xiang [3 ]
Goh, Phoi Chin [4 ]
Wei, Jun [2 ]
Hardacre, David [4 ]
Li, Hua [1 ]
机构
[1] Nanyang Technol Univ, Sch Mech & Aerosp Engn, Singapore Ctr 3D Printing, 50 Nanyang Ave, Singapore 639798, Singapore
[2] ASTAR, Singapore Inst Mfg Technol, 73 Nanyang Dr, Singapore 637662, Singapore
[3] Coventry Univ, Fac Engn Environm & Comp, Coventry CV1 5FB, W Midlands, England
[4] Lloyds Register Global Technol Ctr, 1 Fusionopolis Pl,09-11 Galaxis, Singapore 13852, Singapore
来源
12TH INTERNATIONAL FATIGUE CONGRESS (FATIGUE 2018) | 2018年 / 165卷
关键词
RESIDUAL-STRESS; PROCESSING PARAMETERS; MECHANICAL-PROPERTIES; BEHAVIOR; MICROSTRUCTURE; METALS; SLM;
D O I
10.1051/matecconf/201816522006
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Laser powder bed fusion (L-PBF) is an emerging additive manufacturing technique for building structural components. L-PBF processing defects, such as lack of fusion pores, promote fatigue crack initiation and shorten the fatigue life. With well-controlled processing, critical pores can be avoided such that the microstructure-driven intergranular crack initiation mode becomes operative. In this work, the fatigue crack initiation behaviours of as-built and solution annealed L-PBF stainless steel 316L were studied. Crack initiation of the as-built samples is driven by de-bonding of the dendritic grain boundaries. High temperature annealing results in the formation of thermally-induced defects, possibly via the reheat cracking mechanism and the nucleation of pre-existing gas pores. As heat treating could have led to recrystallization and annihilation of the original grain boundary defects, the thermally-induced defects became the new sites for crack initiation. In addition, heat treatment incurred significant reduction in yield strength, such that the interaction of fatigue and ratcheting strain accumulation dominated the deformation behaviour of the material. The resulting fatigue strength in the finite life regime was reduced by about 13% but the fatigue endurance limit was not affected.
引用
收藏
页数:6
相关论文
共 41 条
  • [1] Bai Y., 2017, MAT SCI ENG A
  • [2] Bina M. H., 2012, METALLURGY ADV MAT P
  • [3] Crack propagation and fracture toughness of Ti6A14V alloy produced by selective laser melting
    Cain, V
    Thijs, L.
    Van Humbeeck, J.
    Van Hooreweder, B.
    Knutsen, R.
    [J]. ADDITIVE MANUFACTURING, 2015, 5 : 68 - 76
  • [4] da Silva Bartolo PJ., 2013, P 6 INT C ADV RES VI
  • [5] Processing and mechanical properties of porous 316L stainless steel for biomedical applications
    Dewidar, Montasser M.
    Khalil, Khalil A.
    Lim, J. K.
    [J]. TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2007, 17 (03) : 468 - 473
  • [6] Determination and controlling of grain structure of metals after laser incidence: Theoretical approach
    Dezfoli, Amir Reza Ansari
    Hwang, Weng-Sing
    Huang, Wei-Chin
    Tsai, Tsung-Wen
    [J]. SCIENTIFIC REPORTS, 2017, 7
  • [7] Additive manufacturing in the context of structural integrity
    Gorelik, Michael
    [J]. INTERNATIONAL JOURNAL OF FATIGUE, 2017, 94 : 168 - 177
  • [8] Fatigue performance of additive manufactured TiAl6V4 using electron and laser beam melting
    Greitemeier, Daniel
    Palm, Frank
    Syassen, Freerk
    Melz, Tobias
    [J]. INTERNATIONAL JOURNAL OF FATIGUE, 2017, 94 : 211 - 217
  • [9] Effects of processing parameters on tensile properties of selective laser melted 304 stainless steel
    Guan, Kai
    Wang, Zemin
    Gao, Ming
    Li, Xiangyou
    Zeng, Xiaoyan
    [J]. MATERIALS & DESIGN, 2013, 50 : 581 - 586
  • [10] The Influence of Processing Parameters on the Mechanical Properties of SLM Parts
    Hanzl, Pavel
    Zetek, Miroslav
    Baksa, Tomas
    Kroupa, Tomas
    [J]. 25TH DAAAM INTERNATIONAL SYMPOSIUM ON INTELLIGENT MANUFACTURING AND AUTOMATION, 2014, 2015, 100 : 1405 - 1413